Thermal oxidation and its effect on the wear of Mg alloy AZ31B
Source abstract
Abstract
Magnesium alloy AZ31B is an important lightweight, high specific strength material for new generations of energy-effective vehicles. Presently, a critical challenge that the vehicle production is facing is how to prevent the material from surface oxidation at elevated temperatures. This paper aims to investigate the effect of thermal oxidation and chemical compositions of oxides on the wear of AZ31B. The tribology experiments were conducted by a contact pair of pin-on-disc under elevated temperatures. The disc and pin were made by AZ31B and the production tooling steel 86CrMoV7, respectively. The composition and morphology of the disc surface were examined by the scanning electron microscope (SEM). It was found that the initial surface oxide film naturally formed prior to testing at room temperature (RT) was thin, compact and protective. However, the film would lose its protection capability when the temperature rose because of the thickened film layer and the emergence of the oxide nodules. At a higher temperature, the oxide nodules grew more quickly. Besides, more oxide nodules emerged, and the film started to crack as the temperature increased, leading to a higher wear rate. The friction coefficient varied at different temperatures due to the change in the dominant wear mechanism of AZ31B. The minimum wear rate was found to occur at 200 degrees C and the maximum at 400 degrees C. It was also found that the surface hardness of AZ31B decreased from 75 HV2 at 25 degrees C to 50 HV2 at 200 degrees C, and then fluctuated around 50 HV2 at higher temperatures, which further accelerated the wear process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Magnesium and its alloys applications in automotive industry10.1007/s00170-007-1279-2 ↗
2. Magnesium: properties—applications—potential10.1016/S0921-5093(00)01351-4 ↗
3. Fundamentals and advances in magnesium alloy corrosion10.1016/j.pmatsci.2017.04.011 ↗
4. Enhancing plastic deformability of Mg and its alloys—a review of traditional and nascent developments10.1016/j.jma.2017.11.001 ↗
5. Mechanical behavior of AZ31B Mg alloy sheets under monotonic and cyclic loadings at room and moderately elevated temperatures10.3390/ma7021271 ↗
6. Poerschke · 2009
7. Birks · 2006 · 39
8. Birks · 2006 · 101
9. The oxidation behaviour of an AZ91D magnesium alloy at high temperatures
10. Oxidation characteristics of magnesium alloys
11. J. An, sliding wear map for AZ31 magnesium alloy10.1080/10402004.2014.933939 ↗
12. Sliding wear characteristics of AZ91D alloy at ambient temperatures of 25–200 °C10.1007/s11249-009-9569-5 ↗
13. Effect of temperature and applied load on sliding wear behaviour of AZ91D magnesium alloy
14. Tribology characteristics of magnesium alloy AZ31B and its composites10.1016/j.triboint.2014.02.024 ↗
15. Dry sliding wear behaviour of as-cast AZ31B magnesium alloy
16. Wear mechanisms of AZ31B magnesium alloy during dry sliding condition
17. Oxidation of magnesium alloys at elevated temperatures in air: a review10.1016/j.corsci.2016.06.018 ↗
18. Birks · 2006 · 1
19. Dry sliding wear behavior of magnesium alloys10.1016/j.wear.2007.08.021 ↗
20. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
21. New insights on the relationship between flow stress softening and dynamic recrystallization behavior of magnesium alloy AZ31B10.1016/j.matchar.2018.10.031 ↗
22. Effect of laser surface melting with alternating magnetic field on wear and corrosion resistance of magnesium alloy10.1016/j.surfcoat.2016.11.077 ↗
23. Investigation of the wear behaviors of Ag/Cu multilayers by nanoscratch10.1016/j.wear.2008.04.025 ↗
24. Study of the plastic flow behaviors of AZ91 magnesium alloy during thermomechanical processes10.1016/j.jallcom.2009.05.089 ↗
25. Kato · 2000 · 273
26. Effect of magnesium content on the high temperature adhesion of Al–Mg alloys to steel surfaces10.1016/j.surfcoat.2009.01.041 ↗
27. Sliding wear behaviour and its mechanisms of carbonitrided AISI 8620 steel at 100°C under unlubricated conditions10.1179/1743294415Y.0000000090 ↗
28. Wear behaviour of a Mg alloy subjected to friction stir processing10.1016/j.wear.2013.02.023 ↗
29. Evaluation of sliding wear behaviour of feldspar particle-reinforced magnesium alloy composites10.1016/S0043-1648(00)00349-5 ↗
30. Seifert · A method for the study of wear particles in lubricating oil · 1972 · 21 · 27
31. Anderson · 1982
32. Mechanical wear debris feature, detection, and diagnosis: a review10.1016/j.cja.2017.11.016 ↗