Abstract In order to improve the surface tribological properties of TC4 titanium alloy, this paper used laser processing technology to prepare a cell-like texture on TC4 surface. The cells of cell-like texture were separated by regular cracks caused by recasting of TC4, which could be got at the parameters of 1 μm distance of adjacent laser spots and 2.5 μm patch of adjacent laser paths with a certain laser power density. The laser treatment increased the surface microhardness from 351 to 445 HV. The relationship between tribological properties of TC4 and the laser power density was studied. At 0.32 GW/cm2, under the lubricant of simulated body fluid (SBF), the average friction coefficient between TC4 and UHMWPE reduced significantly by 32.4%, and the wear rate of UHMWPE ball decreased by 59%, compared with the original surface. The cell-like texture could increase the transmission speed of the lubricant at the friction interface by three times with the help of capillary force, and it could also store lubricant in the texture to improve the tribological performance. The channels around cells were assumed to be rectangular groove. The width of the channel which was observed with a 3D confocal microscope was 3.2 μm, and the capillary force produced by a single rectangular groove was calculated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tribology and Lubrication Engineering · Adhesion, Friction, and Surface Interactions · Laser-induced spectroscopy and plasma

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. An overview on application status and processing technology development of titanium alloy
2. Titanium in biomedical applications—properties and fabrication: a review[J]10.1166/jbt.2015.1361 ↗
3. Durability evaluation of biopolymer coating on titanium alloy substrate10.1016/j.jmbbm.2014.03.003 ↗
4. Micro-scale abrasive wear behavior of medical implant material Ti-25Nb-3Mo-3Zr-2Sn alloy on various friction pairs10.1016/j.msec.2014.05.039 ↗
5. Research progress on laser surface modification of titanium alloys10.1016/j.apsusc.2004.08.011 ↗
6. Mitigation of abrasive wear damage of Ti–6Al–4V by laser surface alloying10.1016/j.matdes.2015.02.010 ↗
7. Microstructure and wear resistance of laser clad Ti5Si3/NiTi2 intermetallic composite coating on titanium alloy10.1016/S0921-5093(02)00076-X ↗
8. Potential for adhesive wear in friction couples of UHMWPE running against oxidized zirconium, titanium nitride coatings, and cobalt-chromium alloys10.1002/jbm.b.31604 ↗
9. Vibration damping performance of ZrTiN coating deposited by arc ion plating on TC4 Titanium alloy10.1016/j.surfcoat.2012.05.140 ↗
10. Characterization and tribological investigation of sol–gel ceramic films on Ti–6Al–4V10.1016/j.wear.2005.05.006 ↗
11. Fretting wear study on micro-arc oxidation TiO2 coating on TC4 titanium alloys in simulated body fluid10.1007/s11249-010-9665-6 ↗
12. Enhanced wear resistance of titanium surfaces by a new thermal oxidation treatment10.1016/S0043-1648(99)00359-2 ↗
13. Laser peening of metals - enabling laser technology
14. Effect of laser peening on residual stress and micro-hardness of TC4 titanium alloy10.4028/www.scientific.net/AMR.710.208 ↗
15. Anodization of TC4 alloy and friction and wear property with PTFE composite coating
16. Surface modifications induced by pulsed-laser texturing-Influence of laser impact on the surface properties10.1016/j.apsusc.2013.10.069 ↗
17. Laser shock processing: a review of the physics and applications10.1007/BF00326477 ↗
18. Laser modification of the materials surface layer - a review paper
19. Investigation on the microstructure and creep behavior of laser remelted thermal barrier coating10.1016/j.surfcoat.2019.04.068 ↗
20. Adhesion and corrosion resistance of laser-oxidized titanium in potential biomedical application10.1016/j.surfcoat.2019.03.032 ↗
21. Laser-induced coloring of titanium alloy using ultraviolet nanosecond pulses scanning technology10.1016/j.jallcom.2017.04.290 ↗
22. Role of nano second laser wavelength embedded recast layer and residual stress on electrochemical corrosion of titanium alloy10.1088/2053-1591/ab1fb2 ↗
23. Effect of laser peening on friction and wear behavior of medical Ti6Al4V alloy10.1016/j.optlastec.2018.08.005 ↗
24. Growth characteristics and properties of micro-arc oxidation coating on SLM-produced TC4 alloy for biomedical applications10.1016/j.apsusc.2019.02.142 ↗
25. Mechanism and size characteristics of micro crack on polished Ti6A14V
26. A study of fatigue damage evolution on pulsed Nd:YAG Ti6Al4V laser welded joints10.1016/j.engfracmech.2014.01.005 ↗
27. On the use of infrared thermography for analysis of fatigue damage in Ti6Al4V-welded joints10.1007/s11665-014-1031-7 ↗
28. Influence of mechanical behavior on the wear of 4 clinically relevant polymeric biomaterials in a hip simulator10.1016/S0883-5403(00)90647-8 ↗
29. Preparation of a biomimetic nanocomposite scaffold for bone tissue engineering via mineralization of gelatin hydrogel and study of mineral transformation in simulated body fluid10.1002/jbm.a.34074 ↗
30. An · 2002 · vol. 3 · 226
31. Thermal effects of laser marking on microstructure and corrosion properties of stainless steel10.1364/AO.55.000D35 ↗
32. Structure formation on titanium during oxidation induced by cumulative pulsed Nd:YAG laser irradiation10.1007/s00339-002-2054-8 ↗
33. Thermodynamic evolution of phase explosion during high-power nanosecond laser ablation10.1103/PhysRevE.67.016410 ↗
34. The role of the phase explosion of metals in the explosive electron emission process
35. Precision micromachining with pulsed green lasers10.2351/1.521863 ↗
36. Sugioka · 2010 · vol. 135 · 1
37. Effect of nanosecond pulsed laser parameters and texture machining methods on surface texture flattening
38. Deformation and fracture of a mudflat-cracked laser-fabricated oxide on Ti10.1007/s10853-013-7217-9 ↗
39. Wetting considerations in capillary rise and imbibition in closed square tubes and open rectangular cross-section channels10.1007/s10404-013-1145-5 ↗