Thermomechanical modeling of transient thermal damage in cannon bore materials
Source abstract
Abstract
Modeling of cannon firing damage is extended to include time-varying gas temperature and convection coefficient data as inputs to finite difference calculations of near-bore temperature. Results are described for convective gas heating typical of cannon firing and for laser and combustor simulations of firing. Modeling is also extended to constant heat input conditions for comparison with laser simulation of firing. Slip-zone coating failure concepts of Evans and Hutchinson are adapted to predict shear stress on segments of thermally damaged material, including chromium and silicon carbide. Three measures of thermal damage are described: peak near-bore temperatures, which are highest for laser heating due to its relatively long 5 ms pulse duration; temperature difference between the heated surface and 0.1 mm below the surface, which is highest for cannon firing due to its peak convection during the initial 1 ms of the cannon firing pulse; and coating segment shear stress, which is relatively constant among the various types of cannon firing and simulated firing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electromagnetic Launch and Propulsion Technology · Force Microscopy Techniques and Applications · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. Compressive thermal yielding leading to hydrogen cracking in a fired cannon10.1115/1.2883658 ↗
2. Thermal damage, cracking and rapid erosion of cannon bore coatings10.1115/1.1593077 ↗
3. Laser pulse heating of gun bore coatings10.1016/S0257-8972(01)01367-6 ↗
4. Thermo-mechanical and fracture analysis of SiC in cannon bore applications10.1002/9780470294826.ch73 ↗
5. The thermomechanical integrity of thin films and multilayers10.1016/0956-7151(94)00444-M ↗
6. Crack propagation in a gun barrel due to the firing thermo-mechanical stresses10.1115/1.1592813 ↗
7. Erosion predictions for the final configuration of the M829E3 round
8. Hardness tests