journal article·2023-08Open access

Adatom controlled emergence of high hardness in biocompatible beta-Ti3Au intermetallic thin film surfaces

Cecil Cherian Lukose, Ioannis Anestopoulos, Leon Bowen, Mihalis I. Panayiotidis, Martin Birkett

Abstract

There is growing international interest in hard biocompatible thin film surface coatings to extend the lifetime of medical implants. Parameters of the physical vapour deposition technique can be utilized to fine tune the microstructure and resulting properties of the growing thin film surface by modifying the adatom mobility of the incoming species. This work investigates the evolution of high hardness and biocompatibility of sputter deposited beta-Ti3Au intermetallic thin film surfaces as a function of growth temperature and pressure. Titanium and gold are sputtered in an optimised 3:1 ratio over glass and Ti6Al4V substrates at varying pressures of 0.3 to 1.2 Pa and temperatures of 25 to 450°C. The microstructure and crystallinity of the deposited films improved with reduction in pressure from 1.2 to 0.3 Pa but development of the β-Ti3Au intermetallic compound occurred at temperatures above 350˚C. The density of the films also increased with reducing pressure, whereas improvement in their columnar structure was observed with increasing substrate temperature. These microstructural changes caused by adatom mobility variation, led to the emergence of superior mechanical surface hardness, reaching a peak value of 12.5 GPa for films grown at 0.3 Pa and 450°C. All thin film surfaces were highly biocompatible with ion leaching levels below 1 ppm, and films deposited at lower pressure exhibited much safer cytotoxic profiles against L929 mouse fibroblasts. This work demonstrates the emergence of high hardness and biocompatibility in Ti3Au thin film surfaces with potential as next generation medical implant coating materials.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Biocompatibility of Ti-alloys for long-term implantation10.1016/j.jmbbm.2012.11.014 ↗
2. Magnetron-sputtered TixNy thin films applied on titanium-based alloys for biomedical applications: Composition-microstructure-property relationships10.1016/j.surfcoat.2018.05.068 ↗
3. Enhanced biocompatibility of Co-Cr implant material by Ti coating and micro-arc oxidation10.1002/jbm.b.31270 ↗
4. In-situ formation of laser Ti6Al4V–TiB composite coatings on Ti6Al4V alloy for biomedical application10.1016/j.surfcoat.2015.10.079 ↗
5. Synthesis and evaluation of TaC nanocrystalline coating with excellent wear resistance, corrosion resistance, and biocompatibility10.1016/j.ceramint.2021.03.333 ↗
6. Deposition of titanium nitride and hydroxyapatite-based biocompatible composite by reactive plasma spraying10.1016/j.apsusc.2011.12.049 ↗
7. Development of Ti-Nb-Zr alloys with high elastic admissible strain for temporary orthopedic devices10.1016/j.actbio.2015.03.023 ↗
8. Characterisation of the microplasma spraying of biocompatible coating of titanium10.1111/jmi.12849 ↗
9. A graded nano-TiN coating on biomedical Ti alloy: Low friction coefficient, good bonding and biocompatibility10.1016/j.msec.2016.10.033 ↗
10. First principles study of structural, electronic, mechanical and thermal properties of A15 intermetallic compounds Ti3X (X=Au, Pt, Ir)10.1016/j.physb.2012.08.029 ↗
11. Evolution of the mechanical properties of Ti-based intermetallic thin films doped with different metals to be used as biomedical devices10.1016/j.apsusc.2019.144617 ↗
12. Reactive combinatorial synthesis and characterization of a gradient Ag-Ti oxide thin film with antibacterial properties10.1016/j.actbio.2014.09.048 ↗
13. Influence of the surface properties on bactericidal and fungicidal activity of magnetron sputtered Ti-Ag and Nb-Ag thin films10.1016/j.msec.2016.01.029 ↗
14. Influence of Cu-Ti thin film surface properties on antimicrobial activity and viability of living cells10.1016/j.msec.2015.06.013 ↗
15. Influence of Cu, Au and Ag on structural and surface properties of bioactive coatings based on titanium10.1016/j.msec.2016.11.091 ↗
16. Deposition of thin titanium–copper films with antimicrobial effect by advanced magnetron sputtering methods10.1016/j.msec.2011.06.009 ↗
17. Antibacterial and Biocompatible Titanium-Copper Oxide Coating May Be a Potential Strategy to Reduce Periprosthetic Infection: An In Vitro Study10.1007/s11999-016-4713-7 ↗
18. Mechanical properties and microstructures of dental cast Ti-Ag and Ti-Cu alloys10.4012/dmj.21.270 ↗
19. Mechanical properties and microstructures of cast Ti–Cu alloys10.1016/S0109-5641(02)00027-1 ↗
20. Grindability of cast Ti–Cu alloys10.1016/S0109-5641(02)00080-5 ↗
21. Grindability and mechanical properties of experimental Ti–Au, Ti–Ag and Ti–Cu alloys10.1016/j.ics.2005.06.006 ↗
22. What controls the antibacterial activity of Ti-Ag alloy, Ag ion or Ti2Ag particles?10.1016/j.msec.2019.110548 ↗
23. In vitro cytotoxicity evaluation of elemental ions released from different prosthodontic materials10.1016/j.dental.2009.07.008 ↗
24. In vitro cytotoxicity of metallic ions released from dental alloys10.1007/s10266-014-0192-z ↗
25. Biocompatibility of gold nanoparticles: In-vitro and In-vivo study10.1016/j.matpr.2020.12.826 ↗
26. High hardness in the biocompatible intermetallic compound β-Ti3Au10.1126/sciadv.1600319 ↗
27. Ιntermetallic β-Ti3Au hard thin films prepared by magnetron sputtering10.1016/j.tsf.2017.11.027 ↗
28. Effect of gold addition on the microstructure, mechanical properties and corrosion behavior of Ti alloys10.1007/s13404-014-0138-9 ↗
29. Cytocompatibility and electrochemical properties of Ti-Au alloys for biomedical applications10.1002/jbm.b.30798 ↗
30. Generalization of intrinsic ductile-to-brittle criteria by Pugh and Pettifor for materials with a cubic crystal structure10.1038/s41598-021-83953-z ↗
31. Thermal activation of Ti(1-x)Au(x) thin films with enhanced hardness and biocompatibility
32. The effect of sputtering gas pressure on structure and photocatalytic properties of nanostructured titanium oxide self-cleaning thin film10.1016/j.vacuum.2010.08.001 ↗
33. Optimisation of ZnO:Al films by change of sputter gas pressure for solar cell application10.1016/S0169-4332(02)00611-6 ↗
34. Structure-Zone Modeling of Sputter-Deposited Thin Films: A Brief Review10.5757/ASCT.2019.28.6.179 ↗
35. Structure-Zone Models of Thin Films10.1117/12.941846 ↗
36. Effects of radio-frequency plasma on structure and properties in Ti film deposition by dc and pulsed dc magnetron sputtering10.1016/j.tsf.2009.03.055 ↗
37. Structural, morphological and mechanical hardness properties of titanium nitride thin films deposited by DC magnetron sputtering: Effect of substrate temperature
38. The effect of substrate temperature and biasing on the mechanical properties and structure of sputtered titanium nitride thin films10.1016/S0257-8972(99)00606-4 ↗
39. Effect of Deposition Pressure, Nitrogen Content and Substrate Temperature on Optical and Mechanical Behavior of Nanocomposite Al-Si-N Hard Coatings for Solar Thermal Applications10.1007/s11665-018-3730-y ↗
40. Effect of deposition power and pressure on rate deposition and resistivity of titanium thin films grown by DC magnetron sputtering10.1080/00387010.2016.1212244 ↗
41. Effect of sputtering pressure and temperature on DC magnetron sputtered CrN films10.1179/174329409X389326 ↗
42. Sputtering power and deposition pressure effects on the electrical and structural properties of copper thin films10.1007/s10853-005-1362-8 ↗
43. Effect of Deposition Parameters on Microstructure of the Ti-Mg Immiscible Alloy Thin Film Deposited by Multi-Arc Ion Plating10.3390/met9111229 ↗
44. The effect of deposition parameters and Ti content on structural and wear properties of MoS2Ti coatings10.1016/j.wear.2005.03.004 ↗
45. The effect of target density and its morphology on TiO2 thin films grown on Si(100) by PLD10.1016/S0169-4332(99)00269-X ↗
46. Effect of deposition pressure on structural, optical and electrical properties of zinc selenide thin films10.1016/j.physb.2011.02.022 ↗
47. The Scherrer Formula for X-Ray Particle Size Determination10.1103/PhysRev.56.978 ↗
48. The Au-Ti (Gold-Titanium) system10.1007/BF02868667 ↗
49. An Energy Balance Criterion for Nanoindentation-Induced Single and Multiple Dislocation Events10.1115/1.2125988 ↗
50. Behavior of Ti0.5Al0.5N thin film in nanoscale deformation with different loading rates10.1016/j.tsf.2008.06.002 ↗
51. Nanoindentation Studies of Yield Point Phenomena on Gold Single Crystals10.1557/PROC-436-159 ↗
52. Mechanical properties and fracture toughness of multilayer hard coatings using nanoindentation10.1016/S0040-6090(00)01004-X ↗
53. Effects of internal stresses on the mechanical properties of deposition thin films10.1016/j.jmatprotec.2007.11.258 ↗
54. TEM and nanoindentation studies on sputtered Ti40Ni60 thin films10.1016/j.matchemphys.2005.08.020 ↗
55. Effect of surface roughness on nanoindentation test of thin films10.1016/j.engfracmech.2008.06.016 ↗
56. Effect of surface roughness in the determination of the mechanical properties of material using nanoindentation test10.1002/sca.21111 ↗
57. Thermal stability of nitride thin films10.1016/S0042-207X(00)00143-3 ↗
58. Microstructural design of hard coatings10.1016/j.pmatsci.2006.02.002 ↗
59. Effect of grain size on the indentation hardness for polycrystalline materials by the modified strain gradient theory10.1016/j.ijsolstr.2013.05.002 ↗
60. Elastic modulus of Ti–6Al–4V–xB alloys with B up to 0.55wt.%10.1016/j.scriptamat.2009.09.022 ↗
61. Effects of the substrate on the determination of thin film mechanical properties by nanoindentation10.1016/S1359-6454(01)00328-7 ↗
62. Titanium-Based Biomaterials for Preventing Stress Shielding between Implant Devices and Bone10.1155/2011/836587 ↗
63. Modeling Effect of Surface Roughness on Nanoindentation Tests10.1016/j.procir.2013.06.112 ↗
64. Measurement of Thin-film Coating Hardness in the Presence of Contamination and Roughness: Implications for Tribology10.1007/s11661-016-3342-9 ↗
65. Finite element simulation of the effect of surface roughness on nanoindentation of thin films with spherical indenters10.1016/j.surfcoat.2007.07.038 ↗
66. Wear Resistance of Ti-6Al-4V Alloy Ball Heads for Use in Implants10.3390/jfb12040065 ↗
67. Tribological property of the cobalt-chromium femoral head with different regions of wear in total hip arthroplasty10.1243/09544119JEIM709 ↗
68. Oxidized Zirconium Total Knee Arthroplasty Implant Failure in a Patient with Knee Instability10.1016/j.artd.2020.06.015 ↗
69. Cytotoxicity, in Vivo Skin Irritation and Acute Systemic Toxicity of the Mesoporous Magnesium Carbonate Upsalite10.4236/jbnb.2015.64024 ↗
70. ISO 10993-5 Biological evaluation of medical devices - part 5 - tests for in vitro cytotoxicity, 2009, pp. 34.
71. A new porous titanium–nickel alloy: Part 2. Sensitization, irritation and acute systemic toxicity evaluation
72. Oxygen plasma treatment to restrain nickel out-diffusion from porous nickel titanium orthopedic materials10.1016/j.surfcoat.2006.07.072 ↗
73. Toxicity of surface-modified copper oxide nanoparticles in a mouse macrophage cell line: Interplay of particles, surface coating and particle dissolution10.1016/j.chemosphere.2017.12.182 ↗