Microstructure and dry sliding wear behaviour of titania and alumina–titania coatings
Source abstract
Abstract
The microstructure, hardness and wear properties of atmospheric plasma spray coating of TiO2 and Al2O3–13TiO2 with incremental hydrogen fractions (11·1–23·8%) in primary gas have been investigated in this work. TiO2 coating shows a fine bead-like surface structure, while Al2O3–13TiO2 predominantly exhibits a splat-like morphology. The microstructure shows a slight refinement in the structure for the highest hydrogen content possibly due to the higher specific enthalpy of the plasma plume. Both coatings show the highest hardness for samples coated with the highest hydrogen content possibly due to the refined structure. The roughness shows a mild decreasing trend for TiO2 coating, while the reverse trend is observed for Al2O3–13TiO2 coating. The wear loss and friction coefficient show a flat trend (0·4–0·6) for all the hydrogen contents. The worn tracks show a compacted mixture of ceramic, graphite and metallic particles.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Advanced Engineering Ashok Leyland Technical Center, Vellivoyalchavadi, Chennai 600103, India
Department of Metallurgical and Materials Engineering Indian Institute of Technology Madras, Chennai 600036, India
References (31)
Show source-provided references
1. 10.1016/S0039-6028(97)01000-510.1016/S0039-6028(97)01000-5 ↗
2. 10.1016/j.triboint.2005.08.00410.1016/j.triboint.2005.08.004 ↗
3. 10.1016/S0169-4332(01)00642-010.1016/S0169-4332(01)00642-0 ↗
4. 10.1016/S0043-1648(98)00181-110.1016/S0043-1648(98)00181-1 ↗
5. 10.1016/j.wear.2005.02.02510.1016/j.wear.2005.02.025 ↗
6. 10.1016/j.ijrmhm.2009.08.00610.1016/j.ijrmhm.2009.08.006 ↗
7. Pierre F · Surf. Eng. · 2008 · 24 · 110.1179/174329408X300379 ↗
8. 10.1016/j.wear.2009.01.02210.1016/j.wear.2009.01.022 ↗
9. 10.1016/j.triboint.2009.12.02310.1016/j.triboint.2009.12.023 ↗
10. 10.1016/j.corsci.2009.08.00510.1016/j.corsci.2009.08.005 ↗
11. 10.1016/j.actamat.2010.07.00110.1016/j.actamat.2010.07.001 ↗
12. 10.1016/j.matdes.2010.08.01910.1016/j.matdes.2010.08.019 ↗
13. 10.1016/j.ceramint.2009.07.01210.1016/j.ceramint.2009.07.012 ↗
14. 10.1016/j.jeurceramsoc.2006.04.09910.1016/j.jeurceramsoc.2006.04.099 ↗
15. 10.1016/j.surfcoat.2007.04.05710.1016/j.surfcoat.2007.04.057 ↗
16. 10.1016/j.ceramint.2004.11.01410.1016/j.ceramint.2004.11.014 ↗
17. 10.1016/j.jmapro.2008.10.00110.1016/j.jmapro.2008.10.001 ↗
18. 10.1016/S0257-8972(02)00890-310.1016/S0257-8972(02)00890-3 ↗
19. 10.1016/j.surfcoat.2006.11.02610.1016/j.surfcoat.2006.11.026 ↗
20. 10.1016/j.wear.2011.03.02310.1016/j.wear.2011.03.023 ↗
21. Naumann T, Berger L.M, Ingwerth M, Vuoristo P: in ‘Thermal spray 2003: advancing the science and applying the technology’, 1441–1445; 2003, Materials Park, OH, ASM International.10.31399/asm.cp.itsc2003p1441 ↗
22. 10.1016/j.jmatprotec.2007.06.00110.1016/j.jmatprotec.2007.06.001 ↗
23. 10.1016/j.jmatprotec.2010.10.02010.1016/j.jmatprotec.2010.10.020 ↗
24. 10.1016/j.wear.2006.11.01210.1016/j.wear.2006.11.012 ↗
25. Zhang Y · Trans. Nonferrous Met. Soc. China · 2005 · 15 · 594
26. Zhang W · Mater. Forum · 2007 · 31 · 76
27. 10.1179/174329407X17443410.1179/174329407X174434 ↗
28. 10.1016/j.surfcoat.2007.03.01010.1016/j.surfcoat.2007.03.010 ↗
29. 10.1016/j.jmatprotec.2010.10.02110.1016/j.jmatprotec.2010.10.021 ↗
30. 10.1179/174329405X3002010.1179/174329405X30020 ↗
31. 10.1016/j.tsf.2010.11.04710.1016/j.tsf.2010.11.047 ↗