journal article·2007-05Open access

The effectiveness of PTFE nanoparticle powder as an EP additive to mineral base oils

E. Fernández Rico, I. Minondo, D. García Cuervo

Wear· Volume 262· Issue 11-12

Abstract

Abstract This paper describes experiments using a four-ball tester to evaluate the extreme pressure (EP) and wear reduction properties of AISI 52100 steel balls with several mineral oils with and without additive. The lubricants studied include PTFE nanoparticle powder as an additive in different percentages with SN-350 and Bright Stock as mineral base oils with very different viscosities (9 and 32.4 cSt, respectively, at 100 °C). Plots of wear scar diameters versus applied loads, load wear indexes and weld points are given for all the lubricants that were tested. The contact angle for the different oils tested both with and without additive is estimated experimentally in order to provide some understanding of the behaviour described in the results. Results indicate a reduction of the average scar in the three lower balls and an increase of the Welding Point for both oils. They also point to an increase in the load wear index (LWI) in line with increasing percentages of additive. The oil specimens with EP antiwear additive had higher welding loads, higher load wear indexes and smaller scars for the same load. The topography and surface chemistry of the ball-bearing specimens were examined using scanning electron microscopy and LINK techniques, respectively, thereby highlighting the protection mechanism of the additive, which works either by mechanical deformation or by filling the micro-cracks.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tribology and Wear Analysis · Lubricants and Their Additives · Mechanical stress and fatigue analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Energy saving lubricants containing colloidal PTFE
2. Behavior of PTFE suspensions in rolling/sliding contacts
3. Bhushan · 1991
4. Effect of two-phase liquid lubricant on fatigue life10.1016/S0043-1648(96)07213-4 ↗
5. ASTM D 2266-86, Standard Test Method for Wear Preventive Characteristics of Lubricanting Grease (Four-Ball Metohd).
6. Stanhope—Sheta Ltd. London N.E. 2, “Manual for the Sheta-Shell four ball E.P. Lubricant testing machine” No 29–72 (1980).
7. The tribological behaviour of ZnO nanoparticles as an additive to PAO610.1016/j.wear.2005.10.001 ↗
8. The load-carrying properties of certain S-alkylisothiamides and their efectiveness as EP lubricant additives10.1016/0043-1648(81)90231-3 ↗
9. The role of certain substituted 2-amino-benzothiazolylbenzoylthiocarbamides as additives in extreme pressure lubrication of steel bearing balls10.1016/0043-1648(90)90156-5 ↗
10. Miller · 1969
11. Hesse · 1999
12. Halling · 1975
13. Influence of surface wettability on friction wear test10.1016/S0043-1648(98)00256-7 ↗
14. The behavior of suspended solid particles in rolling and sliding EHL contacts10.1080/10402008808981793 ↗
15. Behavior of colloidally-dispersed solid particles in very thin film lubricated contacts
16. Mechanism of action of colloidal solid dispersions10.1115/1.1537752 ↗
17. The behavior of colloidal solid particles in lubricated contacts10.1080/10402000008982354 ↗