journal article·2019-10-02

Effect of Lanthanum Zirconate on High Temperature Resistance of Thermal Barrier Coatings

Le Wang, Yuelan Di, Haidou Wang, Xuehuan Li, Lihong Dong, Tao Liu

Publisher page

Abstract

Thermal barrier coatings (TBCs) typically have low thermal conductivity and high resistance to oxidation at elevated temperatures. TBCs are used to protect the turbine blades of aircraft engines operating at high temperature. The commonly used YSZ (8 wt% Y2O3-stabilized ZrO2) cannot function at temperatures higher than 1200°C for an extended period of time, which hinders the necessary improvement in the aircraft thrust-to-weight ratio. In this work, thermal barrier coatings consisting of a YSZ ceramic layer and of a lanthanum zirconate (LZ) + YSZ composite structure were prepared on a nickel-based high-temperature substrate using atmospheric plasma spraying. Thermal insulation properties and high temperature oxidation performance of TBCs with single layer structure and double layer structure were compared. The growth mechanism and influencing factors of high-temperature oxidation of thermally grown oxide (TGO) were discussed. The results showed that the LZ had good thermal insulation performance and oxygen isolation compared to the YSZ layer. This performance effectively reduces the growth of TGO in TBCs, thereby delaying the coating failure.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Mechatronics Engineering, Nanchang University, Nanchang 330031, China

National Key Laboratory for Remanufacturing, Academy of Army Armored Forces, Beijing 100072, China

School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300130, China

References (32)

Show source-provided references
1. N. P. Padture, M. Gell and E. H. Jordan, Science, 296, 280-284 (2002).
2. 10.1016/j.corsci.2018.06.03510.1016/j.corsci.2018.06.035 ↗
3. 10.1016/j.ceramint.2015.05.04910.1016/j.ceramint.2015.05.049 ↗
4. 10.1016/j.apsusc.2017.05.03010.1016/j.apsusc.2017.05.030 ↗
5. 10.1016/j.surfcoat.2017.07.05410.1016/j.surfcoat.2017.07.054 ↗
6. Meng M. Y. · Thermal Spray Technol. · 2015 · 7 · 30
7. 10.1016/j.molliq.2017.09.00110.1016/j.molliq.2017.09.001 ↗
8. 10.1016/j.jeurceramsoc.2012.08.02010.1016/j.jeurceramsoc.2012.08.020 ↗
9. 10.1007/s12613-017-1451-010.1007/s12613-017-1451-0 ↗
10. 10.1016/j.ceramint.2012.06.07710.1016/j.ceramint.2012.06.077 ↗
11. 10.1016/j.jeurceramsoc.2016.02.01110.1016/j.jeurceramsoc.2016.02.011 ↗
12. 10.1080/0371750X.2019.156602310.1080/0371750X.2019.1566023 ↗
13. 10.1016/j.surfcoat.2019.06.05610.1016/j.surfcoat.2019.06.056 ↗
14. 10.1080/0371750X.2016.121002410.1080/0371750X.2016.1210024 ↗
15. 10.1016/j.ceramint.2007.12.00210.1016/j.ceramint.2007.12.002 ↗
16. 10.1016/S0955-2219(03)00129-810.1016/S0955-2219(03)00129-8 ↗
17. 10.1080/0371750X.2019.157869510.1080/0371750X.2019.1578695 ↗
18. 10.1007/s10765-007-0232-910.1007/s10765-007-0232-9 ↗
19. 10.1016/j.corsci.2016.11.01510.1016/j.corsci.2016.11.015 ↗
20. 10.1016/j.ceramint.2016.11.11910.1016/j.ceramint.2016.11.119 ↗
21. 10.1016/j.ceramint.2017.11.12710.1016/j.ceramint.2017.11.127 ↗
22. 10.1016/S0167-2738(97)00198-710.1016/S0167-2738(97)00198-7 ↗
23. Si K. · Eng. Failure Anal. · 2017 · 27 · 150
24. 10.1016/j.surfcoat.2007.09.04210.1016/j.surfcoat.2007.09.042 ↗
25. 10.1016/j.matchar.2016.09.00610.1016/j.matchar.2016.09.006 ↗
26. 10.1016/j.jallcom.2015.05.29010.1016/j.jallcom.2015.05.290 ↗
27. 10.1016/j.jallcom.2008.09.16110.1016/j.jallcom.2008.09.161 ↗
28. 10.1016/j.jeurceramsoc.2015.11.01810.1016/j.jeurceramsoc.2015.11.018 ↗
29. 10.1016/j.ceramint.2017.12.11210.1016/j.ceramint.2017.12.112 ↗
30. 10.1016/j.ceramint.2011.12.07610.1016/j.ceramint.2011.12.076 ↗
31. Zhang W. F. · Coatings · 2018 · 8
32. 10.1016/j.vacuum.2016.09.01210.1016/j.vacuum.2016.09.012 ↗