journal article·2017-08

Surface crack formation on rails at grinding induced martensite white etching layers

Carsten Jørn Rasmussen, Søren Fæster, Somrita Dhar, Jesper Viggo Quaade, Manuel Bini, Hilmar Kjartansson Danielsen

Wear· Volume 384-385
Publisher page

Abstract

Abstract The connection between profile grinding of rails, martensite surface layers and crack initiation has been investigated using visual inspection, optical microscopy and 3D X-ray computerized tomography. Newly grinded rails were extracted and found to be covered by a continuous surface layer of martensite with varying thickness formed by the grinding process. Worn R350HT and R200 rails were extracted from the Danish rail network as they had transverse bands resembling grinding marks on the running surface. The transverse bands were shown to consist of martensite which had extensive crack formation at the martensite/pearlite interface. The cracks in R350HT propagated down into the rail while those in the soft R200 returned to the surface causing only very small shallow spallation. The transverse bands had the same shape, size, orientation, location and periodicity which would be expected from grinding marks, showing a clear connection between grinding and crack initiation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced machining processes and optimization · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Thermal model and temperature field in rail grinding process based on a moving heat source10.1016/j.applthermaleng.2016.06.071 ↗
2. Analytical 1D model for analysis of the thermally affected zone formed during railway wheel skid10.1016/S0043-1648(99)00167-2 ↗
3. The “magic” wear rate
4. Rolling contact fatigue of white etching layer Part 1 Crack morphology10.1016/j.wear.2007.01.003 ↗
5. Rolling contact fatigue of white etching layer Part 2 Numerical results10.1016/j.wear.2007.01.002 ↗
6. Microstructural evaluation and interpretation of the mechanically and thermally affected zone under railway wheel flats10.1016/S0043-1648(99)00166-0 ↗
7. Investigation of white etching layers on rails by optical microscopy, electron microscopy, X-ray and synchrotron X-ray diffraction10.1016/S0921-5093(00)01842-6 ↗
8. Microstructure features on rolling surfaces of railway rails subjected to heavy loading10.1016/S0921-5093(03)00327-7 ↗
9. Microstructural investigation of white etching layer on pearlite steel rail10.1016/j.msea.2006.01.033 ↗
10. Formation of white-etching layers on rail treads10.1016/0043-1648(95)06733-7 ↗
11. C.J. Rasmussen, X. Zhang, H.K. Danielsen, S. Fæster, Grinding induced martensite on the surface of rails, Risoe International Symposium on Materials Science. Proceedings 35439-446, 2014.
12. Rolling contact fatigue in relation to rail grinding10.1016/j.wear.2016.03.015 ↗
13. 3D characterization of rolling contact fatigue crack networks10.1016/j.wear.2016.06.027 ↗
14. Joint investigations on squats at Banedanmark