Abstract

Abstract Glasses with nominal composition (mol%) 34BaO-10Al2O3-17B2O3-34SiO2-(5-x)La2O3-xTiO2 (x = 0, 1, 2, 3, 4) were prepared by melt quenching technique. Activation energy of crystallization (Ea ) was calculated by Kissinger's model considering the shift in peak crystallization temperature (Tc ) at three different heating rates (10°, 15° and 20°C.min−1) in differential thermal analysis. Among the glasses studied, composition with x = 1 had the maximum Ea as a result of its slower crystallization rate. Thermal expansion coefficients of as prepared bulk glasses matched with that of Crofer 22APU alloy. Sandwich type seals were made with two Crofer plates at 990°C and their vacuum integrity was tested at room temperature. Cross-sectional interface of the seals was studied under scanning electron microscope with energy dispersive X-ray analysis. Very different morphology at metal to glass-ceramics interface was observed with varying TiO2 concentration. Microstructure at the interface of the seal with x = 1 glass had less porosity and less chromium enrichment at the interface than the other compositions which was probably due to slower rate of crystallization during the heat treatment. Keywords: GlassGlass-ceramicsCrystallization kineticsHigh temperature sealant
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Glass properties and applications · Advanced ceramic materials synthesis · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Fergus J. W. · J. Power Sources · 2005 · 147 · 4610.1016/j.jpowsour.2005.05.002 ↗
2. Mahapatra M. K. · J. Power Sources · 2010 · 195 · 712910.1016/j.jpowsour.2010.06.003 ↗
3. Menzler N. H. · J. Power Sources · 2005 · 152 · 15610.1016/j.jpowsour.2005.02.072 ↗
4. Meinhardt K. D. · J. Power Sources · 2008 · 182 · 18810.1016/j.jpowsour.2008.03.079 ↗
5. Sohn S. · J. Non-Cryst. Solids · 2002 · 297 · 10310.1016/S0022-3093(01)01042-0 ↗
6. Minquan W. · J. Non-Cryst. Solids · 1986 · 80 · 37910.1016/0022-3093(86)90420-5 ↗
7. Ghosh S. · J. Eur. Ceram. Soc. · 2008 · 28 · 6910.1016/j.jeurceramsoc.2007.05.008 ↗
8. Ghosh S. · Int. J. Hydrogen Energy · 2010 · 35 · 27210.1016/j.ijhydene.2009.10.006 ↗
9. Sun T. · Ceram. Int. · 2010 · 36 · 82110.1016/j.ceramint.2009.09.045 ↗
10. Lin S. · J. Eur. Ceram. Soc. · 2011 · 31 · 197510.1016/j.jeurceramsoc.2011.04.017 ↗
11. Tiwari B. · Int. J. Hydrogen Energy · 2011 · 36 · 1500210.1016/j.ijhydene.2011.04.018 ↗
12. Mahapatra M. K. · J. Power Sources · 2010 · 195 · 712910.1016/j.jpowsour.2010.06.003 ↗
13. Donald I. W. · J. Non-Cryst. Solids · 2008 · 354 · 30110.1016/j.jnoncrysol.2007.06.102 ↗
14. Tiwari B. · J. Am. Ceram. Soc. · 2011 · 9 · 144010.1111/j.1551-2916.2010.04292.x ↗
15. Kissinger H. E. · J. Res. Natl. Bureau Stand. · 1956 · 57 · 21710.6028/jres.057.026 ↗