journal article·1988-01

Chloride pitting of electroless nickel coatings

A. P. van Gool, P. J. Boden, S. J. Harris

Transactions of the IMF· Volume 66· Issue 1
Publisher page

Abstract

SummaryA study has been made of the pitting corrosion of an electroless nickel coating produced from a heavy metal-organic thiocompound stabilised bath. The deposit was immersed as part of a rotating disc electrode in an oxygenated 3% sodium chloride solution at a series of temperatures in the range 25–80°C. The aggressive conditions at 60°C revealed that pitting attack at numerous sites had begun within a period of 9h and that rapid penetration (20h) of the coating had taken place up to a depth of 12μm. Beyond this stage, pits grew in depth and radially at a slower pace. A 25μm thick coating remained intact up to 360h. At lower temperatures (<40°C) and lower chloride concentrations it is suggested that pitting attack will occur at a much reduced rate but detailed investigation on the kinetics under these conditions remains to be carried out.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Electrodeposition and Electroless Coatings

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (3)

Show source-provided references
1. 10.1080/00202967.1984.1187069110.1080/00202967.1984.11870691 ↗
2. 10.1179/00070598679827224410.1179/000705986798272244 ↗
3. 10.1080/00202967.1987.1187078210.1080/00202967.1987.11870782 ↗