journal article·2010-02Open access

The wear performance of PEEK-OPTIMA based self-mating couples

S.C. Scholes, A. Unsworth

Wear· Volume 268· Issue 3-4

Abstract

Polymer-on-polymer wear couples have had limited investigation for use in orthopaedic implants but may provide engineers with new approaches for the design of medical devices such as in spinal arthroplasty or small joints of the extremities. In this study, the wear performance of polyetheretherketone (PEEK-OPTIMA) against itself, carbon fibre reinforced PEEK-OPTIMA (CFR-PEEK) against CFR-PEEK and alternative non-reinforced polyketones such as polyetherketoneetherketoneketone (PEKEKK) and polyetherketone (PEK) against themselves were investigated on a multidirectional pin-on-plate machine. PEKEKK against itself gave the highest wear. Whilst PEK/PEK gave lower wear factors than PEEK-OPTIMA/PEEK-OPTIMA, CFR-PEEK (both Pitch and PAN-based) against itself gave even lower wear. The PAN-based CFR-PEEK combination gave the lowest wear of all material combinations reported here. The average steady-state wear factor was found to be 5.44 × 10−6 mm3 N−1 m−1 for the PEKEKK/PEKEKK samples. This compares with the average steady-state wear factors of 0.300, 0.921, 1.64 and 4.5 × 10−6 mm3 N−1 m−1 for the CFR-PEEK PAN against itself, the CFR-PEEK Pitch against itself, PEK against itself and the PEEK-OPTIMA coupling respectively. Standard PEEK-OPTIMA against itself is currently used in a disc arthroplasty system which is undergoing clinical trials and it is possible that these material combinations may perform well in other prosthetic joints.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Tribology and Wear Analysis · Total Knee Arthroplasty Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. The Swedish Hip Arthroplasty Register, Annual Report 2006, J. Karrholm, G. Garellick, P. Herberts (Eds.), 2006.
2. The problem is osteolysis
3. The role of macrophages in osteolysis of total joint replacement10.1016/j.biomaterials.2004.04.035 ↗
4. Highly, crosslinked polyethylenes in hip replacements: improved wear performance or paradox
5. Wear behaviour of cross-linked polyethylene assessed in vitro under severe conditions10.1016/j.biomaterials.2004.07.070 ↗
6. Highly cross-linked polyethylene. The debate is over – in opposition10.1016/j.arth.2005.03.016 ↗
7. Rim cracking of the cross-linked Longevity polyethylene acetabular liner after total hip arthroplasty10.2106/JBJS.F.00758 ↗
8. Can a safe level for metal ions in patients with metal-on-metal total hip arthroplasties be determined?10.1016/j.arth.2004.09.008 ↗
9. Serum cobalt levels after metal-on-metal total hip arthroplasty10.2106/00004623-200311000-00017 ↗
10. Levels of metal ions after small- and large-diameter metal-on- metal hip arthroplasty10.1302/0301-620X.85B6.14166 ↗
11. Hip implants – paper VI – ion concentrations10.1016/j.matdes.2005.05.018 ↗
12. Ceramic liner fracture after cementless alumina-on-alumina total hip arthroplasty10.1097/BLO.0b013e3180303e87 ↗
13. Isolated fracture of the ceramic head after third-generation alumina-on-alumina total hip arthroplasty10.2106/JBJS.F.01489 ↗
14. Evaluation of wear in an all-polymer total knee replacement. Part 1: laboratory testing of polyethylene on polyacetal bearing surfaces10.1016/0267-6605(93)90033-4 ↗
15. Can a total knee replacement prosthesis be made entirely of polymers?10.1016/S0883-5403(98)90003-1 ↗
16. Evaluation of wear in an all-polymer total knee replacement. Part 2: clinical evaluation of wear in a polyethylene on polyacetal total knee10.1016/0267-6605(93)90034-5 ↗
17. H. Yuan, L. Pimenta, M. Songer, Preliminary clinical evaluation of the NUBAC disc arthroplasty – a Brazil experience, in Spine Arthroplasty Society, Montreal, Canada, 2006.
18. Wear studies on the likely performance of CFR-PEEK/CoCrMo for use as artificial joint bearing materials
19. The wear properties of CFR-PEEK articulating against ceramic assessed on a multidirectional pin-on-plate machine10.1243/09544119JEIM224 ↗
20. A comparison of the wear of cross-linked polyethylene against itself under reciprocating and multi-directional motion with different lubricants10.1016/S0043-1648(01)00660-3 ↗
21. A multi-directional wear screening device and preliminary results of UHMWPE articulating against stainless steel
22. Pin-on-plate studies on the effect of rotation on the wear of metal-on-metal samples
23. Is the wear factor in total joint replacements dependent on the nominal contact stress in ultra-high molecular weight polyethylene contacts?10.1243/095441104322983997 ↗
24. Biological response to wear debris generated in carbon based composites as potential bearing surfaces for artificial hip joints10.1002/jbm.b.10068 ↗
25. In vitro biocompatability of polyetheretherketone and polysulfone composites10.1002/jbm.820240207 ↗
26. In vitro biocompatability testing of polymers for orthopaedic implants using cultured fibroblasts and osteoblasts10.1016/0142-9612(95)94906-2 ↗
27. Use of a novel carbon fibre composite material for the femoral stem component of a THR system: in vitro biological assessment
28. Polyetheretherketone – cytotoxicity and mutagenicity in vitro10.1016/S0142-9612(01)00300-3 ↗