journal article·1976-11

Comparison of Textile Mechanical Properties of Cotton in Crosslinking with Dimethylolethyleneurea and Formaldehyde

U. Meyer, K. Müller, H. Zollinger

Textile Research Journal· Volume 46· Issue 11
Publisher page

Abstract

Cotton fabrics were crosslinked with dimethylolethyleneurea (DMEU) and with formaldehyde by the pad-dry-cure process. The following parameters were varied: concentration of catalyst (MgCl 2 ) and crosslinking agent, reaction time, and temperature. The crosslinked fabrics were characterized by dry and wet crease-recovery angles, tensile strength, and degree of polymerization. The results show that with DMEU a significantly better dry crease-recovery angle/tensile strength relation is obtainable. This difference is due entirely to a greater degradation of cellulose by hydrolysis in treatments with formaldehyde. Furthermore, in the case of DMEU the effect/strength loss relation can be improved by using very high resin concentrations in the padding liquor.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Dyeing and Modifying Textile Fibers · Textile materials and evaluations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Industrial and Engineering Chemistry, Swiss Federal Institute of Technology (ETII), 8006 Zürich, Switzerland

References (9)

Show source-provided references
1. 10.1177/00405175600300070410.1177/004051756003000704 ↗
2. 10.1002/hlca.1973056010910.1002/hlca.19730560109 ↗
3. 10.1177/00405175670370090510.1177/004051756703700905 ↗
4. 10.1177/00405175760460101210.1177/004051757604601012 ↗
5. 10.1177/00405175760460091310.1177/004051757604600913 ↗
6. Müller K. · 1974
7. Pusch G. · Textilveredlung · 1967 · 2 · 416
8. Rebenfeld L. · 1969
9. Rüttiger W. · Melliand Textilber. · 1963 · 41 · 296