journal article·2015-08

Electrochemical boriding of molybdenum in molten borax

O. Kahvecioglu Feridun, V. Sista, O. L. Eryilmaz, A. Erdemir

Surface Engineering· Volume 31· Issue 8
Publisher page

Abstract

In this study, molybdenum plates (99·5% purity) were subjected to electrochemical boriding in a molten borax electrolyte in order to synthesise molybdenum boride phases on exposed surfaces. Electrochemical boriding was carried out at temperatures of 900, 950 and 1000°C for a duration of 30–180 min at a current density of 0·5 A cm−2. Cross-sectional microscopic examination of the plates indicated formation of 20 to 50 μm thick boride layers, depending on process temperature and duration. These layers consisted of two distinct boride phases: Mo2B4·027 and Mo2B5. The boride layer cross-sectional hardness was in the range of 1900–3250 HV with 50 g load. The adhesion of the boride coating to the molybdenum substrate was determined by a Rockwell C indentation adhesion test machine. The boride layers produced due to the electrochemical boriding technique were thick, hard, dense, and homogeneous.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Magnesium Alloys: Properties and Applications · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Argonne National Laboratory, 9700 S. Cass Avenue, Argonne, IL 60439, USA

Baker Hughes Incorporated, 9110 Grogan's Mill Rd, The Woodlands, TX 77380, USA

References (40)

Show source-provided references
1. 10.1016/S0925-8388(00)01082-310.1016/S0925-8388(00)01082-3 ↗
2. 10.1016/S0022-4596(02)00044-010.1016/S0022-4596(02)00044-0 ↗
3. 10.1361/10599630177034922210.1361/105996301770349222 ↗
4. 10.1016/j.jallcom.2014.04.06710.1016/j.jallcom.2014.04.067 ↗
5. 10.1016/j.ceramint.2013.11.02610.1016/j.ceramint.2013.11.026 ↗
6. 10.1016/j.surfcoat.2006.05.04210.1016/j.surfcoat.2006.05.042 ↗
7. Steinitz R · Trans. Am. Inst. Min. Metall. Pet. Eng. · 1952 · 194 · 983
8. Yasuda T, Banno A, Ito T, Kiyoshi K, Ishibayashi K, Chubu Sukegawa Enterprise Co., Ltd, and Kabushiki Kaisha SD: ‘Durability against corrosion by a molten light alloy’, US Patent 6238807 B1, published 29 May 2001.
9. Kudo T, and Obayashi H, Hitachi, Ltd. ‘Electrode catalyst’, US Patent 4242421, published 30 December 1980.
10. 10.1103/PhysRevB.73.14410810.1103/PhysRevB.73.144108 ↗
11. Kugai LN · Poroshk. Metall. · 1971 · 12 · 54
12. 10.1016/j.surfcoat.2006.01.00310.1016/j.surfcoat.2006.01.003 ↗
13. 10.1016/j.surfcoat.2004.05.02110.1016/j.surfcoat.2004.05.021 ↗
14. 10.1016/0022-5088(79)90025-010.1016/0022-5088(79)90025-0 ↗
15. 10.1016/S0955-2219(99)00031-X10.1016/S0955-2219(99)00031-X ↗
16. 10.1016/S0966-9795(96)00061-110.1016/S0966-9795(96)00061-1 ↗
17. Vines L, Cain J, Lee C.O, Koenigseder S, and Fujishiro F, Vlsi Technology, Inc. ‘Molybdenum boride barrier layers between aluminum and silicon at contact points in semiconductor devices’, US Patent 5329161, published 12 July 1994.
18. 10.1016/j.ijrmhm.2014.03.00310.1016/j.ijrmhm.2014.03.003 ↗
19. 10.1016/j.jallcom.2013.08.10710.1016/j.jallcom.2013.08.107 ↗
20. 10.1016/j.jallcom.2013.12.02310.1016/j.jallcom.2013.12.023 ↗
21. 10.1016/S0925-8388(97)00342-310.1016/S0925-8388(97)00342-3 ↗
22. 10.1016/j.jallcom.2007.03.02410.1016/j.jallcom.2007.03.024 ↗
23. 10.1016/0925-8388(96)02294-310.1016/0925-8388(96)02294-3 ↗
24. 10.1016/j.jallcom.2011.02.08310.1016/j.jallcom.2011.02.083 ↗
25. 10.1016/0022-5088(86)90136-010.1016/0022-5088(86)90136-0 ↗
26. 10.1016/j.jallcom.2003.12.02810.1016/j.jallcom.2003.12.028 ↗
27. 10.1016/0300-9416(73)90025-410.1016/0300-9416(73)90025-4 ↗
28. Malyshev VV · Rev. Roum. Chim. · 2010 · 55 · 233
29. 10.1016/j.tsf.2011.07.05710.1016/j.tsf.2011.07.057 ↗
30. 10.1016/j.tsf.2011.08.07710.1016/j.tsf.2011.08.077 ↗
31. 10.1016/j.surfcoat.2012.08.08310.1016/j.surfcoat.2012.08.083 ↗
32. 10.1016/j.surfcoat.2008.03.01110.1016/j.surfcoat.2008.03.011 ↗
33. 10.1016/j.msea.2011.08.01810.1016/j.msea.2011.08.018 ↗
34. 10.1016/j.optlastec.2011.11.01610.1016/j.optlastec.2011.11.016 ↗
35. 10.1016/j.apsusc.2014.01.15110.1016/j.apsusc.2014.01.151 ↗
36. 10.1016/j.matdes.2010.11.03110.1016/j.matdes.2010.11.031 ↗
37. 10.1016/j.surfcoat.2014.07.09210.1016/j.surfcoat.2014.07.092 ↗
38. 10.1070/RC2008v077n05ABEH00376610.1070/RC2008v077n05ABEH003766 ↗
39. 10.1016/j.physb.2006.04.01110.1016/j.physb.2006.04.011 ↗
40. Rogl P and Schuster J C (ed.): ‘Phase diagrams of ternary boron nitride and silicon nitride systems, monograph series on alloy phase diagrams’, 64–67; 1992, Materials Park, OH, ASM International.