journal article·2018-01

Cavitation erosion behaviour of an innovative aluminium alloy for Hybrid Aluminium Forging

Gianmaria Gottardi, Marialaura Tocci, Lorenzo Montesano, Annalisa Pola

Wear· Volume 394-395
Publisher page

Abstract

Abstract Aluminium alloys are commonly used for the production of components, such as cylinders, pistons, pumps, valves and combustion chambers, which in service may incur in cavitation phenomenon. In the present paper, the cavitation erosion resistance of an innovative light-alloy used for Hybrid Aluminium Forging was investigated. The material was tested by means of an ultrasonic vibratory device in compliance with ASTM G32. In order to better estimate the material behaviour, the same investigation was performed on two commercial alloys, 6061 wrought alloy and A356 casting alloy. The cavitation resistance of these materials was evaluated by determining the erosion rate from the progressive measurements of the samples mass loss during the test. The erosion mechanism was studied by means of optical and scanning electron microscope, and its correlation with the alloy hardness and microstructure was evaluated. The innovative alloy shows remarkable cavitation erosion resistance, particularly in heat-treated conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Cavitation Phenomena in Pumps · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Davis · 1999 · 1
2. Cavitation erosion of face centered cubic metals10.1007/BF02661573 ↗
3. Thiruvengadam · 1964
4. Scaling study of cavitation pitting from cavitating jets and ultrasonic horns10.1016/j.wear.2012.07.025 ↗
5. Cavitation erosion of age-hardenable aluminum alloys10.1007/BF02646379 ↗
6. Cavitation erosion and corrosion behavior of copper-manganese-aluminum alloy weldment
7. Cavitation erosion of metals and alloys10.1016/0043-1648(84)90199-6 ↗
8. Correlation of cavitation erosion behavior with mechanical properties of metals10.1016/0043-1648(90)90122-Q ↗
9. Cavitation erosion of iron and steel10.1007/BF02652254 ↗
10. Cavitation wear behaviour of austenitic stainless steels with different grain sizes10.1016/j.wear.2004.03.024 ↗
11. Cavitation erosion of stainless steels10.1016/0043-1648(82)90278-2 ↗
12. Synergistic effect of cavitation erosion and corrosion of various engineering alloys in 3.5% NaCl solution10.1016/S0921-5093(00)00899-6 ↗
13. Improvement of the cavitation erosion resistance of an AISI 304L austenitic stainless steel by high temperature gas nitriding10.1016/j.msea.2004.05.003 ↗
14. Effect of temperature, pH and sulphide on the cavitation erosion behavior of super duplex stainless steel10.1016/S0043-1648(97)00072-0 ↗
15. Erosion corrosion of pump impeller of cyclic cooling water system10.1016/j.engfailanal.2005.07.012 ↗
16. Effect of ultrasonically induced cavitation on corrosion behaviour of a copper-manganese-aluminium alloy10.1179/000705988798271090 ↗
17. Deformation and erosion of F.C.C. metals and alloys under cavitation attack10.1016/0025-5416(84)90031-4 ↗
18. Improvement in cavitation erosion resistance of a copper-based propeller alloy by laser surface melting10.1016/j.surfcoat.2003.08.048 ↗
19. Cavitation erosion of copper and copper-based alloys10.1007/s11661-001-0223-6 ↗
20. A comparison of the cavitation erosion resistance of TiNi alloys, SUS304 stainless steel and Ni-based self-fluxing alloy10.1016/S0043-1648(00)00443-9 ↗
21. Erosion and cavitation corrosion of titanium and its alloys10.1016/S0043-1648(01)00709-8 ↗
22. Effects of materials and solution temperatures on cavitation erosion of pure titanium and titanium alloy in seawater10.1016/j.wear.2006.06.011 ↗
23. J.R. Davis, Aluminum and aluminum alloys, ASM Specialty Handbook, International, Materials Park, 1994, pp. 159–105.
24. Surface analysis of Al-Mg alloy series for ship after cavitation test10.1002/sia.4953 ↗
25. Erosion of aluminum 6061-T6 under cavitation attack in mineral oil and water10.1016/0043-1648(85)90023-7 ↗
26. Analysis of cavitation erosion resistance of cast iron and nonferrous metals based on database and comparison with carbon steel data10.1016/j.wear.2010.04.031 ↗
27. A study of cavitation erosion on engineering materials10.1016/j.wear.2012.11.026 ↗
28. Cavitation erosion of copper and aluminium in water at elevated temperature10.1016/0301-679X(93)90082-C ↗
29. Material and velocity effects on cavitation erosion pitting10.1016/j.wear.2011.09.006 ↗
30. Scaling of cavitation erosion progression with cavitation intensity and cavitation source10.1016/j.wear.2012.01.008 ↗
31. Alloy groupings by application or major characteristic
32. Cavitation erosion of aluminium alloys10.1007/BF00351438 ↗
33. Microstructural phenomena occurring during early stages of cavitation erosion of Al-Si aluminium casting alloys10.4028/www.scientific.net/SSP.227.255 ↗
34. Comparative study regarding the cavitation erosion behavior of Cu and Al alloys
35. Influence of ultrasound treatment on cavitation erosion resistance of AlSi7 alloy10.3390/ma10030256 ↗
36. Effect of globular microstructure on cavitation erosion resistance of aluminium alloys10.4028/www.scientific.net/SSP.256.51 ↗
37. Cavitation erosion of aluminium alloy matrix/ceramic composites10.1007/BF00278151 ↗
38. Fabrication and behaviour of Al-Si/SiC composite in cavitation conditions10.1179/1743133613Y.0000000078 ↗
39. An overview of the development of Al-Si alloy based material for engine applications10.1361/105994903770343132 ↗
40. Polmear · 2005 · 205
41. Campbell · 2003 · 267
42. Study on defects of A356 aluminum alloy wheel
43. Squeeze casting: an overview10.1016/S0924-0136(99)00291-5 ↗
44. Mechanical and corrosion properties of rheocast and low-pressure cast A356-T6 alloy10.1016/j.msea.2004.08.056 ↗
45. Production of A356 aluminum alloy wheels by thixo-forging combined with a low superheat casting process
46. Characterization of a new aluminium alloy for the production of wheels by Hybrid Aluminium Forging10.1016/j.proeng.2015.06.237 ↗
47. ASTM G 32 Standard. Standard Test Method for Cavitation Erosion Using Vibratory Apparatus.
48. Kim · 2014 · 21
49. Optimization of heat treatment parameters for a nonconventional Al-Si-Mg alloy with Cr addition by DoE method
50. Effect of Cr and Mn addition and heat treatment on AlSi3Mg casting alloy10.1016/j.matchar.2016.11.022 ↗
51. Cavitation erosion of materials10.1179/imr.1986.31.1.1 ↗
52. Iron-containing intermetallic phases in Al-Si based casting alloys10.1016/j.mspro.2012.06.004 ↗
53. Mondolfo · 1976