Abstract The present study evaluates the effect of operating temperature on the tribological behaviour of electroless Ni-P-W coating developed over mild steel. The constituent of the coating is found to be uniformly distributed. The incorporation of tungsten increases the as-deposit hardness (670 HV0.1) of Ni-P coatings besides improving its crystallinity. The friction and wear tests are carried out under elevated temperature (100 to 500 °C) in a pin-on-disc setup. The results reveal that Ni-P-W coating (especially heat treated ones) display a stable friction and wear behaviour even when subjected to elevated working temperature. The as-deposited coating on the other hand shows increased wear resistance particularly when tested at 300 and 500 °C which is due to microstructural changes induced in the coating because of exposure to high temperature. This is also supported by the excellent hardness shown by the samples after test (46% increase in hardness after testing at 500 °C compared to as-deposited hardness). The applied load and sliding velocity exhibit marginal influence over the friction behavior of the coating especially for heat treated coatings. Study of worn surface reveals that the wear is governed by both abrasive and adhesive mechanisms. Moreover, the formation of oxide layers on the coating at high temperature is also believed to influence the tribological behavior of Ni-P-W coatings.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Electrocatalysts for Energy Conversion · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Mellor · 2006
2. Nickel plating on steel by chemical reduction
3. Tribology of electroless nickel coatings–a review10.1016/j.matdes.2010.11.013 ↗
4. Electroless deposition of Ni–Cu–P, Ni–W–P and Ni–W–Cu–P alloys10.1016/j.surfcoat.2004.07.068 ↗
5. Thermal reliability of electroless Ni-P-W coating during the aging treatment
6. Electroless deposition of Ni–W–P coating on AZ91D magnesium alloy10.1016/j.apsusc.2006.11.022 ↗
7. Friction and wear behavior of electroless Ni-P and Ni-W-P alloy coatings10.1016/j.wear.2008.01.002 ↗
8. The electroless deposition of nickel-phosphorus tungsten alloys
9. Mechanical and corrosion behavior of amorphous and crystalline electroless Ni–W–P coatings10.1007/s10008-014-2437-8 ↗
10. Thermal stability and mechanical properties of Ni-W-P electroless deposits
11. Studies on electroless Ni-W-P and Ni-W-Cu-P alloy coatings using chloride-based bath10.1016/j.surfcoat.2005.04.053 ↗
12. Properties of electroless nickel at elevated temperature-a review10.1016/j.proeng.2014.12.321 ↗
13. Tribological characterization of electroless Ni –10% P coatings at elevated test temperature under dry conditions10.1007/s00170-011-3832-2 ↗
14. Tribological behaviour of electroless Ni-P deposits under elevated temperature10.1007/s12633-016-9450-8 ↗
15. High temperature friction and wear behaviour of Ni-P-Ag-Al2O3 hybrid nanocomposite coating10.1179/0020296713Z.000000000105 ↗
16. High temperature tribology of nanocrystalline Ni-P-Ag coating10.1179/1743294412Y.0000000085 ↗
17. Nanocomposite and nanostructured tribological materials for space applications
18. Tribological characteristics of electroless Ni–P–MoS2 composite coatings at elevated temperatures10.1016/j.apsusc.2012.10.055 ↗
19. Elevated temperature dry sliding wear behavior of nickel-based composite coating on austenitic stainless steel deposited by a novel central hollow laser cladding10.1016/j.apsusc.2011.08.072 ↗
20. Autocatalytic duplex Ni-P/Ni-W-P coatings on AZ31B magnesium alloy10.1016/j.surfcoat.2013.12.022 ↗
21. Surface morphology and structure of electroless ternary Ni-W-P deposits with various W and P contents10.1016/j.jallcom.2009.06.173 ↗
22. Phase transformation behavior of nanocrystalline Ni–W–P alloys containing various W and P contents10.1016/j.surfcoat.2011.11.024 ↗
23. Studies on autocatalytic deposition of ternary Ni-W-P alloys using nickel sulphamate bath10.1016/j.surfcoat.2005.11.131 ↗
24. Autocatalytic (electroless) nickel-tungsten-phosphorus plating
25. Structural and phase transformation behaviour of electroless Ni–P and Ni–W–P deposits
26. Microstructure evaluation and strengthening mechanism of Ni–P–W alloy coatings
27. The effect of sliding speed and normal load on friction and wear property of aluminum
28. High temperature wear of an electroless Ni-P-BN composite coating
29. Tribological behavior of electroless Ni–P coatings in various corrosive environments10.1142/S0218625X16500402 ↗
30. The friction and wear of electroless Ni-P matrix with PTFE and/or SiC particles composite10.1016/j.triboint.2005.04.032 ↗
31. Preparation and characterization of silicon nitride codeposited electroless nickel composite coatings10.1016/j.jallcom.2006.07.036 ↗
32. Measurement of dynamic material behavior under nearly uniaxial strain condition10.1016/0020-7683(78)90032-X ↗
33. Adhesion and adhesive wear
34. Wear behaviour of silicon carbide/electroless nickel composite coatings at high temperature10.1179/026708401225005359 ↗
35. Initiation and formation of electroless nickel–boron coatings on mild steel: effect of substrate roughness10.1016/j.mseb.2010.08.003 ↗