Biomimetic bamboo leaf double-sided microstructure composite surface and its delayed icing performance
Source abstract
Abstract
Abstract The frost phenomenon occurred on the surface of engineering equipment can not only lead to a reduction in the efficiency of equipment but a higher energy consumption. How to effectively inhibit or delay the frost behavior on a material surface and improve the anti-frost property on the surface is of great importance. It is found that the nano needle structure on the surface of bamboo leaves can provide large Laplace pressure to drive droplets to bounce and hence delay the condensation process. In addition, in the frost crystal growth stage, the nano needle structure can reduce the contact area between droplets and the surface of bamboo leaves, and hence limit the phase-change heat transfer of water vapor and increase the thermodynamic barrier when nucleation of water vapor occurs, thereby delaying the frost crystal growth. In this paper, inspired by bamboo leaves, biomimetic structures are constructed on the surface of an aluminum alloy by laser processing and sol-gel method. Results reveal that delayed frost formation on the surface is realized, which is of immense practical value in engineering and many other aspects.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Surface Modification and Superhydrophobicity · Icing and De-icing Technologies · Adhesion, Friction, and Surface Interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Study of intelligent controller for preventing moist in electrical equipment based on fuzzy control10.15938/j.jhust.2012.02.015 ↗
2. Experimental and theoretical study of frost melting water retention on fin surfaces with different surface characteristics10.1016/j.expthermflusci.2015.10.015 ↗
3. Investigation of defrosting water retention on the surface of evaporator impacting the performance of air source heat pump during periodic frosting–defrosting cycles10.1016/j.apenergy.2014.07.028 ↗
4. Visual and theoretical analyses of the early stage of frost formation on cold surfaces10.1615/JEnhHeatTransf.v14.i3.70 ↗
5. Anti-icing/frosting and self-cleaning performance of superhydrophobic aluminum alloys10.1007/s00339-017-1509-x ↗
6. Experimental study on frosting/defrosting characteristics of microgrooved metal surfaces10.1016/j.ijrefrig.2014.11.002 ↗
7. Frost formation on a super-hydrophobic surface under natural convection conditions10.1016/j.ijheatmasstransfer.2008.03.026 ↗
8. Self-propelled dropwise condensate on superhydrophobic surfaces10.1103/PhysRevLett.103.184501 ↗
9. Jumping-droplet-enhanced condensation on scalable superhydrophobic nanostructured surfaces10.1021/nl303835d ↗
10. Self-propelled droplet behavior during condensation on superhydrophobic surfaces10.1063/1.4949010 ↗
11. Condensed droplet growth on surfaces with various wettability10.1016/j.applthermaleng.2017.01.060 ↗
12. A note on frosting of heat pump evaporator surfaces10.1016/0198-7593(85)90077-3 ↗
13. Analysis and countermeasures discussion for large area icing accident on power grid10.13336/j.1003-6520.hve.2008.02.020 ↗
14. State-of-the-art on power line de-icing10.1016/S0169-8095(97)00057-4 ↗
15. Anti-condensation behavior of bamboo leaf surface (backside) and its bionic preparation10.1088/2053-1591/abfc01 ↗
16. Characterization of multi-scale morphology and superhydrophobicity of water bamboo leaves and biomimetic polydi-methylsiloxane (PDMS) replicas10.1016/S1672-6529(14)60152-9 ↗
17. Delayed freezing on water repellent materials10.1021/la900929u ↗