Ballistic Resistance of Silicon-Carbide-Based Ceramic and Ultrahigh-Molecular-Weight Polyethylene Composite Armor
Source abstract
Abstract
In this study, the ballistic resistance of SiC (silicon carbide) and a SiC mixture S80B20 (80% SiC/20% B4C) backed with UHMWPE (ultra-high-molecular-weight-polyethylene) fiber board was investigated by striking it with a .30-06 armor piercing projectile. The front plate of the high hardness ceramics is intended to passivate the bullet and limit the bullet’s impact kinetic energy, and the high strength backing plate undergoes plastic deformation, absorbing the bullet’s residual energy. Ballistic tests revealed that an 8 mm thick S80B20 ceramics produced at a sintering temperature of 2120° or 2140°C, combined with a composite plate, can successfully resist .30-06 armorpiercing rounds with energy greater than 3900 J. The optimal SiC plate meeting the NIJ 0101.06 Level IV was an 8 mm thick SiC sheet backed with 9 mm of fiber board (total thickness, 17 mm; areal density, 33.217 g/m2). The 8 mm thick 80% SiC/20% B4C plate sintered at 2120°C, backed with 7 mm fiber board, had an areal density of only 29.615 kg/m2. If the depth of penetration is less than 44 mm, the fiber board thickness must be increased from 7 to 8 mm, increasing the areal density to 30.552 kg/m2. Compared with the SiC ballistic plate, the density of the composite is 2.665 kg/m2 lower.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Energetic Materials and Combustion · High-Velocity Impact and Material Behavior · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Power Vehicle and Systems Engineering, CCIT, National Defense University, Taoyuan City, 33551, Taiwan
Department of Textile Engineering, College of Engineering, Chinese Culture University, Taipei City, 11114, Taiwan
Funding
Ministry of Science and Technology, Taiwan · National Chung-Shan Institute of Science
References (28)
Show source-provided references
1. S. Sun, B. Zhao, J. Wang, Z. Wang and R. Bai, Ordna. Mat. Sci. Eng., 2, 70-72(2006).
2. 10.1007/s41779-020-00516-710.1007/s41779-020-00516-7 ↗
3. J. J. Swab, Int. J. App. Ceram. Tec., 1, 1-17 (2004).
4. 10.1016/j.dt.2019.02.00210.1016/j.dt.2019.02.002 ↗
5. R. K. Lenka, P. K. Patro and T. Mahata, Handbook on Synthesis Strategies for Advanced Materials, Volume-II: Processing and Functionalization of Materials, pp. 1-54, Springer Nature, Basel, Switzerland (2022).
6. 10.1016/j.dt.2021.10.00310.1016/j.dt.2021.10.003 ↗
7. P. Wang “Research on the Anti-Elastic Performance of Silicon Carbide Ceramics” Master Thesis Nanjing University of Science and Technology Nanjing China (2012).
8. 10.1177/00219983940280130210.1177/002199839402801302 ↗
9. 10.1016/j.compstruct.2010.08.02510.1016/j.compstruct.2010.08.025 ↗
10. 10.1179/174367610X1280479263534110.1179/174367610X12804792635341 ↗
11. H. H. Yang, Kevlar Aramid Fiber, Chapter 5, pp.119-140, John Wiley & Sons, NY, USA (1993).
12. 10.1016/j.ceramint.2019.04.25110.1016/j.ceramint.2019.04.251 ↗
13. K. K. Wu, Y. L. Chen, J. N. Yeh, W. L. Chen and C. S. Lin, Adv. Mater. Sci. Eng., 2, 1-9 (2020).
14. https://nij.ojp.gov/library/publications/ballistic-resistantprotective-materials-nij-standard-010801
15. https://www.ojp.gov/pdffiles1/nij/223054.pdf.
16. 10.1016/0015-0568(80)90011-110.1016/0015-0568(80)90011-1 ↗
17. http://everyspec.com/MIL-STD/MIL-STD-0500-0699/MILSTD-662F_6718
18. K. Sairamentitled, G. Guo, S. Alam and L. D. Peel, Compos. Part C: Open Access (JCOMC), 2, 385-395 (2020).
19. 10.1063/1.146890310.1063/1.1468903 ↗
20. ASTM E384 A “Vickers Hardness Test Method” A Standard Test Method for Micro Indentation Hardness of Materials ASTM International West Conshohocken PA (2020).
21. J. C. L. LaSalvia S. Kirihar and S. Widjaja “Advances in Ceramic Armor IX ” pp.1-122 in: A Collection of Papers Presented at the 37th International Conference on Advanced Ceramics and Composites 34 Florida USA (2013).
22. 10.1177/030932471245499610.1177/0309324712454996 ↗
23. 10.1179/095066009X1250672166521110.1179/095066009X12506721665211 ↗
24. 10.1111/j.1744-7402.2010.02501.x10.1111/j.1744-7402.2010.02501.x ↗
25. 10.1016/j.dt.2019.06.02010.1016/j.dt.2019.06.020 ↗
26. 10.1515/aucts-2017-002110.1515/aucts-2017-0021 ↗
27. T. Williams “Development of Pressureless Sintered Silicon Carbide-Boron Carbide Composites for Armour Applications” pp. 82-144 PhD Dissertation Engineering doctorate (micro and nano materials) University of Surrey South East of England (2016).
28. 10.1016/S0734-743X(98)00036-010.1016/S0734-743X(98)00036-0 ↗