Effects of microstructure on wear behaviour of wood reinforced polypropylene composite
Source abstract
Abstract
Friction coefficient, wear rate and wear micromechanism of wood reinforced polypropylene (WPC), pine wood and polypropylene (PP) have been compared. WPC and wood present very similar coefficients of friction, whereas PP has the highest value. However, the wear rate is significantly smaller for the WPC than for the other two materials. The higher stiffness and yield stress of the WPC minimises the plasticity inherent to the neat PP in the contact zone, resulting in a lower coefficient of friction and wear rate. Whereas in wood specimen generalised microfisuration and delamination can be observed at the worn surface, the wood fibres embedded in WPC produces fewer wear debris, which is probably due to the restrained deformation of the collapsed and/or matrix filled cellular structure of wood fibres. So, the WPC has shown better wear performances than its neat constituents, polymer and wood.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Tribology and Wear Analysis · Natural Fiber Reinforced Composites · Polymer Nanocomposites and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Are natural fiber composites environmentally superior to glass fiber reinforced composites?10.1016/j.compositesa.2003.09.016 ↗
2. Impact fracture behavior of modified polypropylene/wood fiber composites10.1016/j.polymertesting.2003.10.011 ↗
3. Maleated coupling agents for natural fibre composites10.1016/j.compositesa.2003.09.014 ↗
4. Impact behavior of sawdust/recycled-PP composites10.1002/app.1567 ↗
5. Surface modification and adhesion mechanisms in woodfiber–polypropylene composites10.1023/A:1004790409158 ↗
6. Polypropylene/wood flour composites: treatments and properties10.1016/S0263-8223(01)00089-7 ↗
7. Mechanical properties and morphology of impact modified polypropylene–wood four composites10.1002/(SICI)1097-4628(19980228)67:9<1503::AID-APP1>3.0.CO;2-H ↗
8. Mechanical properties of wood–fiber reinforced polypropylene composites: Effect of a novel compatibilizer with isocyanate functional group10.1016/j.compositesa.2006.05.005 ↗
9. Effects of various fillers on the sliding wear of polymer composites10.1016/j.compscitech.2005.05.028 ↗
10. Wear of polymers10.1243/135065002762355325 ↗
11. Comparative spectroscopic study of the modification of cellulosic materials with different coupling agents10.1002/(SICI)1097-4628(20000110)75:2<256::AID-APP8>3.0.CO;2-Z ↗
12. Friction and wear behaviour of polyamide 6 sliding against steel at low velocity under very high contact pressures10.1016/S0043-1648(96)07500-X ↗
13. Softening and melting mechanisms of polyamides interfering with sliding stability under adhesive conditions10.1016/j.polymer.2006.05.034 ↗
14. Sarrionandia · 2006
15. Tribological behaviour of drawn polypropylene10.1016/S0043-1648(99)00262-8 ↗
16. Materials aspects of polymer wear10.1016/0956-716X(90)90122-W ↗
17. Tribological properties and acoustic emissions of some thermoplastics sliding against SAE5210010.1115/1.2000264 ↗