Microarc Electrodeposition of Ceramic Films on Double Electrodes of AZ91D Magnesium Alloy by Symmetrical AC Pulse Method
Source abstract
Abstract
Using the two direction symmetrical alternating current pulse method, ceramic films were successfully electrodeposited simultaneously on anodic and cathodic AZ91D magnesium specimens by microarc oxidation. This process was named double electrode microarc electrodeposition (DEME). The thickness, morphology and composition of the DEME films were studied using SEM and X-ray diffraction patterns. The rare earth element Ce was detected in both the anodic and cathodic films when CeF4·H2O was added to the film forming an electrolyte. The improvement in corrosion resistance of AZ91D after DEME treatment was shown by comparing potentiodynamic scanning polarisation curves and the electrochemical impedance spectroscopy of the specimens with and without DEME treatment. By immersing the samples with and without DEME treatment in 3.5%NaCl solution, it was found that the corrosion rate of specimens treated using the DEME process was much lower than that of untreated specimens. In order to reduce their porosity, samples with DEME films were further painted with three different kinds of coatings: sol-gel, polysilicone and epoxy lacquer. Samples coated with DEME film and epoxy coatings could sustain a 336 h neutral salt spray test.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Dr YuanGang (lyg_fjj@sina.com.cn), Dr Wei and Dr JiuQing are in the Corrosion and Protection Center, University of Science and Technology, 100083 Beijing, China.
References (16)
Show source-provided references
1. MORDIKE B. L. and EBERT T. J. Mater. ScL Eng., 2001, A302, 37-45.10.1016/S0921-5093(00)01351-4 ↗
2. 10.1016/S0924-0136(01)00780-410.1016/S0924-0136(01)00780-4 ↗
3. GUANGLING S. · COITOS. Sci · 1998 · 40 · 1769
4. 10.1016/S0010-938X(98)00072-910.1016/S0010-938X(98)00072-9 ↗
5. 10.1016/S0010-938X(01)00092-010.1016/S0010-938X(01)00092-0 ↗
6. 10.1016/S0010-938X(01)00101-910.1016/S0010-938X(01)00101-9 ↗
7. 10.1016/S0010-938X(97)00090-510.1016/S0010-938X(97)00090-5 ↗
8. 10.1016/S0010-938X(99)00143-210.1016/S0010-938X(99)00143-2 ↗
9. 10.1016/S0925-8388(01)01899-010.1016/S0925-8388(01)01899-0 ↗
10. 10.1016/S0013-4686(98)00034-610.1016/S0013-4686(98)00034-6 ↗
11. KRISHNA L. RAMA, SOMARAJU K. R. C. and SUNDARAJAN G. Surf Cast. TechnoL, 2003, 163 — 164, 484-490.10.1016/S0257-8972(02)00646-1 ↗
12. 10.1016/S0040-6090(00)01026-910.1016/S0040-6090(00)01026-9 ↗
13. WENBIN X. · Mater. Lett · 2002 · 52
14. RUDD A. L. · COITOS. Sci · 2000 · 42 · 275
15. 10.1149/1.209578610.1149/1.2095786 ↗
16. CHUNG S. C. · COITOS. ScL · 2000 · 42 · 1249