Unlubricated gross slip fretting wear of metallic plasma-sprayed coatings for Ti6Al4V surfaces
Source abstract
Abstract
Plasma-sprayed Al–bronze or CuNiIn coatings are often applied to protect against fretting wear and extend the operational life of Ti-alloy compressor blades in turbine engines. In order to develop a fundamental understanding of how these coating systems perform under gross slip fretting conditions, bench level fretting wear tests were conducted at room temperature to simulate cold engine startup. Alternative coatings such as plasma-sprayed molybdenum and nickel were also evaluated because of their potential for reducing fretting wear under certain simulated engine conditions. The combination of scanning electron microscopy (SEM), surface profilometry, surface chemistry (EDS), and friction analysis were used to study coating performance and evaluate the interfacial wear mechanisms. In this study, it was determined that all coatings caused significant damage to the mating Ti6Al4V surfaces and that the wear mechanisms were all similar to those of the uncoated baseline case.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical stress and fatigue analysis · Metal and Thin Film Mechanics · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. The mechanisms of fretting––a review10.1016/0043-1648(70)90235-8 ↗
2. Fretting behavior of titanium alloys10.1080/10402009308983158 ↗
3. Tribologically transformed structure in fretting10.1016/S0043-1648(00)00464-6 ↗
4. Friction and surface behavior of selected titanium alloys during reciprocating sliding motion10.1016/S0043-1648(01)00517-8 ↗
5. Fretting fatigue10.1179/imr.1992.37.1.77 ↗
6. Fretting fatigue in engineering alloys10.1016/S0142-1123(97)00039-X ↗
7. Mechanisms of fretting fatigue and their impact on test methods development
8. Mixed fretting regime10.1016/0043-1648(94)07081-4 ↗
9. Microstructural characterization of Ti6Al4V subjected to fretting10.1115/1.1792677 ↗
10. Fretting fatigue crack analysis in Ti6Al4V10.1016/j.ijfatigue.2005.07.008 ↗
11. Elevated temperature evaluation of fretting and metal transfer between coated titanium components10.1080/10402000008982391 ↗
12. Protective coatings in the gas turbine engine10.1016/0257-8972(94)90129-5 ↗
13. Gross slip fretting wear analysis of aluminum bronze coatings for Ti6Al4V aerospace components
14. Effect of various surface conditions on fretting fatigue behavior of Ti6Al4V10.1016/S0142-1123(02)00050-6 ↗
15. Using a dovetail fixture to study fretting fatigue and fretting palliatives10.1115/1.2172272 ↗
16. The influence of temperature and wear mode on the deterioration of coatings used for titanium aircraft engine components10.1080/10402000208982539 ↗
17. Effect of surface treatments on fretting fatigue of Ti6Al4V10.1016/j.ijfatigue.2006.10.005 ↗
18. The Structure and mechanism of formation of the ‘glaze’ oxide layers produced on nickel-based alloys during wear at high temperatures10.1016/0010-938X(73)90030-9 ↗
19. The friction and wear behavior of nickel-base alloys in air at room temperature10.1016/0043-1648(73)90158-0 ↗
20. The tribological behavior of nickel–chromium alloys at temperatures from 20 to 800°C10.1016/0043-1648(76)90002-8 ↗
21. The influence of oxides on the friction and wear of alloys10.1016/0301-679X(78)90178-0 ↗
22. The use of coatings to control fretting wear at ambient and elevated temperatures10.1016/0043-1648(85)90102-4 ↗
23. Some frictional features associated with the sliding wear of the nickel-base alloy N80a at temperatures to 250°C10.1016/0043-1648(94)90146-5 ↗
24. The role of triboparticulates in dry sliding wear10.1016/S0301-679X(98)00027-9 ↗
25. Microscopy of glazed layers formed during high temperature sliding wear at 750°C10.1016/S0043-1648(03)00134-0 ↗
26. Hutchings · 1992
27. Characterization of mixed and gross slip fretting wear regimes in Ti6Al4V interfaces at room temperature10.1016/j.wear.2003.10.023 ↗
28. Deresiewicz · 1974
29. Wear analysis in fretting of hard coatings through dissipated energy concept10.1016/S0043-1648(96)07436-4 ↗
30. Gross slip criteria in fretting10.1016/0043-1648(93)90518-Q ↗
31. On fretting maps10.1016/0043-1648(88)90134-2 ↗
32. Fretting laboratory tests: analysis of the mechanical response of test rigs10.1023/A:1022368414455 ↗
33. Analysis of sliding behavior for fretting loadings: determination of transition criteria10.1016/0043-1648(94)06582-9 ↗
34. Mechanisms for transitional friction and wear behavior of sliding metals10.1016/0043-1648(81)90283-0 ↗
35. Plastic deformation and sliding friction of metals10.1016/0043-1648(79)90087-5 ↗
36. Material effects in fretting wear: application to iron, titanium, and aluminum alloys10.1007/BF02667367 ↗
37. Fretting: load carrying capacity of wear debris10.1115/1.3260881 ↗
38. Tomashov · 1966
39. The ploughing and adhesion of sliding metals10.1063/1.1714954 ↗