Formation and dielectric breakdown behaviour of plasma electrolytic oxidation film formed on AA6061 using pulsed current at various cathodic-to-anodic current density ratios
Source abstract
Abstract
The formation and dielectric breakdown behaviour of plasma electrolytic oxidation (PEO) films on 6061 aluminium alloy (AA6061) using pulsed current were investigated under varying cathodic-to-anodic current density ratios (jc/ja). This study systematically examined the effects of jc/ja on arc generation behaviour, PEO film morphology and dielectric breakdown characteristics. When jc/ja ≤ 0.5, the PEO films exhibited large pores (10–80 μm), resulting in reduced dielectric strength. Optimal performance was achieved at jc/ja = 1.2, where the PEO films demonstrated the highest growth rate of 1.72 μm min−1, a denser structure and superior dielectric breakdown voltage. However, at jc/ja ≥ 1.5, the films exhibited multiple cracks, non-uniform thickness and reduced dielectric breakdown voltage. The decrease in dielectric breakdown voltages at jc/ja < 1 and jc/ja ≥ 1.5 is attributed to the presence of large pores and cracks within the PEO films, respectively.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Korea Institute of Materials Science
Pusan National University
Korea University of Science and Technology
Funding
Institute of Materials Science
References (25)
Show source-provided references
1. 10.1016/j.surfcoat.2022.12869210.1016/j.surfcoat.2022.128692 ↗
2. 10.1016/j.mlblux.2019.10001610.1016/j.mlblux.2019.100016 ↗
3. 10.1016/j.surfcoat.2023.12986110.1016/j.surfcoat.2023.129861 ↗
4. 10.1016/j.surfcoat.2024.13088110.1016/j.surfcoat.2024.130881 ↗
5. 10.1016/j.apsusc.2023.15778910.1016/j.apsusc.2023.157789 ↗
6. 10.1016/j.ceramint.2018.10.08310.1016/j.ceramint.2018.10.083 ↗
7. 10.1016/j.apsusc.2019.05.25010.1016/j.apsusc.2019.05.250 ↗
8. 10.1016/j.pmatsci.2020.10073510.1016/j.pmatsci.2020.100735 ↗
9. 10.1016/j.ceramint.2024.05.28810.1016/j.ceramint.2024.05.288 ↗
10. 10.3390/coatings1402021710.3390/coatings14020217 ↗
11. 10.1016/j.corsci.2020.10906510.1016/j.corsci.2020.109065 ↗
12. 10.1016/j.surfcoat.2017.05.06810.1016/j.surfcoat.2017.05.068 ↗
13. 10.1016/j.jma.2017.02.00410.1016/j.jma.2017.02.004 ↗
14. 10.1016/j.surfcoat.2023.13003010.1016/j.surfcoat.2023.130030 ↗
15. 10.1016/j.surfcoat.2022.12809910.1016/j.surfcoat.2022.128099 ↗
16. 10.1149/1945-7111/ac82cc10.1149/1945-7111/ac82cc ↗
17. 10.1016/j.ceramint.2023.08.17810.1016/j.ceramint.2023.08.178 ↗
18. 10.1016/j.electacta.2009.02.00410.1016/j.electacta.2009.02.004 ↗
19. 10.1016/j.apsusc.2014.08.08110.1016/j.apsusc.2014.08.081 ↗
20. 10.1016/j.jma.2020.05.00110.1016/j.jma.2020.05.001 ↗
21. 10.1016/j.ceramint.2021.06.13710.1016/j.ceramint.2021.06.137 ↗
22. 10.1016/j.surfcoat.2015.07.07510.1016/j.surfcoat.2015.07.075 ↗
23. 10.1016/j.corsci.2018.08.03710.1016/j.corsci.2018.08.037 ↗
24. 10.1016/j.surfcoat.2018.02.04210.1016/j.surfcoat.2018.02.042 ↗
25. 10.2478/amm-2014-007010.2478/amm-2014-0070 ↗