journal article·2025-01

Ni and Sb improve the microstructure, mechanical properties, and solder joint reliability of Sn-3.0Ag-0.5Cu alloy

Biao Wang, Jikang Yan, Jiangshan Liu, Jianhua Zhao, Lingyan Zhao

Vacuum· Volume 231
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Low-temperature creep of SnPb and SnAgCu solder alloys and reliability prediction in electronic packaging modules10.1016/j.scriptamat.2012.12.017 ↗
2. Time- and temperature-dependent wetting behavior of eutectic SnPb on Cu leadframes plated with Pd/Ni and Au/Pd/Ni thin films10.1063/1.368136 ↗
3. Effect of graphene nanosheets reinforcement on the performance of Sn Ag Cu lead-free solder10.1016/j.msea.2012.10.079 ↗
4. Effects of Ga addition on microstructure and properties of Sn–Ag–Cu/Cu solder joints10.1016/j.jallcom.2014.11.030 ↗
5. High-reliability low-Ag-content Sn-Ag-Cu solder joints for electronics applications10.1007/s11664-012-2145-z ↗
6. Effects of Ag content on the interfacial reactions between liquid Sn–Ag–Cu solders and Cu substrates during soldering10.1016/j.jallcom.2016.03.177 ↗
7. Reaction properties and interfacial intermetallics for Sn-xAg-0.5Cu solders as a function of Ag content10.3365/met.mat.2008.10.649 ↗
8. Coupling effects of rare-earth Pr and Al2O3 nanoparticles on the microstructure and properties of Sn-0.3Ag-0.7Cu low-Ag solder10.1016/j.jallcom.2019.01.034 ↗
9. Effect of alloying elements on properties and microstructures of SnAgCu solders10.1016/j.mee.2010.04.007 ↗
10. Structural analysis of SAC solder with Bi addition
11. Enhancing the ductility and mechanical behavior of Sn-1.0Ag-0.5Cu lead-free solder by adding trace amount of elements Ni and Sb10.1016/j.microrel.2018.06.015 ↗
12. Controlling Ag3Sn plate formation and its effect on the creep resistance of Sn–3.0Ag–0.7Cu lead-free solder by adding minor alloying elements Fe, Co, Te and Bi10.1007/s12540-020-00856-w ↗
13. Thermal, microstructural, wettability and mechanical properties of Sn1.0Ag0.5Cu composite solder modified with Ti nanoparticles10.1016/j.matchar.2024.113927 ↗
14. Enhancing performance of Sn–Ag–Cu alloy through germanium additions: investigating microstructure, thermal characteristics, and mechanical properties
15. Microstructure, mechanical properties, and interfacial reaction with Cu substrate of Zr-modified SAC305 solder alloy10.1016/j.jallcom.2018.12.098 ↗
16. Tensile creep characteristics of Sn–3.5Ag–0.5Cu (SAC355) solder reinforced with nano-metric ZnO particles10.1016/j.msea.2014.02.061 ↗
17. Nanocomposite SAC solders: the effect of adding CoPd nanoparticles on the morphology and the shear strength of the Sn–3.0Ag–0.5Cu/Cu solder joints10.1007/s13204-020-01325-x ↗
18. Effect of γ-Fe2O3 nanoparticles size on the properties of Sn-1.0Ag–0.5Cu nano-composite solders and joints10.1016/j.jallcom.2015.11.213 ↗
19. Improvement of heat aging resistance and tensile strength of SAC305/Cu solder joints by multi-element microalloying10.1016/j.intermet.2024.108428 ↗
20. Influence of Fe and Ho additions on Sn-3.0Ag-0.5Cu solder alloy: microstructure, electrochemical and mechanical properties10.1016/j.matchar.2023.113307 ↗
21. The influence of Ni and Zn additions on microstructure and phase transformations in Sn–0.7Cu/Cu solder joints10.1016/j.actamat.2014.10.003 ↗
22. Interfacial microstructure, shear strength and wettability of Ni-added Sn-0.3Ag-0.7Cu/Cu solder joint10.1007/s10854-023-11911-8 ↗
23. Improved creep resistance and thermal behavior of Ni-doped Sn–3.0Ag–0.5Cu lead-free solder10.1016/j.jallcom.2013.10.148 ↗
24. Effect of Ce and Sb doping on microstructure and thermal/mechanical properties of Sn-110.1108/SSMT-08-2023-0044 ↗
25. Microstructure, mechanical properties, and deformation behavior of Sn–1.0Ag–0.5Cu solder after Ni and Sb additions10.1016/j.matdes.2012.06.058 ↗
26. The microstructure, thermal, and mechanical properties of Sn-3.0Ag-0.5Cu-xSb high-temperature lead-free solder10.3390/ma13194443 ↗
27. Effects of antimony on the microstructure, thermal properties, mechanical performance, and interfacial behavior of Sn–0.7Cu–0.05Ni–xSb/Cu solder joints10.1007/s10854-021-07135-3 ↗
28. Interfacial transfer and phase evolution between Cu and Sn solder doped with minor Cu, Ag and Ni: experimental and theoretical investigations10.1007/s00339-020-03846-2 ↗
29. Effect of Sb addition on the tensile deformation behavior of lead-free Sn–3.5Ag solder alloy10.1016/j.matdes.2011.05.052 ↗
30. The influence of 0–0.1 wt.% Ni on the microstructure and fluidity length of Sn-0.7Cu-xNi10.1007/s11664-007-0281-7 ↗
31. Effect of Ni addition on the wettability and microstructure of Sn2.5Ag0.7Cu0.1RE solder alloy10.1016/j.matdes.2017.01.046 ↗
32. Effects of Sb addition on the properties of Sn-Ag-Cu/(Cu, Ni) solder systems10.1016/j.jallcom.2016.08.035 ↗
33. Influence of small addition of antimony (Sb) on thermal behavior, microstructural and tensile properties of Sn-9.0Zn-0.5Al Pb-free solder alloy10.1016/j.msea.2017.06.092 ↗
34. Wettability of SACR–xNi solder alloy on Cu leading wire with no-clean flux10.1007/s10854-016-5496-z ↗
35. Effect of Nano-Cu6Sn5 upon development mechanism of Cu–Ni–Sn compounds and mechanical characteristics for mixed solder joints10.1016/j.matchar.2023.113553 ↗
36. The effect of Ni and Bi additions on the solderability of Sn-0.7Cu solder coatings10.1007/s11664-019-07596-7 ↗
37. Effects of Ni addition on mechanical properties of Sn58Bi solder alloy during solid-state aging10.1016/j.msea.2016.05.015 ↗
38. Effects of Sb addition on tensile strength of Sn–3.5Ag–0.7Cu solder alloy and joint10.1016/j.tsf.2005.09.060 ↗
39. Viscoplastic characterization and post-rupture microanalysis of a novel lead-free solder with small additions of Bi, Sb and Ni10.1016/j.jallcom.2016.10.025 ↗
40. Investigating the impact of cobalt incorporation on the transformation of Cu6Sn5 layer to (Cu, Co)6Sn5: microstructural and mechanical insights10.1016/j.matchar.2024.113934 ↗
41. Kinetics of intermetallic phase formation at the interface of Sn–Ag–Cu–X (X = Bi, In) solders with Cu substrate10.1016/j.jallcom.2011.03.164 ↗
42. Interfacial microstructure evolution and shear strength of Sn0.7Cu–xNi/Cu solder joints10.1007/s10854-018-9219-5 ↗
43. Influence of graphene content and nickel decoration on the microstructural and mechanical characteristics of the Cu/Sn–Ag–Cu/Cu soldered joint10.1016/j.jmrt.2020.06.026 ↗
44. Effect of Sb content on the phase structure and interface structure of Sn1.0Ag0.5Cu lead-free solder10.1016/j.microrel.2022.114883 ↗
45. Influence of Sb on IMC growth in Sn–Ag–Cu–Sb Pb-free solder joints in reflow process10.1016/j.tsf.2004.05.063 ↗
46. Formation and growth of interfacial intermetallics in Sn-0.3Ag-0.7Cu-xCeO2/Cu solder joints during the reflow process10.1016/j.jallcom.2018.11.156 ↗
47. Effects of Sb on the properties and interfacial evolution of SAC305-2Bi-xSb/Cu solder joints10.1016/j.jmrt.2024.06.023 ↗
48. Effect of the second-phase particle distribution on the brittle fracture behavior of Sn-3Ag-0.5Cu solder10.1007/s11664-023-10319-8 ↗
49. Reaction of Sn-3.5Ag-0.7Cu-xSb solder with Cu metallization during reflow soldering10.1109/TEPM.2004.830507 ↗
50. Combined effects of Bi and Sb elements on microstructure, thermal and mechanical properties of Sn-0.7Ag-0.5Cu solder alloys10.1016/S1003-6326(22)66021-7 ↗
51. Influence of temperature gradient bonding on the micromorphology and shear performance of Sn-based solder joints: experiments and first principles calculations10.1016/j.jmapro.2024.05.057 ↗
52. Micro-additives and their impact on tensile and fracture performance of solder10.1016/j.microrel.2023.115107 ↗
53. Influence of antimony on reliability of solder joints using Sn-Sb binary alloy for power semiconductor modules10.5104/jiepeng.8.8 ↗
54. The influence of strengthening and recrystallization to the cracking behavior of Ni, Sb, Bi alloyed SnAgCu solder during thermal cycling10.1016/j.msea.2015.10.072 ↗
55. New developments in high-temperature, high-performance lead-free solder alloys
56. Effect of Ni-RGO nanosheets on the creep behavior of Sn–Ag–Cu composite solder joints10.1016/j.matchemphys.2024.129773 ↗
57. Formation and growth of intermetallic compounds in lead-free solder joints
58. Stabilisation of Cu6Sn5 by Ni in Sn-0.7Cu-0.05Ni lead-free solder alloys10.1016/j.intermet.2009.07.005 ↗
59. Mechanical properties and fracture mechanisms of Sn-3.0Ag-0.5Cu solder alloys and joints at cryogenic temperatures10.1016/j.msea.2016.12.058 ↗
60. Characters of multicomponent lead-free solders10.1007/s10854-013-1340-x ↗
61. Effect of Co addition into Ni film on shear strength of solder/Ni/Cu system: experimental and theoretical investigations10.1016/j.msea.2020.139589 ↗