Effects of solution temperature and cooling rate on microstructure and micro-hardness of a hot compressed Ti-6Al-4V alloy
Source abstract
Abstract
Abstract The effects of solution temperature and cooling rate on microstructure and micro-hardness of a hot compressed Ti-6Al-4V alloy are investigated. The microstructure observations reveal the occurrence of static recrystallization during solution treatment. The lamellar α phases firstly decompose into the short-rod phases, and then gradually spheroidize. The increased solution temperature can accelerate the transformation of α grain boundary from the low-angle grain boundaries (LAGB) to the high-angle grain boundaries (HAGB). So, the growth and spheroidization of α grains become more and more obvious. Meanwhile, the precipitation of secondary α phases is promoted. The micro-hardness is significantly improved after the solution treatment, i.e., the micro-hardness undergoes the rapid decrease and slow increase with raising the solution temperature. In addition, the cooling rate has great impact on the microstructures and micro-hardness. With reducing the cooling rate, the mean size of equiaxed α grains and the thickness of lamellar α phases obviously increase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Isothermal tensile deformation behaviors and fracture mechanism of Ti-5Al-5Mo-5V-1Cr-1Fe alloy in β phase field10.1016/j.vacuum.2018.07.034 ↗
2. On the high temperature deformation behaviour of titanium alloy BT3-110.1016/j.msea.2016.12.043 ↗
3. Effects of initial microstructures on hot tensile deformation behaviors and fracture characteristics of Ti-6Al-4V alloy10.1016/j.msea.2017.11.044 ↗
4. Quantitative analysis of dynamic softening behaviors induced by dynamic recrystallization for Ti-10V-2Fe-2Al alloy10.1515/htmp-2014-0106 ↗
5. Relationship between lamellar α evolution and flow behavior during isothermal deformation of Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.msea.2012.08.074 ↗
6. Influence of solution treatment on microstructure and mechanical properties of a near β titanium alloy Ti-733310.1016/j.matdes.2015.06.015 ↗
7. Development of α-phase morphologies during low temperature isothermal heat treatment of a Ti-5Al-5Mo-5V-3Cr alloy10.1016/j.msea.2010.09.061 ↗
8. A physically-based constitutive model for hot deformation of Ti-10-2-3 alloy10.1016/j.jallcom.2016.11.208 ↗
9. Constitutive modeling and fracture behavior of a biomedical Ti–13Nb-13Zr alloy10.1016/j.msea.2017.05.113 ↗
10. Comparative study of constitutive modeling for Ti–6Al–4V alloy at low strain rates and elevated temperatures10.1016/j.matdes.2013.10.089 ↗
11. Deformation homogeneity, mechanical behaviour and strain hardening characteristics of titanium severe plastically deformed by cyclic channel die compression method10.1016/j.matdes.2016.04.004 ↗
12. Evolution mechanisms of the primary α and β phases during α/β deformation of an α/β titanium alloy TC810.1016/j.matchar.2016.08.028 ↗
13. Competition between dynamic recovery and recrystallization during hot deformation for TC18 titanium alloy10.1016/j.msea.2015.03.071 ↗
14. Relationship of RRA heat treatment with exfoliation corrosion, electrical conductivity and microstructure of AA7075 alloy10.1002/maco.201709497 ↗
15. Microstructural evolution of a Ni-Fe-Cr-base superalloy during non-isothermal two-stage hot deformation10.1016/j.vacuum.2018.02.034 ↗
16. Flow curves, dynamic recrystallisation and precipitation in a medium carbon low alloy steel10.1016/j.vacuum.2017.05.010 ↗
17. Microstructural evolution and constitutive models to predict hot deformation behaviors of a nickel-based superalloy10.1016/j.vacuum.2016.12.022 ↗
18. Mechancial properties of fully microstructure in Ti-6Al-4V alloy transformed from refined beta grains obtained by rapid heat treatment(RHT)10.1016/j.scriptamat.2017.05.038 ↗
19. Microstructure evolution and static recrystallization during hot rolling and annealing of an equiaxed-structure TC21 titanium alloy10.1016/j.jallcom.2018.04.148 ↗
20. Achieving fine beta grain structure in a metastable beta titanium alloy through multiple forging-annealing cycles10.1007/s11661-016-3496-5 ↗
21. The influence of temperature and strain rate on the deformation response and microstructural evolution during hot compression of a titanium alloy Ti-6Al-4V-0.1B10.1016/j.jallcom.2012.08.123 ↗
22. Influence of thermomechanical processing and heat treatment on microstructure, tensile properties and fracture toughness of Ti-1100-0.1B alloy10.1016/j.jallcom.2013.11.014 ↗
23. Microstructural tailoring and mechanical properties of a multi-alloyed near β titanium alloy Ti-5321 with various heat treatment10.1016/j.msea.2017.11.029 ↗
24. Multi-step heat treatment design for nano-scale lamellar structures of a cast Ti-45Al-8.5Nb-(W, B, Y) alloy10.1016/j.intermet.2016.09.006 ↗
25. Improvement in fatigue strength of notched Ti-6Al-4V alloy by short-time heat treatment10.1016/j.msea.2016.05.071 ↗
26. Prediction of static globularization of Ti-17 alloy with starting lamellar microstructure during heat treatment10.1016/j.commatsci.2014.05.049 ↗
27. Effect of cooling rate on microstructure evolution during α/β heat treatment of TA15 titanium alloy10.1016/j.matchar.2012.05.009 ↗
28. Beta to alpha transformation kinetics and microstructure of Ti-6Al-4V alloy during continuous cooling10.1016/j.matchemphys.2016.06.082 ↗
29. Effect of solution treatment and aging on microstructure and tensile properties of high strength β titanium alloy, Ti-5Al-5V-5Mo-3Cr10.1016/j.matdes.2014.04.015 ↗
30. Flow softening behavior of Ti–13V–11Cr–3Al beta Ti alloy in double-hit hot compression tests10.1557/jmr.2016.430 ↗
31. Effect of initial alpha lamellar thickness on deformation behavior of a near-α high-temperature alloy during thermomechanical processing10.1016/j.msea.2016.11.063 ↗
32. Modelling of the superplastic deformation of the near-a titanium alloy (Ti-2.5Al-1.8Mn) using arrhenius-type constitutive model and artificial neural network10.3390/met7120568 ↗
33. Prediction of flow stress in a wide temperature range involving phase transformation for as-cast Ti-6Al-2Zr-1Mo-1V alloy by artificial neural network10.1016/j.matdes.2013.02.033 ↗
34. Effect of anisotropy on mechanical properties of Ti-6Al-4V in superplastic region10.1088/1757-899X/346/1/012023 ↗
35. A novel constitutive model for hot deformation behaviors of Ti-6Al-4V alloy based on probabilistic method10.1007/s00339-016-0248-8 ↗
36. Phase transformation and constitutive models of a hot compressed TC18 titanium alloy in the α+β regime10.1016/j.vacuum.2018.08.020 ↗
37. Characterization of hot deformation behaviour of alloy 617 through kinetic analysis, dynamic material modeling and microstructural studies10.1016/j.msea.2016.04.004 ↗
38. Microstructure and flow behavior of cast 2304 duplex stainless steel at elevated temperatures10.1557/jmr.2016.457 ↗
39. Effects of solution treatment on microstructures and micro-hardness of a Sr-modified Al-Si-Mg alloy10.1016/j.msea.2018.04.049 ↗