Abstract

We attempt to recover the surface properties of wool fibers damaged by physical and/or chemical treatment. For this purpose, two kinds of damaged wool fabric samples are prepared, one damaged by corona discharge treatment and the other oxidized with dichloroisocyanuric acid. We confirm that these treatments decrease the content of covalently bound fatty acids and change the fiber surface properties. To recover the surface properties of damaged wool, a fatty acid chloride, stearoyl chloride, is used to treat both damaged samples. The content of covalently bound fatty acids in treated samples recovers to some degree, and the surface characteristics of the treated wool fibers also recover from hydrophilic to hydrophobic. We also evaluate some mechanical properties with the KES-FB method, and we find they recover almost to the level of the original wool fabric sample.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Dyeing and Modifying Textile Fibers · Photopolymerization techniques and applications · Skin Protection and Aging

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Nippon Keori Co., Ltd., Funamoto, Yonedacho, Kakogawa, Hyogo 675-0053, Japan

Heian Jogakuin College, Nampeidai, Takatsuki, Osaka 569-1092, Japan

Kyoto Women's University, Imakumano, Higashiyamaku, Kyoto 605-0926, Japan

Matsue National College of Technology, Matsue, Shimane 690-0865, Japan

References (19)

Show source-provided references
1. 10.1177/00405175010710040510.1177/004051750107100405 ↗
2. Bereck, A. · Textilveredlung · 1996 · 31 · 241
3. Bereck, A. · Textilveredlung · 1997 · 32 · 135
4. 10.1177/00405175970670060810.1177/004051759706700608 ↗
5. 10.1016/0021-9797(91)90243-210.1016/0021-9797(91)90243-2 ↗
6. Ito, H. · J. Soc. Cosmet. Chem. · 1994 · 45 · 183
7. 10.1016/S0968-4328(97)00039-510.1016/S0968-4328(97)00039-5 ↗
8. 10.1002/app.1978.07022082110.1002/app.1978.070220821 ↗
9. Kawabata, S. · 1980
10. 10. Körner, A., Schmidt, H., Merten, T., Peters, S., Thomas, H., and Höcker, H., Changes in the Content of 18-Methylicosanoic Acid in Wool after UV-irradiation and Corona Treatment, in “Proc. 9th Int. Wool Text. Res. Conf., Biella,” vol. 2, 1995, pp. 414-419.
11. Leeder, J. D. · Wool Sci. Rev. · 1986 · 63 · 3
12. 10.1111/j.1478-4408.1985.tb00984.x10.1111/j.1478-4408.1985.tb00984.x ↗
13. 13. Leeder, J. D., Rippon, J. A., and Rivett, D. E., Modification of the Surface Properties of Wool by Treatment with Anhydrous Alkali, in “Proc. 7th Int. Wool Text. Res. Conf., Tokyo,” vol. IV, 1985, pp. 312-321.
14. 10.1177/00405175930630020710.1177/004051759306300207 ↗
15. 10.1177/00405175920620070310.1177/004051759206200703 ↗
16. 10.1111/j.1478-4408.1993.tb01579.x10.1111/j.1478-4408.1993.tb01579.x ↗
17. 10.1016/0021-9797(80)90333-110.1016/0021-9797(80)90333-1 ↗
18. Swift, J. A. · J. Cosmet. Sci. · 1999 · 50 · 23
19. 10.1002/andp.1863195060210.1002/andp.18631950602 ↗