Solid particle erosion behavior of nanolaminated Cr 2 AlC films
Source abstract
Abstract
Abstract In aero-engines particle erosion leads to a removal of vane and blade material particularly in the compressor section, reducing the engine efficiency and operation time. MAX phases were identified as a suitable material for erosion protection due to their good combination of metallic and ceramic properties. The successful application of Cr2AlC through High Power Impulse Magnetron Sputtering (HiPIMS) process on a frequently used engine material (IN718) results in a highly dense and well adherent coating. Understanding the erosion damage mechanism of this coated high temperature material is a key factor to counteract the damage and to increase the durability and reliability of engine components. This paper presents a comparative study of the fundamental erosion mechanism of IN718 and of the recently developed material system, IN718 + Cr2AlC MAX phase coating (7 µm and 20 µm). It is found, that erosion proceeds in four stages. Moreover, the measured erosion rate by means of laboratory particles erosion tests has shown an up to fourfold lifetime improvement of the coated system as compared to the uncoated counterpart.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Erosion caused by airborne particles10.1016/0043-1648(69)90035-0 ↗
2. Erosion Behavior in a Simulated Jet Engine Environment10.2514/3.58611 ↗
3. Turbine Blade Surface Deterioration by Erosion10.1115/1.1860376 ↗
4. Erosion and deposition in turbomachinery10.2514/1.18462 ↗
5. Impact of erosion testing aspects on current and future flight conditions10.1016/j.paerosci.2011.04.001 ↗
6. Solid particle erosion, ASM Handb
7. Wear models and predictive equations: their form and content10.1016/0043-1648(95)90158-2 ↗
8. A model for erosion at normal impact10.1016/S0043-1648(96)07315-2 ↗
9. A comprehensive phenomenological model for erosion of materials in jet flow10.1016/j.powtec.2008.03.003 ↗
10. Erosion of surfaces by solid particles10.1016/0043-1648(60)90055-7 ↗
11. Some reflections on the past and future of erosion10.1016/0043-1648(95)07188-1 ↗
12. Effect of impact angle and velocity on erosion of API X42 pipeline steel under high abrasive feed rate10.1016/j.wear.2014.01.005 ↗
13. Practical estimation of erosion damage caused by solid particle impact Part 1: effects of impact parameters on a predictive equation10.1016/j.wear.2005.01.039 ↗
14. Solid particle erosion mechanisms of protective coatings for aerospace applications10.1016/j.surfcoat.2014.08.037 ↗
15. ASTM G76-13, Standard Test Method for Conducting Erosion Tests by Solid Particle Impingement Using Gas Jets, 2013.
16. ASTM G211-14, Standard Test Method for Conducting Elevated Temperature Erosion Tests by Solid Particle Impingement Using Gas Jets, 2014.
17. Development of mechanistic erosion equation for solid particles10.1016/j.wear.2015.01.031 ↗
18. On the ductile behavior of nominally brittle materials during erosive cutting10.1115/1.3672666 ↗
19. Measurement of coating durability by solid particle erosion10.1016/0257-8972(94)02314-G ↗
20. Abrasive and erosive wear tests for thin coatings: a unified approach10.1016/S0301-679X(98)00004-8 ↗
21. Solid particle erosion mechanisms of hard protective coatings10.1016/j.surfcoat.2013.07.050 ↗
22. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
23. Nanoindentation and nanoscratching of hard carbon coatings for magnetic disks10.1557/PROC-383-447 ↗
24. Relationships between hardness, Young’s modulus and elastic recovery in hard nanocomposite coatings10.1016/S0257-8972(01)01714-5 ↗
25. Multilayer PVD coatings for wear protection10.1016/0257-8972(95)02555-3 ↗
26. Wear of PVD Ti/TiN multilayer coatings10.1016/S0257-8972(96)03141-6 ↗
27. Nanolayered CrAlTiN and multilayered CrAlTiN–AlTiN coatings for solid particle erosion protection10.1016/j.triboint.2014.11.002 ↗
28. Multi-layer coating design architecture for optimum particulate erosion resistance10.1016/j.wear.2011.05.035 ↗
29. Erosion performance and characterization of nanolayer (Ti,Cr)N hard coatings for gas turbine engine compressor blade applications10.1016/j.surfcoat.2011.07.063 ↗
30. The MAX phases a new class of solids thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
31. The MAX Phase unique new carbide and nitride materials10.1511/2001.28.736 ↗
32. Elastic and mechanical properties of the MAX phases10.1146/annurev-matsci-062910-100448 ↗
33. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
34. Bonding and classification of nanolayered ternary carbides10.1103/PhysRevB.70.092102 ↗
35. High power pulsed magnetron sputtered CrNx films10.1016/S0257-8972(02)00479-6 ↗
36. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
37. Systematic study on the pressure dependence of M2AlC phases (M = Ti , V , Cr , Zr , Nb , Mo , Hf , Ta , W)10.1103/PhysRevB.76.224111 ↗
38. HPPMS deposition from composite targets: effect of two orders of magnitude target power density changes on the composition of sputtered Cr-Al-C thin films10.1016/j.vacuum.2017.08.048 ↗
39. Goldstein · 2003
40. Reducing the impurity incorporation from residual gas by ion bombardment during high vacuum magnetron sputtering10.1063/1.2193044 ↗
41. Effect of the composition on the structure of Cr-Al-C investigated by combinatorial thin film synthesis and ab initio calculations10.1002/adem.200400096 ↗
42. Ab initio calculations and experimental determination of the structure of Cr2AlC10.1016/j.ssc.2004.02.047 ↗
43. Crystallization kinetics of amorphous Cr2AlC thin films10.1016/j.surfcoat.2011.06.003 ↗
44. Oxygen incorporation in M2AlC (M=Ti, V, Cr)10.1016/j.actamat.2012.05.011 ↗
45. A critical study of the erosion of an aluminium alloy by solid spherical particles at normal impingement10.1016/0043-1648(83)90302-2 ↗
46. Elastic properties of Cr2AlC thin films probed by nanoindentation and ab initio molecular dynamics10.1016/j.scriptamat.2007.08.006 ↗
47. Assessment of surface hardening effects from shot peening on a Ni-based alloy using electron backscatter diffraction techniques10.1016/j.actamat.2011.04.025 ↗
48. Solid particle erosion resistance and high strain rate deformation behavior of Inconel-625 alloy