Reactive wetting of TA2 pure Ti and TC4 alloy by molten Al 4043 alloy at 873–973 K
Source abstract
Abstract
Abstract Wetting of typical industrial grades of Ti by Al 4043 alloy was studied by the sessile drop method at 873–973 K under high vacuum. Al/Ti is a typical reactive wetting system, and the double phases in TC4 alloy but only one phase in pure Ti caused the different interfacial structure. The mass transport was enhanced at liquid/solid interface due to the loosened Al3Ti layer in Al/TC4, but the compact Ti7Al5Si12 layer would block the mass transport in Al/TA2 pure Ti, that further caused the different final wettability. The spreading dynamics of both TA2 and TC4 can be described by reaction product control model, and the activation energy is in the range of 10–47 kJ/mol, which is corresponding to the surface energy difference per molar area between Ti and TiO2.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Alloy phase transformations driven by high temperature corrosion processes10.1016/S0010-938X(01)00065-8 ↗
2. Intermetallic Ti-Al coatings for protection of titanium alloys: oxidation and mechanical behavior10.1016/S0257-8972(97)00472-6 ↗
3. Liquid-phase aluminizing and siliconizing at the surface of a Ti60 alloy and improvement in oxidation resistance10.1016/j.msea.2006.06.059 ↗
4. Improvement of oxidation resistance of γ-TiAl at 900 and 1000 °C through hot-dip aluminizing10.1007/s11085-009-9187-5 ↗
5. Asthana · 2000
6. Fillability of Al-Si brazing sheet using fluoride flux10.2464/jilm.47.655 ↗
7. Reactive wetting of TiC-Ni cermet by Ag-Cu-Zn alloy during evaporation10.1016/j.vacuum.2017.01.014 ↗
8. Influence of beam current on microstructures and mechanical properties of electron beam welding-brazed aluminum-steel joints with an Al5Si filler wire10.1016/j.vacuum.2017.04.029 ↗
9. Structure, micro-hardness and corrosion behaviour of the Al–Si/Al2O3 coatings prepared by laser plasma hybrid spraying on magnesium alloy10.1016/j.vacuum.2015.04.005 ↗
10. Microstructure and corrosion resistance of laser cladding and friction stir processing hybrid modification Al-Si coatings on AZ31B10.1016/j.vacuum.2016.08.010 ↗
11. Wettability and phase formation in the TiCx/Al system10.1016/S1359-6462(97)00235-2 ↗
12. Reactive wetting of TiC-Ni cermet by Ag-Cu-Zn alloy during evaporation10.1016/j.vacuum.2017.01.014 ↗
13. Wettability of polycrystalline rutile TiO2 by molten Al in different atmospheres10.1016/j.actamat.2005.11.024 ↗
14. Interface phenomena in the B4C/(Me-Ti) systems (Me = Cu, Au and Sn)10.1007/s10853-005-1953-4 ↗
15. Wetting behavior of liquid Fe-C-Ti alloys on sapphire10.1016/j.msea.2007.10.100 ↗
16. Wettability of pure Ti by molten pure Mg droplets10.1016/j.actamat.2009.09.039 ↗
17. Wetting behavior and interface characteristic of Ti32.8Zr30.2Ni5.3Cu9Be22.7/Ti6Al4V10.4028/www.scientific.net/MSF.849.385 ↗
18. The microstructural observation and wettability study of brazing Ti-6Al-4V and 304 stainless steel using three braze alloys10.1023/A:1015356930476 ↗
19. Reactive wetting of low carbon steel by Al 4043 and 6061 alloys at 600–750 °C10.1016/j.surfcoat.2016.06.005 ↗
20. Wetting in high-temperature materials processing: the case of Ni/MgO and NiW10/MgO10.1016/j.scriptamat.2010.03.003 ↗
21. The mystery of molten metal
22. Eustathopoulos · 1999
23. Characteristics of precursor film in the wetting of Zr-based alloys on ZrC substrate at 1253 K10.1016/j.tsf.2014.02.074 ↗
24. Aluminium–silicon–titanium
25. Zhuang · 1989
26. Interfacial reaction wetting in the boron nitride/molten aluminum system10.1016/0956-7151(93)90111-5 ↗
27. Fabrication of transparent silica glass by powder sintering10.1016/S1468-6996(02)00030-X ↗
28. The role of intermetallics in wetting in metallic systems10.1016/S1359-6462(01)01181-2 ↗
29. Si diffusion behavior during laser welding-brazing of Al alloy and Ti alloy with Al-12Si filler wire10.1016/S1003-6326(09)60098-4 ↗
30. Precursor film of tin-based active solder wetting on ceramics10.1007/BF00400889 ↗
31. Wetting: statics and dynamics10.1103/RevModPhys.57.827 ↗
32. The flow of liquid metals on solid metal surfaces and its relation to soldering, brazing, and hot-dip coating
33. The spreading kinetics and precursor film characteristics of Zr-based alloy melt on W substrate10.1016/j.matlet.2013.02.005 ↗
34. Gale · 1998
35. Metal-ceramic interactions: III, surface tension and wettability of metal-ceramic systems10.1111/j.1151-2916.1954.tb13972.x ↗