Characterization of (100)-oriented 0.63BiMg1/2Ti1/2O3–0.37PbTiO3 piezoelectric films by a sol–gel process
Source abstract
Abstract
Abstract 0.63BiMg 1/2 Ti 1/2 O 3 –0.37PbTiO 3 (BMT–PT) thin films with thickness of 600 nm were synthesized on Pt(111)/Ti/SiO 2 /Si(111) substrates. Highly (100) preferential orientation of the BMT–PT thin films was obtained by introducing lead oxide seeding layers. Saturated polarization hysteresis loops with low leakage current were observed, showing a remanent polarization of 24 μC/cm 2 and a coercive field of 54 kV/cm for the (100)-oriented BMT–PT thin films. The dielectric constant and loss for the thin films were 1060 and 0.06, respectively. The Curie temperature appeared at 415 °C. The local effective piezoelectric coefficient d 33 ⁎ was approximately 90 pm/V at zero volt for films with (100) preferential orientation, which was much higher than the value (~ 50 pm/V) obtained from films with random orientation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Multiferroics and related materials · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.