Effect of plating time on electrodeposition of thick nanocrystalline permalloy foils
Source abstract
Abstract
Thick foils of nanostructured permalloy were electrodeposited by applying a current density of 100 mA cm−2 for 48 hours. The bath contained nickel sulphate, iron sulphate, a complex agent, a grain refiner, a stress reducing agent, a buffer and a wetting agent. The bath pH was 3·8. Different parameters were controlled to get thick (approximately 860 µm), uniform permalloy coatings. To investigate the effect of electroplating time on the surface morphology, thickness and structure of foils, scanning electron microscopy, optical microscopy and X-ray diffraction were used. Chemical compositions of foils and the bath were investigated by quantometry and ultra violet–visible spectroscopy. The composition of the coatings was constant during the long period of electroplating, which was attributed to the bath stability. The cathode current efficiency of the electroplated permalloy foils increased slightly on increasing the plating time. Existence of chloride ions, complex agent and saccharin in the bath influenced efficiency.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Electrochemical Analysis and Applications · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Engineering, School of Engineering, Shiraz University, Zand Blvd., Shiraz 7134851154, Iran
References (37)
Show source-provided references
1. 10.1103/PhysRevB.66.01441610.1103/PhysRevB.66.014416 ↗
2. 10.1149/1.139178110.1149/1.1391781 ↗
3. 10.1149/1.208623110.1149/1.2086231 ↗
4. 10.1179/002029605X2940110.1179/002029605X29401 ↗
5. 10.1179/174591909X1255433231154610.1179/174591909X12554332311546 ↗
6. W. H. Safranek: ‘The properties of electrodeposited metals and alloys: a handbook’, 2nd edn, 335–345; 1986, Orlando, FL, American Electroplaters and Surface Finishers Soc.
7. 10.1149/1.240752410.1149/1.2407524 ↗
8. 10.1109/84.80905210.1109/84.809052 ↗
9. 10.1016/B978-1-4831-9808-8.50016-210.1016/B978-1-4831-9808-8.50016-2 ↗
10. 10.1016/j.cap.2013.01.03210.1016/j.cap.2013.01.032 ↗
11. 10.1016/0013-4686(89)87158-010.1016/0013-4686(89)87158-0 ↗
12. 10.1179/0020296713Z.00000000011510.1179/0020296713Z.000000000115 ↗
13. 10.1179/174591911X1316516122828610.1179/174591911X13165161228286 ↗
14. 10.1149/1.242793410.1149/1.2427934 ↗
15. Lin K. · J. Electrochem. Soc. · 1995 · 95 · 626
16. 10.1149/1.275325210.1149/1.2753252 ↗
17. 10.1016/j.jallcom.2004.09.02410.1016/j.jallcom.2004.09.024 ↗
18. 10.1016/j.surfcoat.2004.11.03510.1016/j.surfcoat.2004.11.035 ↗
19. 10.1149/1.212881610.1149/1.2128816 ↗
20. 10.1016/0013-4686(64)85009-X10.1016/0013-4686(64)85009-X ↗
21. Namboodiri P. N. N. · Trans. SAEST · 1972 · 7 · 122
22. 10.1007/BF0061693910.1007/BF00616939 ↗
23. Mallory G. O. · 1996
24. 10.1016/j.jallcom.2006.01.10510.1016/j.jallcom.2006.01.105 ↗
25. 10.1016/j.matchar.2005.12.01610.1016/j.matchar.2005.12.016 ↗
26. 10.1016/S0013-4686(03)00380-310.1016/S0013-4686(03)00380-3 ↗
27. Liu W. · GCA · 2012 · 94 · 276
28. 10.2320/matertrans.M201229210.2320/matertrans.M2012292 ↗
29. 10.1016/j.intermet.2010.02.02610.1016/j.intermet.2010.02.026 ↗
30. Abdel-Karim R. · JNM · 2011 · 2011 · 1
31. 10.1088/1674-1056/19/8/08680210.1088/1674-1056/19/8/086802 ↗
32. 10.1155/TSM.14-18.75710.1155/TSM.14-18.757 ↗
33. 10.1103/PhysRevB.51.198510.1103/PhysRevB.51.1985 ↗
34. Vasucievan R. · Met. Finish. · 1992 · 90 · 23
35. Mallory G. O. · 1990
36. 10.1149/1.212738510.1149/1.2127385 ↗
37. 10.1016/S0254-0584(03)00316-X10.1016/S0254-0584(03)00316-X ↗