Abstract Oil and gas pipelines operate under severe mechanical and chemical conditions, which could lead to catastrophic failure. Electroless nickel-phosphorous (Ni-P) coatings are an excellent candidate for protection against wear and corrosion for oil and gas pipelines. Ni-P coatings exhibit superior corrosion resistance over many commercially available coatings, as well as high hardness. However, electroless Ni-P coatings suffer from low toughness, which has limited its use in applications where high scratch and dent resistance is required. To enhance the toughness of the Ni-P coatings, nano-sized particles of superelastic NiTi alloy were incorporated within the coating. In the present work novel Ni-P-nano-NiTi composite coating has been successfully plated on API X100 pipe steel. Scratch tests under constant and increasing loads were performed to determine the effect of NiTi nano-particles on wear damages. Indentation tests were carried out to assess the dent resistance and crack modes of the coating. The addition of superelastic nano-particles into the Ni-P matrix led to toughening through transformation toughening, crack bridging, deflection, and microcracking. The composite coatings exhibited lower hardness in comparison to monolithic Ni-P coatings, but still provided considerable improvement upon the steel substrate. Optical and scanning electron examinations showed evidence of delamination, radial, and Hertzian cracking, as well as a reduction in crack length with the addition of superelastic NiTi.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Indentation and erosion behaviour of electroless Ni-P coating on pipeline steel10.1016/j.wear.2016.12.054 ↗
2. FP-based formulations as protective coatings in oil/gas pipelines10.1016/j.porgcoat.2015.06.028 ↗
3. Nickel plating on steel by chemical reduction10.6028/jres.037.019 ↗
4. Electroless nickel, alloy, composite and nano coatings - A critical review10.1016/j.jallcom.2013.03.107 ↗
5. Effect of reducing agent and nano Al2O3 particles on the properties of electroless Ni-P coating10.1016/j.apsusc.2014.04.092 ↗
6. Taheri · 2003
7. The effect of hydrogen on plastic deformation of electroless nickel phosphorous amorphous coating10.1016/j.msea.2006.07.122 ↗
8. Synthesis and tribological behaviour of electroless Ni-P-WS2 composite coatings10.1016/j.apsusc.2012.09.051 ↗
9. Tribology of electroless nickel coatings- a review10.1016/j.matdes.2010.11.013 ↗
10. Influence of SiO2 nanoparticles on hardness and corrosion resistance of electroless Ni-P coatings10.1016/j.surfcoat.2014.11.044 ↗
11. Preparation and characterization of Ni-P/nanodiamond coatings: Effects of surfactants10.1016/j.diamond.2012.10.003 ↗
12. Dent resistance and effect of indentation loading rate on superelastic TiNi alloy10.1007/s11661-013-1727-6 ↗
13. Neupane · 2014
14. Impact damage resistance and damage suppression properties of shape memory alloys in hybrid composites-a review10.1088/0964-1726/20/1/013001 ↗
15. Taya · 1989
16. Microcrack toughening in brittle materials containing weak and strong interfaces10.1016/1359-6454(96)00002-X ↗
17. Ductile phase toughned brittle materials
18. Transformation induced crack deflection in a metastable titanium alloy and implications on transformation toughening10.1016/j.actamat.2016.07.041 ↗
19. Toughening by stress-induced microcracking in two-phase ceramics10.1111/j.1151-2916.1988.tb06419.x ↗
20. Mechanisms of fatigue crack propagation inMetals, ceramics and composites: role of crack tip shielding10.1016/0025-5416(88)90547-2 ↗
21. Fundamental formulation for transformation toughening10.1016/j.ijsolstr.2010.08.002 ↗
22. Indentation and bending behavior of electroless Ni-P-Ti composite on pipeline steel10.1016/j.surfcoat.2017.10.074 ↗
23. Electrochemical impedance spectroscopy and indentation studies of pure and composite electroless Ni-P coatings10.1016/j.surfcoat.2013.09.057 ↗
24. Characterization and corrosion resistance of duplex electroless Ni-P composite coatings on magnesium alloy10.1016/j.surfcoat.2013.05.047 ↗
25. Preparation of the Ni-P composite coating co-deposited by nano TiC particles and evaluation of it's corrosion property10.1016/j.apsusc.2011.10.101 ↗
26. Development of high performance electroless Ni-P-HNT composite coatings10.1016/j.apsusc.2012.09.020 ↗
27. Preparation and corrosion resistance of electroless Ni-P/SiC funtionally gradient coatings on AZ91D magnesium alloy10.1016/j.apsusc.2013.09.079 ↗
28. The influence of the phosphorous content and heat treatment on the nano-micro-structure, thickness and micro-hardness of electroless Ni-P coatings on steel10.1016/j.apsusc.2017.06.168 ↗
29. On the deformation of superelastic TiNi alloy10.1007/s11249-009-9507-6 ↗
30. Enhanced surface hardness by boron implantation in nitinol alloy10.1016/S0099-2399(96)80015-X ↗
31. Role of some plating parameters in the properties of Ni-P/Al2O3 nanocomposite coatings on Mg alloy10.20964/2016.08.67 ↗
32. Electroless Ni-P composite coatings10.1023/A:1025572410205 ↗
33. Fischer-Cripps · 2007
34. Electroless nickel phosphorous plating on carbon steel
35. Young's modulus and Poisson's ratio of CVD diamond10.1016/0925-9635(93)90250-6 ↗
36. Nanoindentation and nanoscratch behavior of electroless deposited nickel-phosphorous coating10.1016/j.matchemphys.2016.04.022 ↗
37. Indentation-based methods to assess fracture toughness for thin coatings10.1088/0022-3727/45/20/203001 ↗
38. Effects of NiTi additions on the microstructure and mechanical properties of Ti(C,N)-based cermets10.1016/j.ijrmhm.2013.04.003 ↗