An experimental study to corelate water jet impingement erosion resistance and properties of metallic materials and coatings
Source abstract
Abstract
Abstract This paper describes the water jet impingement erosion characteristics of titanium alloy (Ti6Al4V), Hadfield steel, laser hardened, plasma nitrided and pack borided 12Cr steel along with most commonly used steels in hydro turbines. Round samples as per ASTM G73-98 were tested for water jet impingement erosion study. While testing, in the incubation period, plasma nitrided and pack borided 12Cr steel performed much better than 12Cr and 13Cr4Ni steels. Plasma nitrided 12Cr steel performed much better than pack borided 12Cr steel. This is due to the integrity of plasma nitrided layers and their ability to absorb shocks due to jet impingement. During incubation as well as in the long run, Hadfield steel and laser hardened 12Cr steel performed exceptionally well followed by 17Cr4Ni ‘PH’ steel. Based on this experimental study, a suitable criterion based on ultimate resilience (UR) for metallic materials and a composite modified resilience (CMR) for hard metallic coatings has been discussed. Water jet impingement erosion test results along with the mechanical properties of materials and coatings, and their scanning electron microstructural details are reported in this paper.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Erosion and Abrasive Machining · Nuclear Materials and Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. International cavitation erosion test and quantitative assessment of material resistance to cavitation10.1016/S0043-1648(99)00195-7 ↗
2. F.J. Heymann, Conclusions from the ASTM inter-laboratory test programme with liquid impact erosion facilities, in: Proceedings of the 5th International Conference on Erosion by Liquid and Solid Impact, Cambridge, UK, 1979.
3. Cavitation damage and correlation with mechanical and fluid properties10.1115/1.3609699 ↗
4. R.T. Knapp, T.W. Daily, F.G. Hammitt, Cavitation, McGraw-Hill, New York, 1970.
5. Erosion by Cavitation or Impingement, ASTM STP 408, 1967, pp. 3–158.
6. W.F. Adler, The Mechanics of Liquid Impact Treatise on Materials Science and Technology, Vol. 16, 1979, pp. 127–183.
7. A statistical analysis of cavitation erosion pits10.1115/1.2926539 ↗
8. ASTM Standard for Liquid Impingement Erosion Testing, ASTM 1982, G73-82.
9. W.F. Adler (Ed.), Erosion, Prevention and Useful Application, ASTM STP 664, 1979.10.1520/STP35792S ↗
10. Erosion and Cavitation, ASTM STP 307, 1961.
11. C.M. Preece (Ed.), Treatise on materials science and technology, Erosion, Vol. 16, Academic Press, New York, NY, 1979.
12. Liquid jet impact on liquid and solid surfaces10.1016/0043-1648(95)07187-3 ↗
13. M.B. Lesser, J.E. Field, The impact of compressible liquids, in: M.U. Dyke, J.V. Wehausen, J.L. Lumley (Eds.), Annual Review of Fluid Mechanics, Vol. 15, Annual Review Inc., Palo Alto, CA, 1983, pp. 73–122.10.1146/annurev.fl.15.010183.000525 ↗
14. Liquid impact resistance of a range of IR-transparent materials10.1016/0043-1648(95)07150-4 ↗
15. Synergistic effects of rain and sand erosion10.1016/S0043-1648(00)00367-7 ↗
16. Correlation of cavitation erosion behaviour with mechanical properties of metals10.1016/0043-1648(90)90122-Q ↗
17. A metallurgical approach to improve cavitation-erosion resistance10.1007/s11665-997-0057-5 ↗
18. Characteristics and Determination of Erosion resistance, ASTM STP 474, 1970.
19. Cavitation erosion of metals and alloys10.1016/0043-1648(84)90199-6 ↗
20. Cavitation erosion of titanium carbide coatings on cemented carbide and other substrates10.1016/0043-1648(83)90312-5 ↗
21. V.G. Behal, A.S. Melilli, Stainless Steel Castings, ASTM STP 756, 1982, pp. 315–403.
22. A new cast steel for hydraulic machinery
23. Cavitation-erosion studies with venturi and rotating disc in water10.1115/1.3425070 ↗
24. A. Thiruvengadam, S. Waring, Mechanical properties of metals and cavitation damage resistance, J. Ship Res. March (1966) 1–9.10.5957/jsr.1966.10.1.1 ↗
25. A. Thiruvengadam, Theory of erosion hydronautics, Incorporated Technical Report 233-11, March 1967 (also see, Proceedings of the 2nd Meersburg Conference on Rain Erosion, Royal Aircraft Establishment, Farnborough, UK, August 1967).
26. Cavitation erosion characteristics of nickel based alloy-composite coatings obtained by plasma spraying10.1016/0043-1648(85)90121-8 ↗
27. Boronising of cast martensitic chromium nickel stainless steel and its abrasion and cavitation-erosion behaviour10.1016/S0043-1648(96)07374-7 ↗
28. Cavitation erosion and pitting corrosion behaviour of laser surface melted martensitic stainless steel UNSS 4200010.1016/S0257-8972(00)00533-8 ↗
29. Laser surface modification of UNS S31603 stainless steel using NiCrSiB alloy for enhancing cavitation-erosion resistance10.1016/S0257-8972(98)00549-0 ↗
30. Wear properties of induction hardened, conventional plasma nitrided and pulse plasma nitrided AISI 4140 steel in dry sliding conditions10.1016/S0043-1648(99)00151-9 ↗
31. Microstructure and residual stresses of plasma nitrided M2 tool steel10.1016/S0257-8972(99)00063-8 ↗
32. A.M. Staines, T. Bell, Technological importance of plasma induced nitrided and carburized layers of steels, Thin Solid Films 86 (1981) 201–211.10.1016/0040-6090(81)90289-3 ↗
33. T. Bell, Z.L. Zhang, J. Lanagan, A.M. Staines, Plasma nitriding treatment for enhanced wear and corrosion resistance, Metallic and Inorganic Coatings, 1988, pp. 165–177 (Chapter 12).
34. T. Spalvins, in: Proceedings of the ASM International Conference on Ion Nitriding, Cleveland, OH, September 1986.
35. K. Kawagishi, S. Kawasaki, et al., Protective design and boride coating against solid particle erosion of first-stage turbine nozzle, Advances in Steam Turbine Technology for Power Generation PWR-10, 1990, pp. 23–29.
36. A. Barletta, A. Ball, The cavitation-erosion of coated and surface treated steels, ICM, 4, 2, 421–428.10.1016/B978-1-4832-8372-2.50051-8 ↗
37. Abrasive and erosive wear characteristics of plasma nitriding and HVOF coatings: their application in hydro turbines10.1016/S0043-1648(01)00537-3 ↗
38. B. Bajic, Intelligent cavitation diagnostics and monitoring, Int. Water Power Dam Constr. May (2001) 33–36.