A method is described for measuring lateral load-deformation relations of fibers. The results of tests on Lincoln wool fibers are given, for aqueous test liquids at pH 2.1, 6, and 9.1, and for fibers treated with formaldehyde, with an anionic detergent, and with mercuric acetate. In water at 20° C the shear modulus (for loading times of several seconds) is near to 2 X 10 8 dynes/cm 2 and does not vary greatly with the chemical treatment or the acidity of the test liquid. As the temperature increases, the shear modulus slowly decreases. At a certain temperature, approximately 80° C for this Lincoln wool in water, the modulus starts to decrease much more rapidly with temperature. This transition is accentuated and dis placed to lower temperatures at pH 9.1 or by the treatment with mercuric acetate. Measurements of viscous flow under constant load were also obtained. Between 70° and 100° C the native wool fibers show a viscosity of the order of 10 11 -10 12 poise, with an activation energy of about 26 kcl/mole. Some structural implications of these phenomena are discussed.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dyeing and Modifying Textile Fibers · Textile materials and evaluations · Collagen: Extraction and Characterization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Division of Textile Physics, C.S.I.R.O. Wool Research Laboratories, Ryde, Sydney, Australia
References (8)
Show source-provided references
1. 10.1177/00405175610310011210.1177/004051756103100112 ↗
2. 10.1149/1.242817410.1149/1.2428174 ↗
3. 10.1177/00405175640340110110.1177/004051756403401101 ↗
4. 10.1177/00405175640340121410.1177/004051756403401214 ↗
5. Mason, P., Textile Res. J. (submitted).
6. 10.1038/203484a010.1038/203484a0 ↗
7. 10.1063/1.171307610.1063/1.1713076 ↗
8. 10.1021/j100803a03810.1021/j100803a038 ↗