journal article·2024-01Open access

Effect of annealing on AZ31 magnesium alloy on MAO coatings

Shanshan Lu, Bo Jiang, Aoyun Fan, Renguo Song

Surface Engineering· Volume 40· Issue 1

Abstract

AZ31 magnesium alloy with different annealing temperatures was subjected to micro-arc oxidation (MAO) treatment, and its corrosion behaviour was studied using immersion experiments, polarisation curves, electrochemical impedance spectra, scanning electron microscopy (SEM) and X-ray diffraction (XRD) spectra. The alloy, when annealed at 300 °C, had the smallest grain size and the lowest electrical conductivity. Compared to other annealed alloys, the MAO coating had the smallest pore size and porosity and better corrosion resistance. The corrosion resistance of the alloy increased initially and then decreased with the increase in annealing temperature. This is mainly because the grain size first decreases and then increases, leading to a decline in electrical conductivity and then a rise, resulting in changes in the microstructure of the coating surface.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Changzhou University, Changzhou, Jiangsu, China

Jiangsu Key Laboratory of Materials Surface Science and Technology, Changzhou University, Changzhou, Jiangsu, China

References (32)

Show source-provided references
1. 10.1002/adem.20220074110.1002/adem.202200741 ↗
2. 10.1038/s41467-018-04981-410.1038/s41467-018-04981-4 ↗
3. 10.1021/acs.iecr.0c0336810.1021/acs.iecr.0c03368 ↗
4. 10.1007/s12666-015-0621-x10.1007/s12666-015-0621-x ↗
5. 10.1039/D2RA07829E10.1039/D2RA07829E ↗
6. 10.1007/s40195-022-01462-y10.1007/s40195-022-01462-y ↗
7. 10.3390/ma1513471210.3390/ma15134712 ↗
8. 10.3390/ijms23181070810.3390/ijms231810708 ↗
9. 10.1038/s41598-017-08242-010.1038/s41598-017-08242-0 ↗
10. 10.1021/acsomega.9b0406010.1021/acsomega.9b04060 ↗
11. Liu N · Int J Appl Ceram Technol · 2022 · 19 · 2556
12. 10.1080/02670844.2019.165637110.1080/02670844.2019.1656371 ↗
13. 10.1016/j.scriptamat.2022.11460410.1016/j.scriptamat.2022.114604 ↗
14. 10.1002/sia.379210.1002/sia.3792 ↗
15. 10.1016/j.jallcom.2015.12.10810.1016/j.jallcom.2015.12.108 ↗
16. 10.1063/1.165268010.1063/1.1652680 ↗
17. 10.1016/j.actamat.2016.12.01810.1016/j.actamat.2016.12.018 ↗
18. 10.1080/02670844.2019.169373210.1080/02670844.2019.1693732 ↗
19. 10.1111/ijac.1389110.1111/ijac.13891 ↗
20. 10.1080/02670844.2016.119012310.1080/02670844.2016.1190123 ↗
21. 10.3390/met1307116110.3390/met13071161 ↗
22. 10.3390/coatings1308137010.3390/coatings13081370 ↗
23. 10.1016/j.jelechem.2022.11620610.1016/j.jelechem.2022.116206 ↗
24. 10.1016/j.matchemphys.2023.12796310.1016/j.matchemphys.2023.127963 ↗
25. 10.1007/s11665-022-06724-510.1007/s11665-022-06724-5 ↗
26. 10.1016/j.rinp.2019.01.09510.1016/j.rinp.2019.01.095 ↗
27. 10.1016/j.apsusc.2019.14377210.1016/j.apsusc.2019.143772 ↗
28. 10.1080/1478422X.2023.220996210.1080/1478422X.2023.2209962 ↗
29. 10.1002/adem.20070024610.1002/adem.200700246 ↗
30. 10.1007/s10853-022-06977-410.1007/s10853-022-06977-4 ↗
31. 10.1080/02670844.2019.159657710.1080/02670844.2019.1596577 ↗
32. 10.1016/j.jallcom.2020.15372110.1016/j.jallcom.2020.153721 ↗