Enhancing tensile strength of Mg–Al–Ca wrought alloys by increasing Ca concentration
Source abstract
Abstract
Abstract The tensile strengths of the as-extruded Mg–Al–Ca ternary alloys at both ambient and elevated temperatures are enhanced via adding a high content of Ca element up to 6 wt%. High-temperature strength of the present rare-earth-free Mg alloys can be even compared with those of the reported Mg-RE alloys. The as-extruded Mg–6Al–6Ca (wt. %, AX66) alloy exhibits a tensile yield strength (YS) of ~404 MPa and an ultimate tensile strength (UTS) of ~415 MPa at room temperature, and YS of ~225 MPa and UTS of ~265 MPa at 200 °C, respectively. For the AX66 alloy, the nucleation rates of dynamic recrystallized (DRXed) grains are larger than those of the AX62 and AX64 alloys due to the typical particle stimulated nucleation effect. A number of long-rod Al2Ca phase is dispersed at the grain boundaries of AX66 alloy, and a restricted degree of DRX is induced. Consequently, the majority ofα-Mg matrix exists in the as-deformed state involving a high density of subgrains. The combined effects of grain refinement hardening, texture hardening and precipitation hardening guarantee the high strength. Specially, numerous micron-scale bulk (Mg, Al)2Ca phases are found to distribute among matrix, which play a critical role in maintaining the high thermal-resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Effect of deformation twinning on crystallographic texture evolution in a Mg–6.6Zn–0.2Ca (ZX70) alloy during recrystallisation10.1016/j.jallcom.2018.10.065 ↗
2. Effect of various Ca content on microstructure and fracture toughness of extruded Mg-2Zn alloys10.1016/j.jallcom.2017.11.276 ↗
3. Crack behavior in Mg/Al alloy thin sheet during hot compound extrusion10.1016/j.jma.2019.09.006 ↗
4. Comparison of microstructures and mechanical properties of composite extruded AZ31 sheets10.1016/j.jma.2019.09.007 ↗
5. Grain refining mechanism of Al-containing Mg alloys with the addition of Mn–Al alloys10.1016/j.jallcom.2010.07.164 ↗
6. Magnesium for automotive applications: primary production cost assessment10.1007/s11837-003-0204-x ↗
7. High-conductivity binary Mg–Zn sheet processed by cold rolling and subsequent aging10.1016/j.jallcom.2013.06.082 ↗
8. Enhancing mechanical properties of Mg–Sn alloys by combining addition of Ca and Zn10.1016/j.matdes.2015.06.032 ↗
9. Recent developments in rare-earth free wrought magnesium alloys having high strength: a review10.1016/j.jallcom.2015.12.057 ↗
10. Effect of Ca/Al ratio on microstructure and mechanical properties of Mg-Al-Ca-Mn alloys10.1016/j.msea.2016.11.026 ↗
11. Development of high-strength, low-cost wrought Mg–2.5mass% Zn alloy through micro-alloying with Ca and La10.1016/j.matdes.2015.07.029 ↗
12. Microstructure and mechanical property of a high-strength Mg–10Gd–6Y–1.5Zn–0.5Zr alloy prepared by multi-pass equal channel angular pressing10.1016/j.jma.2017.05.002 ↗
13. The effect of extrusion conditions on the properties and textures of AZ31B alloy10.1016/j.jma.2017.03.002 ↗
14. Manufacturing high-performance Mg alloy through hot extrusion
15. Recent research and developments on wrought magnesium alloys10.1016/j.jma.2017.09.001 ↗
16. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
17. High temperature mechanical behavior of low-pressure sand-cast Mg–Gd–Y–Zr magnesium alloy10.1016/j.jma.2019.07.006 ↗
18. Fabrication of ultra-high strength magnesium alloys over 540 MPa with low alloying concentration by double continuously extrusion10.1016/j.jma.2018.04.003 ↗
19. A super high-strength Mg-Gd-Y-Zn-Mn alloy fabricated by hot extrusion and strain aging10.1016/j.matdes.2019.107666 ↗
20. Remarkably enhanced mechanical properties of Mg-8Gd-1Er-0.5 Zr alloy on the route of extrusion, rolling and aging10.1016/j.matlet.2017.10.003 ↗
21. Age hardening responses of as-extruded Mg-2.5Sn-1.5Ca alloys with a wide range of Al concentration10.1016/j.jmst.2019.06.025 ↗
22. Development of low-alloyed and rare-earth-free magnesium alloys having ultra-high strength10.1016/j.actamat.2018.03.002 ↗
23. Ultra-fine grain size and exceptionally high strength in dilute Mg–Ca alloys achieved by conventional one-step extrusion10.1016/j.matlet.2018.11.080 ↗
24. High-strength extruded Mg–Al–Ca–Mn alloy10.1016/j.scriptamat.2011.04.026 ↗
25. Unexpected influence of Mn addition on the creep properties of a cast Mg–2Al–2Ca (mass%) alloy10.1016/j.actamat.2011.08.049 ↗
26. Mechanistic investigation of a low-alloy Mg–Ca-based extrusion alloy with high strength–ductility synergy10.1016/j.actamat.2020.01.017 ↗
27. Processing and properties of magnesium containing a dense uniform dispersion of nanoparticles10.1038/nature16445 ↗
28. Effects of Ca and Sr addition on mechanical properties of a cast AZ91 magnesium alloy at room and elevated temperature10.1016/j.msea.2005.05.028 ↗
29. Recent magnesium alloy development for elevated temperature applications10.1179/095066004225010497 ↗
30. Effect of Gd content on high temperature mechanical properties of Mg–Gd–Y–Zr alloy10.1016/j.msea.2015.11.047 ↗
31. Evaluation of magnesium die-casting alloys for elevated temperature applications: microstructure, tensile properties, and creep resistance10.1007/s11661-015-2946-9 ↗
32. On the microstructure and mechanical property of as-extruded Mg-Gd-Y-Zn alloy with Sr addition10.1016/j.msea.2016.10.016 ↗
33. Prominent role of a high volume fraction of Mg17Al12 particles on tensile behaviors of rolled Mg–Al–Zn alloys10.1016/j.jallcom.2017.08.289 ↗
34. Hot tearing of ternary Mg− Al− Ca alloy castings10.1007/s11661-006-1059-x ↗
35. Thermodynamic modeling of the Mg–Al–Ca system10.1016/j.actamat.2008.10.037 ↗
36. Creep and microstructure of magnesium-aluminum-calcium based alloys10.1007/s11661-002-0118-1 ↗
37. Computational phase equilibria and experimental investigation of magnesium–aluminum–calcium alloys10.1016/j.intermet.2012.01.001 ↗
38. Effect of extrusion temperature on the microstructure and mechanical properties of Mg–5Al–2Ca alloy10.1007/s40195-015-0289-6 ↗
39. Solidification paths and eutectic intermetallic phases in Mg–Al–Ca ternary alloys10.1016/j.actamat.2005.03.001 ↗
40. Phase equilibria in the Mg-Al-Ca ternary system at 773 and 673 K10.1007/s11661-006-0070-6 ↗
41. Fabrication of extraordinary high-strength magnesium alloy by hot extrusion10.1016/j.scriptamat.2009.06.003 ↗
42. Bimodally grained microstructure development during hot extrusion of Mg–2.4 Zn–0.1 Ag–0.1 Ca–0.16 Zr (at.%) alloys10.1016/j.actamat.2009.07.057 ↗
43. Tensile creep behavior and microstructure evolution of Mg-11Gd-2Y-0.5Zr alloy10.1016/j.vacuum.2019.06.040 ↗
44. The effect of Y addition on recrystallization and mechanical properties of Mg–6Zn–xY–0.5Ce–0.4Zr alloys10.1016/j.vacuum.2018.06.048 ↗
45. Effects of alloying composition on the microstructures and mechanical properties of Mg-Al-Zn-Ca-RE magnesium alloy10.1016/j.vacuum.2018.10.072 ↗
46. Significant improvement in the strength of Mg-Al-Zn-Ca-Mn extruded alloy by tailoring the initial microstructure10.1016/j.vacuum.2019.01.016 ↗
47. Creep and microstructure of magnesium-aluminum-calcium based alloys
48. Fabrication of TiC particulate reinforced magnesium matrix composites10.1016/S1359-6462(02)00551-1 ↗
49. Mg-Al-Ca in-situ composites with a refined eutectic structure and their compressive properties10.1007/s11661-008-9488-3 ↗
50. In situ synthesis of TiC/Mg composites in molten magnesium10.1016/S1359-6462(03)00014-9 ↗
51. Grain-scale creep processes in Mg–Al–Ca base alloys: implications for alloy design10.1016/j.scriptamat.2010.03.055 ↗
52. Effect of grain size on prismatic slip in Mg–3Al–1Zn alloy10.1016/j.scriptamat.2012.05.017 ↗
53. Effect of precipitate shape on slip and twinning in magnesium alloys10.1016/j.actamat.2010.11.060 ↗
54. Strengthening mechanisms acting in extruded Mg-based long-period stacking ordered (LPSO)-phase alloys10.1016/j.actamat.2018.10.016 ↗
55. The contribution of long-period stacking-ordered structure (LPSO) to high strength-high ductility combination and nanoscale deformation behavior of magnesium-rare earth alloy10.1016/j.msea.2017.12.056 ↗
56. The microstructure evolution with lamellar 14H-type LPSO structure in an M996.5Gd2.5Zn1 alloy during solid solution heat treatment at 773 K10.1016/j.jallcom.2008.10.126 ↗
57. Koike · 2000
58. Luo · 1998
59. Luo · 2001
60. Development of heat resistant Mg-Zn-Al-based magnesium alloys by addition of La and Ca: microstructure and tensile properties10.1016/j.jallcom.2016.05.137 ↗
61. Microstructures and tensile properties of as-extruded Mg-Sn binary alloys10.1016/S1003-6326(09)60298-3 ↗
62. Powell · 2001
63. Microstructure, mechanical and creep properties of high Ca/Al ratio Mg-Al-Ca alloy10.1016/j.msea.2016.03.001 ↗
64. Influence of the Al2Ca phase on microstructure and mechanical properties of Mg–Al–Ca alloys10.1016/j.jallcom.2015.06.060 ↗
65. Development of microstructure in solution-heat-treated Mg-5Al-x Ca alloys10.3139/146.030886 ↗