journal article·2017-01

High temperature oxidation behavior and wear resistance of Ti0.53Al0.47N coating by cathodic arc evaporation

Z.T. Wu, P. Sun, Z.B. Qi, B.B. Wei, Z.C. Wang

Vacuum· Volume 135
Publisher page

Abstract

Abstract In this study, oxidation and tribology behavior of Ti 0.53 Al 0.47 N coating deposited by cathodic arc evaporation were investigated. The effects of varying temperature from RT to 850 °C on microstructure, phase composition, oxidation behavior, and wear resistance of the coating were evaluated. The phase structure of the Ti 0.53 Al 0.47 N coating changes slightly with the elevated temperature, whereas the oxidation behavior of the coating reveals a remarkable variation due to the formation of different type oxide scales. The final oxide scale consists of an outer Al 2 O 3 dominated layer and an inner TiO 2 dominated layer, exhibiting a bilayer structure. A serious wear of the Ti 0.53 Al 0.47 N coating occurs during the room temperature test. With increasing the test temperature up to 700 °C, the coating show promoted wear resistance owing to the Al 2 O 3 oxide scale provides an excellent protection against the wear. However, further increasing the temperature up to 850 °C produces a fast growth of the TiO 2 . This deteriorates the protection of the Al 2 O 3 scale, resulting in an accelerated oxidation of the coating. Consequently, the Ti 0.53 Al 0.47 N coating illustrates a degraded wear resistance at 850 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Hard and superhard nanocomposite coatings10.1016/S0257-8972(99)00586-1 ↗
2. Hard nanocomposite coatings: thermal stability, oxidation resistance and toughness10.1016/j.surfcoat.2012.05.073 ↗
3. Flexible hard nanocomposite coatings10.1039/C5RA09586G ↗
4. Heat generation and temperature prediction in metal cutting: a review and implications for high speed machining10.1016/j.ijmachtools.2005.07.024 ↗
5. The influence of Johnson–Cook material constants on finite element simulation of machining of AISI 316L steel10.1016/j.ijmachtools.2006.06.006 ↗
6. Oxidation of TiN, ZrN, TiZrN, CrN, TiCrN and TiN/CrN multilayer hard coatings reactively sputtered at low temperature10.1016/0040-6090(96)08663-4 ↗
7. Oxidation resistance of TiN, CrN, TiAlN and CrAlN coatings deposited by lateral rotating cathode arc10.1016/j.tsf.2009.03.038 ↗
8. Effect of ductile layers in mechanical behaviour of TiAlN thin coatings10.1016/S0924-0136(03)00454-0 ↗
9. Single layer and multilayer wear resistant coatings of (Ti, Al) N: a review10.1016/S0921-5093(02)00259-9 ↗
10. Effect of N2 partial pressure on the microstructure and mechanical properties of reactively sputtered (Ti, Al) N coatings10.1016/j.matlet.2005.02.068 ↗
11. Wear behavior and cutting performance of nanostructured hard coatings on cemented carbide cutting tools in hard milling10.1016/j.triboint.2013.02.035 ↗
12. Thermal stability and oxidation resistance of arc evaporated TiAlN, TaAlN, TiAlTaN, and TiAlN/TaAlN coatings10.1016/j.surfcoat.2014.10.024 ↗
13. Hard amorphous Ti–Al–N coatings deposited by sputtering10.1016/j.tsf.2008.02.006 ↗
14. Scratch adhesion characteristics of PVD TiAlN deposited on high speed steel, cemented carbide and PCBN substrates10.1016/j.wear.2013.08.025 ↗
15. Microstructural and tribological characterisation of a nitriding/TiAlN PVD coating duplex treatment applied to M2 high speed steel tools10.1016/j.surfcoat.2015.03.034 ↗
16. Mechanical properties and machining performance of Ti1-xAlxN-coated cutting tools10.1016/j.surfcoat.2004.04.056 ↗
17. Relationship between tribological properties and oxidation behavior of Ti0.34Al0.66N coatings at elevated temperature up to 900 °C10.1016/j.surfcoat.2012.02.017 ↗
18. Effects of aluminum concentration on the oxidation behaviors of reactively sputtered TiAlN films10.1111/j.1151-2916.1999.tb01819.x ↗
19. Oxidation behaviors of TiAl(La)N coatings deposited by ion plating10.1016/j.scriptamat.2004.11.013 ↗
20. Large-scale fabrication of hard superlattice thin films by combined steered arc evaporation and unbalanced magnetron sputtering10.1016/S0257-8972(97)00028-5 ↗
21. High temperature oxidation of (Ti1-xAlx) N coatings made by plasma enhanced chemical vapor deposition10.1116/1.581562 ↗
22. Oxidation of metastable single-phase polycrystalline Ti0.5Al0.5N films: kinetics and mechanisms10.1063/1.345664 ↗
23. Oxidation resistance of (Ti, Al, Si) N coatings in air10.1016/S0257-8972(97)00127-8 ↗
24. High temperature oxidation behavior and mechanical properties of TiAlN/SiN decorative films on borosilicate glass by magnetron sputtering10.1016/j.tsf.2015.03.013 ↗
25. Tribological characteristics of CrCN coatings at elevated temperature10.1016/j.vacuum.2005.07.033 ↗
26. Wear mechanisms of several cutting tool materials in hard turning of high carbon–chromium tool steel10.1016/j.triboint.2013.10.011 ↗
27. Microstructure, mechanical properties and cutting performance of superhard (Ti, Si, Al) N nanocomposite films grown by dc reactive magnetron sputtering10.1016/j.surfcoat.2003.08.056 ↗
28. Effect of Al content on microstructure and mechanical properties of Ti–Al–Si–N nanocomposite coatings10.1016/j.ijrmhm.2008.12.002 ↗
29. Machining performance of Ti–Al–Si–N coated inserts10.1016/j.surfcoat.2010.07.043 ↗
30. Microstructure and mechanical properties of cathodic arc ion-plated (Al,Ti)N coatings10.1016/S0257-8972(02)00610-2 ↗
31. Thermal stability and thermo-mechanical properties of magnetron sputtered Cr–Al–Y–N coatings10.1116/1.2806943 ↗
32. Thermal stability of arc evaporated high aluminum-content Ti1-xAlxN thin films10.1116/1.1503784 ↗
33. Metastable phases and spinodal decomposition in Ti1-xAlxN system studied by ab initio and thermodynamic modeling, a comparison with the TiN–Si3N4 system10.1016/j.msea.2006.10.012 ↗
34. Thermal stability and oxidation resistance of Ti–Al–N coatings10.1016/j.surfcoat.2011.12.028 ↗
35. Cross-sectional structure-property relationship in a graded nanocrystalline Ti1-xAlxN thin film10.1016/j.actamat.2015.09.007 ↗
36. Strain evolution during spinodal decomposition of TiAlN thin films10.1016/j.tsf.2012.04.059 ↗
37. Birks · 2006
38. Microstructure and chemical state of Ti1-xYxN film deposited by reactive magnetron sputtering10.1116/1.1319680 ↗
39. Anti-oxidation properties of TiAlN film prepared by plasma-assisted chemical vapor deposition and roles of Al10.1016/S0040-6090(97)00212-5 ↗
40. Corrosion of CrN and TiAlN coatings in chloride-containing atmospheres10.1016/S0257-8972(99)00270-4 ↗
41. Thermal stability of nitride thin films10.1016/S0042-207X(00)00143-3 ↗
42. Hard amorphous nanocomposite coatings with oxidation resistance above 1000 °C10.1179/174367508X306460 ↗
43. High-temperature tribological characterization of commercial TiAlN coatings10.1088/0953-8984/18/32/S04 ↗
45. Oxidative wear of heat-treated steels10.1016/S0043-1648(01)00661-5 ↗
46. Comparison of tribological behaviour of TiN, TiCN and CrN at elevated temperatures10.1016/j.surfcoat.2004.07.098 ↗
47. Macroparticle contamination in cathodic arc coatings: generation, transport and control10.1016/0257-8972(92)90369-L ↗
48. Anders · 2008
49. Oxidation of WC–Co, WC–Ni and WC–Co–Ni hard metals in the temperature range 500–800 °C10.1016/0263-4368(96)00009-1 ↗
50. Kinetics inversion in isothermal oxidation of uncoated WC-based carbides between 450 and 800 °C10.1016/j.corsci.2008.12.022 ↗
51. Non-isothermal oxidation kinetics of WC–6Co cemented carbides in air10.1016/j.ijrmhm.2013.02.003 ↗