journal article·2011-07

Influence of hydrogen on room temperature recrystallisation of electrodeposited Cu films: thermal desorption spectroscopy

N Fukumuro, T Adachi, S Yae, H Matsuda, Y Fukai

Transactions of the IMF· Volume 89· Issue 4
Publisher page

Abstract

The mechanism of recrystallisation observed at room temperature in electrodeposited Cu films has been examined in light of the enhancement of metal atom diffusion by hydrogen induced superabundant vacancies. Thermal desorption spectroscopy revealed that Cu films electrodeposited from acid sulphate bath containing some specific additives showed a pronounced peak, which was ascribed to the break-up of vacancy–hydrogen clusters. The amount of desorbed hydrogen was comparable to that of vacancy type clusters estimated in previous positron annihilation experiments. The grain size of Cu films increased as hydrogen desorption proceeded. Such grain growths were not observed in the films deposited from the baths without additives. These results indicate that the room temperature recrystallisation of electrodeposited Cu films is caused by hydrogen induced superabundant vacancies.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Copper Interconnects and Reliability · Nanomaterials and Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. 10.1147/rd.425.056710.1147/rd.425.0567 ↗
2. 10.1149/1.139090410.1149/1.1390904 ↗
3. 10.1149/1.137663610.1149/1.1376636 ↗
4. 10.1149/1.305427310.1149/1.3054273 ↗
5. 10.1179/174591910X1269257643457210.1179/174591910X12692576434572 ↗
6. 10.1179/174591910X1269271139039010.1179/174591910X12692711390390 ↗
7. 10.1179/002029610X1279198150788410.1179/002029610X12791981507884 ↗
8. 10.1149/1.157559210.1149/1.1575592 ↗
9. 10.1149/1.214929910.1149/1.2149299 ↗
10. 10.4139/sfj.59.69610.4139/sfj.59.696 ↗
11. 10.1149/1.240072510.1149/1.2400725 ↗
12. Nakahara S · Electrochem. Solid-State Lett. · 2007 · 154 · D145
13. 10.2320/jinstmet.70.11810.2320/jinstmet.70.118 ↗
14. 10.1063/1.200981310.1063/1.2009813 ↗
15. 10.1063/1.287449710.1063/1.2874497 ↗
16. 10.1016/S0925-8388(02)01269-010.1016/S0925-8388(02)01269-0 ↗
17. 10.1238/Physica.Topical.103a0001110.1238/Physica.Topical.103a00011 ↗
18. Fukai Y: ‘The metal-hydrogen system, basic bulk properties’, 2nd edn, Chap. 5; 2005, Heidelberg, Springer.10.1007/3-540-28883-X ↗
19. 10.1016/S0925-8388(02)01270-710.1016/S0925-8388(02)01270-7 ↗
20. 10.1088/0953-8984/16/8/01710.1088/0953-8984/16/8/017 ↗
21. 10.1016/j.actamat.2005.02.04910.1016/j.actamat.2005.02.049 ↗