Initiation of nodules from small protrusions in electroless Ni–P films
Source abstract
Abstract
Electroless nickel – phosphorus (Ni–P) underlayers in electroless nickel/immersion gold (ENIG) finishes can develop nodules that impair reliability. The authors investigated nodule initiation in electroless Ni–P on Cu activated by a Pd catalyst method or by an Fe contact method (Pd-free, Cu reference). Films were characterised by SEM, 3D-SEM/FIB, and cross-sectional STEM/EDS. Early-stage nodules were far more numerous on Pd-activated films. Late-stage nodules were less distinct. Cross-sectional STEM/EDS revealed ∼50–100 nm protruding Pd aggregates at the Cu surface directly beneath early-stage nodules and showed an increased EDS P signal throughout the nodule (apparent phosphorus enrichment). Nodules also initiated at micrometre-scale residues and mechanically formed asperities, whereas regions bearing only an ultrathin, smooth Pd layer did not yield nodules in this study’s observations. These results suggest an observation-based protrusion size scale ≥50 nm; suppressing such protrusions may mitigate nodules and may decrease Pd consumption.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Copper Interconnects and Reliability · Nanoporous metals and alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Kanto Gakuin University
SILVEC Co., Ltd.
JEOL Ltd.
References (28)
Show source-provided references
1. 10.3390/ma1618611610.3390/ma16186116 ↗
2. 10.1007/s40735-021-00568-710.1007/s40735-021-00568-7 ↗
3. G. O. Mallory and J. B. Hajdu (eds): ‘Electroless Plating: Fundamentals and Applications’, 207–227; 1990, Orlando, FL, AESF.
4. R. Parkinson: Properties and applications of electroless nickel. Nickel Dev. Inst.Tech. Ser., 1997, 10081, 1–37.
5. 10.1080/1478422X.2022.209632210.1080/1478422X.2022.2096322 ↗
6. 10.1007/s11664-007-0360-910.1007/s11664-007-0360-9 ↗
7. 10.1039/D1RA07952B10.1039/D1RA07952B ↗
8. 10.1016/j.matchemphys.2005.10.00110.1016/j.matchemphys.2005.10.001 ↗
9. 10.4139/sfj.42.30310.4139/sfj.42.303 ↗
10. 10.1007/s11664-018-6335-110.1007/s11664-018-6335-1 ↗
11. S. A. Armyanov: Electroless nickel-phosphorus deposition on aluminum: Interface and internal stress. Met. Finish., 1992, 90, 36–41.
12. 10.1016/j.triboint.2019.06.03110.1016/j.triboint.2019.06.031 ↗
13. 10.4139/sfj.56.46310.4139/sfj.56.463 ↗
14. 10.1007/s11661-015-2892-610.1007/s11661-015-2892-6 ↗
15. 10.1016/j.surfcoat.2024.13117410.1016/j.surfcoat.2024.131174 ↗
16. 10.1007/s10854-024-14149-010.1007/s10854-024-14149-0 ↗
17. 10.4139/sfj.47.34910.4139/sfj.47.349 ↗
18. 10.5104/jiep.5.35910.5104/jiep.5.359 ↗
19. 10.4139/sfj.60.66110.4139/sfj.60.661 ↗
20. 10.30509/pccc.2010.7576610.30509/pccc.2010.75766 ↗
21. 10.1149/2.088202jes10.1149/2.088202jes ↗
22. 10.1007/s10853-023-08281-110.1007/s10853-023-08281-1 ↗
23. 10.4139/sfj.75.18510.4139/sfj.75.185 ↗
24. G. O. Mallory and J. B. Hajdu (eds): ‘Electroless plating: fundamentals and applications’, 58–59; 1990, Orlando, FL, AESF.
25. N. K. Dirjal, K. A. Holbrook and P. B. Wells: The role of electroless plating bath constituents in the catalytic oxidation of the hypophosphite ion. Plat. Surf. Finish., 1998, 85(4), 74–78.
26. 10.1149/1.362378210.1149/1.3623782 ↗
27. 10.1016/j.electacta.2006.05.01710.1016/j.electacta.2006.05.017 ↗
28. 10.1002/1616-3028(200110)10.1002/1616-3028(200110) ↗