Optimisation of process parameters and characterisation of composite ceramic coating with NaF additive on Ti-3Zr-2Sn-3Mo-25Nb by micro-arc oxidation

Mei Yang, Wenhao Zhang, Yang Li, Xiufang Gong, Liping Nie, Jingxiang Lu, Ning Tang, Pengcheng Li

Transactions of the IMF· Volume 98· Issue 6
Publisher page

Abstract

Ceramic coatings containing calcium and phosphorus were prepared on the surface of Ti-3Zr-2Sn-3Mo-25Nb by micro-arc oxidation. The effects of Ca/P ratio, oxidation time, current density and duty ratio on the coating were studied by orthogonal experiment under a phosphate electrolyte to determine the optimal process parameters. To analyse the effects of NaF additions, 1 g L−1, 2 g L−1, 3 g L−1, 4 g L−1 and 5 g L−1 NaF were added into the electrolyte, respectively. From analysis, the authors draw the following conclusions: NaF can improve the conductivity of electrolyte and facilitate the densification of coating; the hardness, thickness and roughness of the coating have been improved to some extent; the most obvious improvement to the coating is effected by adding 3 g L−1 NaF into the electrolyte. Furthermore, passivation has occurred on the MAO-NaF-coatings immersed in simulated body fluids. The most improved corrosion resistance of the MAO-oxidation coating is gained by adding 3 g L−1.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials Science and Engineering, Southwest Petroleum University, Chengdu, People’s Republic of China

Sichuan Petroleum Enginering Construction Co., Ltd, Chengdu, People’s Republic of China

State Key Laboratory of Long-life High Temperature Materials, Dong Fang Turbine Co., Ltd., Deyang, People’s Republic of China

References (22)

Show source-provided references
1. 10.1016/j.matchemphys.2004.10.02510.1016/j.matchemphys.2004.10.025 ↗
2. Luo Y. · 2013
3. 10.20964/2019.09.0910.20964/2019.09.09 ↗
4. 10.1108/PRT-06-2018-005410.1108/PRT-06-2018-0054 ↗
5. 10.1016/j.biomaterials.2003.09.04810.1016/j.biomaterials.2003.09.048 ↗
6. 10.1016/j.apsusc.2012.11.07410.1016/j.apsusc.2012.11.074 ↗
7. Min K.-K. · Korean J. Dent. Mater. · 2013 · 40 · 103
8. 10.1002/jbm.82021120310.1002/jbm.820211203 ↗
9. 10.1016/j.jmst.2012.12.01510.1016/j.jmst.2012.12.015 ↗
10. 10.1016/j.apsusc.2014.10.14510.1016/j.apsusc.2014.10.145 ↗
11. 10.1016/j.apsusc.2015.03.05110.1016/j.apsusc.2015.03.051 ↗
12. 10.1016/j.ceramint.2014.12.13410.1016/j.ceramint.2014.12.134 ↗
13. Wang Y. · Sci. Technol. · 2014 · 30 · 984
14. 10.1016/j.msea.2011.06.03210.1016/j.msea.2011.06.032 ↗
15. Tang N. · 2020
16. Ma X.-Q. · Chinese J. Nonferrous Metals · 2019 · 29 · 74
17. 10.1080/00202967.2018.150250610.1080/00202967.2018.1502506 ↗
18. Yang M. · Rare Metal Mater. Eng. · 2020 · 49 · 0404
19. 10.1016/j.surfcoat.2007.04.12410.1016/j.surfcoat.2007.04.124 ↗
20. Guo X. · Chinese Ceramics · 2016 · 52 · 44
21. 10.1016/j.biomaterials.2003.09.10310.1016/j.biomaterials.2003.09.103 ↗
22. 10.1016/j.corsci.2009.10.01610.1016/j.corsci.2009.10.016 ↗