Load-Deformation Behavior of Wool at High Temperatures in Different Media
Source abstract
Abstract
Load-extension measurements were made on wool fibers and yams in steam, air at 100°C, and water at different tem peratures in the range 20-90°C. Samples were subjected to the action of steam, air at 100°C, and water at 90°C for different periods before being loaded in the respective media. It was found that for all three heating media, extensibility passed through a maximum value when wool was elongated in the process of heat absorption. Temperature-dependent transitions in water were found to be around 40° and 70°C for reduced wool. Load-extension measurements of wool in steam showed that the effect of crosslinking treatment can be seen, if comparison is made between the load-extension curves of crosslinked and pretreated wool and not between crosslinked and untreated wool.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Textile materials and evaluations · Dyeing and Modifying Textile Fibers
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Swedish Institute for Textile Research, Gothenburg 5, Sweden
References (8)
Show source-provided references
1. Astbury, W.T. · Phil. Trans. Proc. Roy. Soc · 1933 · 232 · 359
2. 10.1177/00405175590290040410.1177/004051755902900404 ↗
3. Mark, H. and Tobolsky, A.V. "Physical Chemistry of High Polymer Systems," New York , Interscience, 1950, p. 346.
4. 10.1177/00405175670370080510.1177/004051756703700805 ↗
5. Nordhammer, G. and Muhl, I., TEFO Reaearch Report 6, 14-16 (1970) (Swedish).
6. Peters, L. and Woods, H.J. "Mechanical Properties of Textile Fibers," Ed. Meredith, New York, North Holland, 1956, p. 180.
7. 10.1177/00405175720420010710.1177/004051757204200107 ↗
8. Weigmann, H-D. and Dansizer, C.J., Proc. 4th Int. Wool Text. Res. Conf., Part II, New York, Interscience , 795-807 (1971).