Further Results with New Metal-Pigmented Paints
Source abstract
Abstract
SummaryTests have been carried out: (1) on panels of painted steel carrying mill-scale interrupted by scratches and carrying various salts shut in below the paint, exposed (a) over water for 1–4 months, (6) on a roof at Cambridge for 13–26 months; (2) on aluminium alloy specimens with a bare square and scratch-line partly immersed in seawater or sodium chloride at 25°C; (3) on steel panels exposed at Aden for 4 months before painting and 18 months subsequently, with a scratch-line through the paint. In all cases, metal-pigmented paints behaved better than others, and at Aden the best result was shown by one of the new paints pigmented with metallic zinc, cadmium and aluminium along with barium and calcium phosphates, covered with ‘traffic blue ‘ (DEF 1044). In some of the tests at Cambridge, zinc-rich polystyrene (without cadmium, aluminium or phosphates) behaved as well or better than the new paints.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Cultural Heritage Materials Analysis · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (5)
Show source-provided references
1. Evans U. R. · Trans Inst Met Finishing · 1962 · 39 · 18810.1080/00202967.1962.11879208 ↗
2. 10.1002/jctb.500049142410.1002/jctb.5000491424 ↗
3. Mayne J. E. O. · J Oil Colour Chem Assoc · 1957 · 40 · 185
4. 10.1080/00202967.1959.1186976410.1080/00202967.1959.11869764 ↗
5. 10.1002/jctb.500047101110.1002/jctb.5000471011 ↗