Influence of Ti on the mechanical properties, thermal stability and oxidation resistance of Al–Cr–N coatings
Source abstract
Abstract
Abstract Al0.68Cr0.32N, Al0.66Cr0.25Ti0.09N and Al0.62Cr0.20Ti0.18N coatings prepared by cathodic arc evaporation exhibit single phase cubic structure. Increasing Ti content from 0 to 18 at% causes a continuous hardness promotion from ∼27.4 to 33.2 GPa, however, a drop in elastic modulus from ∼481.8 to 337.1 GPa. Annealing of Al–Cr–N in Ar results in a transition into stable phases of wurtzite (w-) AlN and Cr via an intermediate phase Cr2N. Alloying with Ti into Al–Cr–N promotes the w-AlN formation, but retards the N-loss, where the finally stable phases of w-AlN, Cr and TiN after annealing are obtained. Nevertheless, the Ti-addition has a significantly inferior effect on the oxidation resistance of Al–Cr–N coating due to the higher affinity between Ti and oxygen, where the Al0.68Cr0.32N and Al0.62Cr0.20Ti0.18N coatings after oxidation at 1100 °C for 20 h reveal oxide scales of ∼1.3 and 4.0 μm, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Investigation of the properties of Al1−xCrxN coatings prepared by cathodic arc evaporation10.1016/j.surfcoat.2005.01.043 ↗
2. Correlation of the impact resistance of variously doped CrAlN PVD coatings with their cutting performance in milling aerospace alloys10.1016/j.surfcoat.2008.08.009 ↗
3. Oxidation resistance of magnetron-sputtered CrAlN coatings on 430 steel at 800 °C10.1016/j.surfcoat.2006.08.049 ↗
4. Oxidation of arc-evaporated Al1−xCrxN coatings10.1116/1.2738492 ↗
5. Thermal stability of nitride thin films10.1016/S0042-207X(00)00143-3 ↗
6. Microstructure, mechanical and thermal properties of TiAlN/CrAlN multilayer coatings10.1016/j.ijrmhm.2013.01.020 ↗
7. Structure and phase evolution of Cr–Al–N coatings during annealing10.1016/j.surfcoat.2008.04.075 ↗
8. Thermal stability of Al–Cr–N hard coatings10.1016/j.scriptamat.2006.02.023 ↗
9. Hardness evolution of Al–Cr–N coatings under thermal load10.1557/JMR.2008.0366 ↗
10. Thermal and thermo-mechanical properties of Ti–Al–N and Cr–Al–N coatings10.1016/j.ijrmhm.2012.06.007 ↗
11. Micro-hardness, microstructures and thermal stability of (Ti,Cr,Al,Si)N films deposited by cathodic arc method10.1016/j.vacuum.2007.07.048 ↗
12. Effects of Ti alloying of AlCrN coatings on thermal stability and oxidation resistance10.1016/j.tsf.2013.03.003 ↗
13. Chemical and microstructural characterization of (Y or Zr)-doped CrAlN coatings10.1016/j.surfcoat.2011.07.071 ↗
14. Improved hardness and oxidation resistance for CrAlN hard coatings with Y addition by magnetron co-sputtering10.1016/j.surfcoat.2014.02.034 ↗
15. Determination of the local environment of silicon and the microstructure of quaternary CrAl(Si)N films10.1016/j.actamat.2006.11.014 ↗
16. Vanadium containing self-adaptive low-friction hard coatings for high-temperature applications: A review10.1016/j.surfcoat.2013.04.034 ↗
17. The effect of yttrium incorporation on the oxidation resistance of Cr–Al–N coatings10.1016/j.surfcoat.2008.06.161 ↗
18. Tribological adaptability of TiAlCrN PVD coatings under high performance dry machining conditions10.1016/j.surfcoat.2005.08.057 ↗
19. Study on thermal stability of CrTiAlN coating for dry drilling10.1016/j.surfcoat.2006.07.166 ↗
20. The Effect of AlCrTiN Coatings on Product Quality in Micro-milling of 45 HRC Hardened H13 Die Steel
21. Design and performance of AlTiN and TiAlCrN PVD coatings for machining of hard to cut materials10.1016/j.surfcoat.2009.08.021 ↗
22. Microstructure and cutting performance of CrTiAlN coating for high-speed dry milling10.1016/S1003-6326(14)63256-8 ↗
23. The effects of deposition temperature and post-annealing on the crystal structure and mechanical property of TiCrAlN films with high Al contents10.1016/j.surfcoat.2005.03.013 ↗
24. High temperature oxidation of CrTiAlN hard coatings prepared by unbalanced magnetron sputtering10.1016/j.tsf.2009.03.115 ↗
25. Properties of (Ti,Cr,Al)N coatings with high Al content deposited by new plasma enhanced arc-cathode10.1016/S0257-8972(03)00580-2 ↗
26. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
27. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
28. Spinodal decomposition of cubic Ti1–xAlxN: Comparison between experiments and modeling10.3139/146.101570 ↗
29. Lide · 2010
30. Oxidation behavior of CrNx and (Cr,Al)Nx hard coatings10.1002/maco.19900411222 ↗
31. Thermal oxidation of Ti1−xAlxN coatings in air10.1016/S0955-2219(97)00050-2 ↗
32. Effect of CrN addition on the structure, mechanical and thermal properties of Ti–Al–N coating10.1016/j.surfcoat.2013.08.010 ↗
33. High temperature behavior of nanolayered CrAlTiN coating: thermal stability, oxidation, and tribological properties10.1016/j.surfcoat.2014.07.053 ↗