journal article·1981-01

Studies on Eutectic Liquid Sintering of Zirconium Dioxide

A. Naik, G. N. Agrawal, V. C. Joshi

Publisher page

Abstract

AbstractInvestigations were carried out on eutectic sintering of zirconium dioxide powder (–45μ particle size, calcined at 1000°C for 1 hour) with tri-component eutectics. An intimate mixture of the eutectics from the CaO-Al2O3-SiO2 and MgO-Al2O3-SiO2 compositions was prepared at 1350° and 1400°C respectively. It was then powdered and sieved to–45μ particle size. Pellets of ZrO2 were prepared at 15 tons/inch sq with varying amount of eutectic mixtures (0.05% to 0.25% by weight), and sintered at temperatures 1150°, 1250°, 1350° and 1450°C with different soaking periods ranging from 10 to 300 minutes. The data obtained were analysed using the empirical equations (i) D = k log t + C and (ii) ΔL/L0 = Ktn. The shrinkage data were analysed to understand the mechanism of sintering. The study revealed that ZrO2 pellets of specified density and grain development could be obtained by making a suitable choice of the additive and varying its content.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Injection Molding Process and Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (7)

Show source-provided references
1. Vornonin N. I. · Ogneupory · 1963 · 1 · 30
2. Moorthy V. K. · Trans. Ind. Ceram. Soc. · 1968 · 27 · 1610.1080/0371750X.1968.10855626 ↗
3. Moorthy V. K. · Trans. Ind. Ceram. Soc. · 1965 · 24 · 10310.1080/0371750X.1965.10855525 ↗
4. Kingery W. D. · J. Appl. Phys. · 1959 · 30 · 30110.1063/1.1735155 ↗
5. Kingery W. D. · J. Amer. Ceram. Soc. · 1961 · 44 · 2910.1111/j.1151-2916.1961.tb15343.x ↗
6. Bhargava A. K. · Ind. Ceram. · 1977 · 20 · 115
7. Levin E. M. · 1956