Temperature-induced wear micro-mechanism transition in additively deposited nickel alloys with different solid lubricants
Source abstract
Abstract
Additive manufacturing of self-lubricating alloys plays a crucial role in the production of complex wear-resistant components and in expanding repair capabilities, especially for intricate wear parts with low tolerances (e.g. with cooling channels). Herein, we report a novel approach providing nickel-based alloy with an excellent tribological performance in dry sliding contacts. Laser-deposited self-lubricating nickel alloys, infused with anti-wear additives of molybdenum disulfide, nickel sulfide, copper sulfide, or bismuth sulfide, were subjected to dry sliding wear tests against an alumina ball counterbody at a temperature range of up to 800 °C. The self-lubricating alloys exhibited a significant decline in friction (43 %) and wear (45 %) at room temperature, 400 °C (friction 40 %, wear rate 55 %), and 600 °C (MoS 2-based, friction 58 %, wear rate 75 %). The MoS 2-based alloy coating demonstrated excellent performance characteristics up to 800 °C (friction coefficient ⁓0.25, wear rate 11 × 10 −6 mm 3 N −1 m −1 ) due to the formation of a ‘glazed’ tribolayer. Wear mapping allowed to identification of a critical condition for self-lubricating alloys where positive transitions in wear mechanisms led to a synergistic lubrication mode involving the formation of tribologically induced new lubricious phases such as silver molybdate or nickel-bismuth intermetallic. This work provides a comparative evaluation of the micromechanisms, surface transitions, and tribochemistry of solid lubricants at a wide temperature range and a variety of applications.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Lubricants and Their Additives · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (82)
Show source-provided references
1. Influence of tribology on global energy consumption, costs and emissions10.1007/s40544-017-0183-5 ↗
2. Ecotribology: Environmentally acceptable tribological practices10.1016/j.triboint.2005.07.002 ↗
3. Future perspectives on sustainable tribology10.1016/j.rser.2012.02.064 ↗
4. Role of additive manufacturing in industry 4.0
5. Solid lubrication at high-temperatures—a review10.3390/ma15051695 ↗
6. Intelligent lubricating materials: a review10.1016/j.compositesb.2020.108450 ↗
7. Kumar · 2022
8. Microstructure and high temperature tribological behaviour of self-lubricating Ti-TiBx composite doped with NiBi10.1016/j.surfcoat.2022.128827 ↗
9. Remanufacture of hot forging dies by LMD-p using a cobalt based hard-facing alloy10.1007/s00501-021-01108-z ↗
10. Environmentally benign tribo-systems for metal forming10.1016/j.cirp.2010.05.007 ↗
11. Hot sliding wear of 88 wt.% TiB–Ti composite from SHS produced powders10.3390/ma14051242 ↗
12. Tribological behaviour of self-lubricating materials at high temperatures10.1080/09506608.2017.1410944 ↗
13. Nanoparticles as novel lubricating additives in a green, physically based lubrication technology for DLC coatings10.1016/j.wear.2013.03.009 ↗
14. Progress in sustainable recycling and circular economy of tungsten carbide hard metal scraps for industry 5.0 and onwards
15. Recycling prospect and sustainable lubrication mechanism of water-based MoS2 nano-lubricant for steel cold rolling process10.1016/j.jclepro.2020.123991 ↗
16. Assessment of 3D printed steels and composites intended for wear applications in abrasive, dry or slurry erosive conditions10.1016/j.ijrmhm.2019.105126 ↗
17. Design and fabrication of conformal cooling channels in molds: review and progress updates10.1016/j.ijheatmasstransfer.2021.121082 ↗
18. Additive manufacture of tools and dies for metal forming
19. Defects in additive manufacturing and their influence on structural integrity
20. Advanced cutting conditions for the milling of aeronautical alloys10.1016/S0924-0136(99)00372-6 ↗
21. Wear mechanisms analysis for turning Ti-6Al-4V-towards the development of suitable tool coatings10.1007/s00170-011-3427-y ↗
22. Bioinspired and multifunctional tribological materials for sliding, erosive, machining, and energy-absorbing conditions: a review10.3390/biomimetics9040209 ↗
23. Surface post-treatments for metal additive manufacturing: progress, challenges, and opportunities
24. Tribological measures for controlling material flow in sheet-bulk metal forming10.1007/s11740-016-0695-2 ↗
25. Analysis of surface finishing mechanism in a newly developed rotational magnetorheological honing process for its productivity improvement10.1016/j.wear.2019.01.001 ↗
26. Maintenance and repair of gas turbine components
27. Remanufacturing of turbine blades by laser direct deposition with its energy and environmental impact analysis10.1016/j.jclepro.2014.05.084 ↗
28. Recent trends in laser cladding and surface alloying10.1016/j.optlastec.2020.106619 ↗
29. Compositionally graded metals: a new frontier of additive manufacturing10.1557/jmr.2014.208 ↗
30. Opportunities and challenges in additive manufacturing of functionally graded metallic materials via powder-fed laser directed energy deposition: a review10.1016/j.jmatprotec.2021.117117 ↗
31. Tribology of additively manufactured materials: fundamentals, modeling, and applications
32. Developing a sustainable omnichannel strategic framework toward circular revolution: an integrated approach
33. Assessment of self-lubricating coated cutting tools fabricated by laser additive manufacturing technology for friction-reduction10.1016/j.jmatprotec.2023.118010 ↗
34. High-temperature sliding wear of metals10.1016/S0301-679X(02)00041-5 ↗
35. Sliding wear performance of in-situ spark plasma sintered Ti-TiBw composite at temperatures up to 900 °C
36. Mechanisms of sliding wear of metals and alloys at elevated temperatures10.1016/j.triboint.2007.10.003 ↗
37. Transfer, mixing and associated chemical and mechanical processes during the sliding of ductile materials10.1016/S0043-1648(00)00460-9 ↗
38. A. R. Lansdown, “High-temperature Lubrication”.
39. Synergistic lubrication mechanisms of AISI 4140 steel in dual lubrication systems of multi-solid coating and oil lubrication10.1016/j.triboint.2022.107484 ↗
40. Solid lubrication with MoS2: a review10.3390/lubricants7070057 ↗
41. Molybdenum disulfide as a lubricant and catalyst in adaptive nanocomposite coatings10.1016/j.surfcoat.2006.08.014 ↗
42. Reactive formation of a few 2D layers of MoS2 using triboactive Mo surfaces and their interaction with anti-wear additives and dispersants10.1016/j.wear.2023.204756 ↗
43. Tribological behavior of Ni-based self-lubricating claddings containing sulfide of nickel, copper, or bismuth at temperatures up to 600 °C10.1016/j.surfcoat.2023.129270 ↗
44. A Ni-Bi self-lubricating Ti6Al4V alloy for high temperature sliding contacts10.1016/j.jallcom.2023.169216 ↗
45. Solid lubricity of WS2 and Bi2S3 coatings deposited by plasma spraying and air spraying
46. Tribological properties of bismuth sulfide (Bi2S3) particles as grease additive for aluminum forming operations
47. Sliding wear behaviour of WC-Co reinforced NiCrFeSiB HVOAF thermal spray coatings against WC-Co and Al2O3 counterbodies10.1016/j.surfcoat.2020.125468 ↗
48. Effect of counterbody on the dry sliding wear performance of plasma sprayed calcia-stabilized zirconia coating10.1016/j.ijrmhm.2020.105284 ↗
49. High-temperature dry sliding wear behavior of additively manufactured austenitic stainless steel (316L)
50. Influence of laser metal deposition direction in the abrasive and adhesive wear resistance of Ni-Cr-B-Si coatings10.2351/7.0000099 ↗
51. High temperature hardness of steels and iron-based alloys10.1016/j.msea.2016.06.058 ↗
52. High-temperature wear performance of hBN-added Ni-W composites produced from combustion-synthesized powders10.3390/ma15031252 ↗
53. The effect of temperature and sliding speed on friction and wear of Si3N4, Al2O3, and ZrO2 balls tested against AlCrN PVD coating10.1016/j.triboint.2017.05.035 ↗
54. Synergistic effect of Ag and MoS2 on high-temperature tribology of self-lubricating NiCrBSi composite coatings by laser metal deposition
55. Tribological performance of iron- and nickel-base self-lubricating claddings containing metal sulfides at high temperature10.1007/s40544-021-0578-1 ↗
56. NiCrSiBC coatings: effect of dilution on microstructure and high temperature tribological behavior10.1016/j.wear.2016.01.015 ↗
57. Lubrication behavior of Ni–Cr-based alloys containing MoS2 at high temperature10.1016/S0043-1648(01)00803-1 ↗
58. Surface-driven bulk reorganization of gold nanorods10.1021/nl051149h ↗
59. Equilibrium shape and temperature; Lead on graphite10.1016/S0039-6028(83)80036-3 ↗
60. High temperature lubricants — oils and greases10.1016/0301-679X(83)90072-5 ↗
61. High-temperature fluid lubrication10.1080/05698196408972050 ↗
62. Effects of magnetic ionic liquid as a lubricant on the friction and wear behavior of a steel-steel sliding contact under elevated temperatures10.1007/s40544-019-0324-0 ↗
63. Wear mechanism of Ag as solid lubricant for wide range temperature application in micro-beam plasma cladded Ni60 coatings10.1016/j.triboint.2021.107402 ↗
64. A crystal chemical approach to the formulation of self-lubricating nanocomposite coatings10.1016/j.surfcoat.2005.08.054 ↗
65. The dual role of metal sulfides as lubricant and abrasive: an interface study in friction composite10.1088/2053-1591/aafd5a ↗
66. Effect of cBN content and additives on sliding and surface fatigue wear of spark plasma sintered Al2O3-cBN composites
67. Oxidation behavior of GTD111 Ni-based superalloy at 900 °C in air10.1016/j.corsci.2015.07.031 ↗
68. High temperature corrosion behavior of DS GTD-111 in oxidizing and sulfidizing environments
69. Preparation and high temperature tribological properties of laser in-situ synthesized self-lubricating composite coatings containing metal sulfides on Ti6Al4V alloy10.1016/j.apsusc.2019.03.092 ↗
70. Enhancing tribological performance of NiAl–Bi2O3–Cr2O3 composite coating via in-situ grown NiBi compound
71. Transfer during unlubricated sliding wear of selected metal systems10.1016/0043-1648(85)90005-5 ↗
72. Surface energy, surface topography and adhesion10.1016/S0143-7496(03)00068-X ↗
73. Elevated-temperature tribology of metallic materials10.1016/j.triboint.2010.01.003 ↗
74. Effect of temperature and load on three-body abrasion of cermets and steel10.1016/j.triboint.2011.06.029 ↗
75. A wear map of bearing steel lubricated by silver films10.1016/S0043-1648(03)00148-0 ↗
76. Regimes of soft lubrication10.1017/jfm.2021.96 ↗
77. B. H. and F. A., “Tribological stability of metallic materials at elevated temperatures,” Wear, vol. 162–164, pp. 441–449.10.1016/0043-1648(93)90528-T ↗
78. Antigalling and low friction properties of a laser processed Co-based material10.2351/1.1514218 ↗
79. Czichos · 2009
80. Extreme grain refinement by severe plastic deformation: a wealth of challenging science10.1016/j.actamat.2012.10.038 ↗
81. Microstructure and the wear mechanism of grain-refined aluminum during dry sliding against steel disc10.1016/j.wear.2007.05.010 ↗
82. Effect of Ti on the wear behavior of AlCoCrFeNi high-entropy alloy during unidirectional and bi-directional sliding wear processes10.1016/j.wear.2021.203650 ↗