Ablation resistance enhancement of CVD-HfC on nose-shaped C/C composites by optimizing interface layer thickness and thermal stress distribution
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Advanced ceramic materials synthesis · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. A review of carbon fiber surface modification methods for tailor-made bond behavior with cementitious matrices10.1016/j.pmatsci.2022.101040 ↗
2. Oxidation failure behavior and repair of the damaged SiC-ZrB2 of C/C composites10.1016/j.apsusc.2024.160865 ↗
3. Ablation resistance of ZrB2-SiC/SiC coating prepared by pack cementation for graphite10.1016/j.jallcom.2016.04.010 ↗
4. Oxidation protection of C/C composites with a multilayer coating of SiC and Si + SiC + SiC nanowires10.1016/j.carbon.2011.10.048 ↗
5. Microstructure and mechanical properties of carbon fiber reinforced multilayered (PyC–SiC)n matrix composites10.1016/j.matdes.2015.07.018 ↗
6. Ablation behavior of HfC coating with different thickness for carbon/carbon composites at ultra-high temperature10.1016/j.jeurceramsoc.2020.10.055 ↗
7. MoSi2 modified HfC coating for the ablation protection of SiC-coated C/C composites: ablation resistance and behavior10.1016/j.corsci.2022.110418 ↗
8. WSi2 modified HfB2-SiC coating: Microstructure and ablation resistance10.1016/j.jeurceramsoc.2023.07.070 ↗
9. A low-temperature preparation strategy of SiC/ZrB2-CrSi2-Si/SiC multilayer oxidation-resistant coating for C/C composites: process, kinetics and mechanism research10.1016/j.apsusc.2021.149993 ↗
10. Ablation behavior of high-entropy boride (Hf-Zr-Ta-Ti)B2 coating fabricated via supersonic atmospheric plasma spraying for carbon/carbon composites10.1016/j.compositesb.2023.111137 ↗
11. Diffusion and solid solution formation between the binary carbides of TaC, HfC and ZrC10.1016/j.ijrmhm.2013.03.009 ↗
12. Preparation and ablation resistance of ZrC nanowires-reinforced CVD-ZrC coating on sharp leading edge C/C composites10.1016/j.apsusc.2022.152617 ↗
13. Development, and characterisation of ultra-high-temperature ceramics composite (UHTC)
14. Effect of microstructure on the ablation behavior and mechanical properties of CVD-HfC coating10.1016/j.corsci.2021.109815 ↗
15. Ablation mechanism of HfC-HfO2 protective coating for SiC-Coated C/C composites in an oxyacetylene torch environment10.1016/j.jmst.2016.11.010 ↗
16. Design, preparation and properties of carbon fiber reinforced ultra-high temperature ceramic composites for aerospace applications: a review10.1016/j.jmst.2016.08.004 ↗
17. Micro/nano multiscale reinforcing strategies toward extreme high-temperature applications: Take carbon/carbon composites and their coatings as the examples10.1016/j.jmst.2021.03.076 ↗
18. Ablation resistance of HfC-TaC-Hf6Ta2O17 composite coatings prepared by vacuum plasma spraying10.1016/j.corsci.2023.111368 ↗
19. MoSi2-HfC/TaC-HfC multi-phase coatings synthesized by supersonic atmospheric plasma spraying for C/C composites against ablation10.1016/j.corsci.2021.109884 ↗
20. Ablation behavior of (ZrC/SiC)3 alternate coating prepared on sharp leading edge C/C composites by CVD10.1016/j.jmst.2021.10.049 ↗
21. Effect of PyC interface phase on the cyclic ablation resistance and flexural properties of two-dimensional Cf/HfC composites10.1016/j.jeurceramsoc.2020.08.049 ↗
22. Microstructure and anti-ablation performance of HfC-TaC and HfC-ZrC coatings synthesized by CVD on C/C composites10.1016/j.ceramint.2020.01.006 ↗
23. Improvement of ablation resistance of CVD-HfC/SiC coating on hemisphere shaped C/C composites by introducing diffusion interface10.1016/j.jeurceramsoc.2021.02.004 ↗
24. Effect of CVD ZrB2 coating thickness on anti-ablation performance of C/SiC composites10.1016/j.ceramint.2018.01.264 ↗
25. Analytical solution of quenching-induced deposition stress in functionally graded thermal barrier coatings10.1016/j.ceramint.2019.03.163 ↗
26. Discussion on structural parameters of the multilayer ZrC/TaC coatings based on stress analysis and ablation behaviors10.1016/j.surfcoat.2022.128243 ↗
27. Investigation of residual stress in lead-free BNT-based ceramic/ceramic composites10.1016/j.actamat.2018.02.014 ↗
28. Disclosing residual thermal stresses in UHT fibre-reinforced ceramic composites and their effect on mechanical behaviour and damage evolution10.1016/j.compositesb.2022.110369 ↗
29. Fiber/matrix interfacial shear strength of C/C composites with PyC–TaC–PyC and PyC–SiC–TaC–PyC multi-interlayers10.1016/j.ceramint.2013.01.080 ↗
30. Microstructure and mechanical properties of Cf/SiC composites with dispersed C-SiC interphase prepared by chemical vapor infiltration10.1016/j.compositesa.2022.107339 ↗
31. Key role of interphase in continuous fiber 3D printed ceramic matrix composites10.1016/j.compositesa.2022.107127 ↗
32. Optimizing and ablation behavior of ZrC-SiC coating prepared by a coupling process10.1016/j.matchar.2025.114787 ↗
33. Ablation resistance of HfC-TaC/HfC-SiC alternate coating for SiC-coated carbon/carbon composites under cyclic ablation10.1016/j.jeurceramsoc.2021.01.050 ↗
34. Characterization and thermal shock behavior of Y2O3 films deposited on freestanding CVD diamond substrates10.1016/j.apsusc.2016.03.086 ↗
35. Design and optimization of the coating thickness on chopped carbon fibers and sintering temperature for ZrB2-SiC-Cf composites prepared by hot pressing10.1016/j.jeurceramsoc.2019.03.038 ↗
36. Growth process and mechanism of SiC layer deposited by CVD method at normal atmosphere10.1016/j.jeurceramsoc.2019.07.022 ↗
37. Design optimization for thermal conductivity of plain-woven textile composites10.1016/j.compstruct.2020.112830 ↗
38. Research advances in residual thermal stress of ceramic/metal brazes10.1016/j.ceramint.2021.04.220 ↗