Effects of high-pressure cooling in the flank and rake faces of WC tool on the tool wear mechanism and process conditions in turning of alloy 718
Source abstract
Abstract
The exceptional properties of Heat Resistant Super Alloys (HRSA) justify the search for advanced technologies that can improve the capability of machining these materials. One such advanced technology is the application of a coolant at high pressure while machining, a strategic solution known for at least six decades. The aim is to achieve extended tool life, better chip control and improved surface finish. Another aim is to control the temperature in the workpiece/tool interface targeting for optimum cutting conditions. In most of the existing applications with high-pressure coolant media, the nozzles are positioned on the rake face side of the insert and they are directed towards the cutting edge (the high-temperature area). The coolant is applied at high-pressure to improve the penetration of the cooling media along the cutting edge in the interface between the insert and workpiece material (chip) as well as to increase chip breakability. However, the corresponding infusion of coolant media in the interface between the flank face of the insert and the work material (tertiary shear zone) has been previously only scarcely addressed, as is the combined effect of coolant applications on rake and clearance sides of the insert. The present work addresses the influence of different pressure conditions in (flank: 0, 4 and 8 MPa; rake: 8 and 16 MPa) on maximum flank wear, flank wear area, tool wear mechanism, and overall process performance. Round uncoated inserts are used in a set of face turning experiments, conducted on the widely used HRSA “Alloy 718” and run in two condition tests with respect to cutting speed (45 (low) and 90 (high) m/min). The results show that an increase in rake pressure from 8 to 16 MPa has certainly a positive impact on tool life. Furthermore, at higher vc of 90 m/min, cutting edge deterioration: due to an extensive abrasion and crack in the wear zone were the dominant wear mechanism. Nevertheless, the increase in coolant pressure condition to 16 MPa reduced the amount of abrasion on the tool compared to 8 MPa. At the lower cutting speed, no crack or plastic deformation or extensive abrasion were found. When using 8 MPa pressure of coolant media on the flank, the wear was reduced by 20% compared to flood cooling conditions. Application of high-pressure cooling on the flank face has a positive effect on tool life and overall machining performance of Alloy 718.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced machining processes and optimization · Advanced materials and composites · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Tool wear on nickel alloys with different coolant pressures: comparison of Alloy 718 and Waspaloy10.1016/j.jmapro.2017.01.012 ↗
2. An overview of the machinability of aeroengine alloys10.1016/S0924-0136(02)01042-7 ↗
3. Pigott · 1952
4. Vosough · 2005
5. Effect of high-pressure coolant supply when machining nickel-base, Inconel 718, alloy with coated carbide tools10.1016/j.jmatprotec.2004.04.329 ↗
6. “Tool life and wear mechanisms in high speed machining of Ti–6Al–4V alloy with PCD tools under various coolant pressures10.1016/j.jmatprotec.2013.03.008 ↗
7. Evaluation of energy efficiency in cutting aerospace materials with high-pressure cooling lubricant supply10.1007/s12541-014-0454-2 ↗
8. EDS analysis of flank wear and surface integrity in machining of alloy 718 with forced coolant application10.1016/j.procir.2016.02.144 ↗
9. Investigation of micro-textured cutting tools used for face turning of alloy 718 with high-pressure cooling10.1016/j.jmapro.2018.12.023 ↗
10. Geometry and volume measurement of worn cutting tools with an optical surface metrology device
11. ISO 3685:1993 · 2011
12. Influence of surface features for increased heat dissipation on tool wear10.3390/ma11050664 ↗
13. Oxford Instruments · 2011
14. Trent · 2000
15. Tool wear mechanisms in the machining of Nickel based super-alloys: a review10.1007/s11465-014-0301-2 ↗
16. Klocke · 2011
17. Ndlovu · 2009
18. Analysis of tool wear patterns in finishing turning of Inconel 71810.1016/j.wear.2012.11.004 ↗
19. Altintas · 2012
20. The effect of high-pressure coolant supply when machining a heat-resistant nickel-based superalloy
21. Machining of nickel-base, Inconel 718, alloy with ceramic tools under finishing conditions with various coolant supply pressures10.1016/j.jmatprotec.2005.02.144 ↗
22. The effect of a high-pressure jet on machining
23. Effects of high-pressure cooling on the wear patterns on turning inserts used on alloy IN71810.1080/10426914.2016.1244838 ↗
24. Wear and tribological performance of different ceramic tools in dry high speed machining of Ni-Co-Cr precipitation hardenable aerospace superalloy
25. Wear on SiC-whiskers reinforced ceramic inserts when cutting Inconel with waterjet assistance10.1080/10402009908982243 ↗
26. Investigation on machining performance of Inconel 718 under high pressure cooling conditions10.5545/sv-jme.2012.730 ↗
27. Klocke · 2011
28. The effects of cutting speed on tool wear and tool life when machining Inconel 718 with ceramic tools10.1016/j.matdes.2006.09.004 ↗
29. Influence of high-pressure flushing through the rake face of the cutting tool10.1016/S0007-8506(07)61162-7 ↗
30. Using high pressure coolant in the drilling and turning of low machinability alloys10.1007/s001700050012 ↗
31. Effect of high-pressure coolant supplies when machining nickel-base, Inconel 718, alloy with ceramic tools10.1080/10402000308982667 ↗
32. Investigation of machining performance in high-pressure jet assisted turning of Inconel 718: an experimental study10.1016/j.ijmachtools.2009.07.010 ↗
33. The machinability of nickel-based alloys in high-pressure jet assisted (hpja) turning
34. Influence of the lubricoolant strategy on thermo-mechanical tool load10.1016/j.cirpj.2013.09.001 ↗