Effects of Ni content on microstructure and wear behavior of Al–13Si–3Cu–1Mg-xNi-0.6Fe-0.6Mn alloys
Source abstract
Abstract
As one of the lightweight and wear-resistance metallic structural materials, cast Al–Si alloys have been widely studied in automobile and defense industries to meet the greater demands for elevated-temperature wear-resistance properties. In this study, the effect of Ni content on the microstructure and wear behavior of Al–13Si–3Cu–1Mg-xNi-0.6Fe-0.6Mn alloys were investigated by thermodynamic modeling, X-ray diffraction (XRD), scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS) and ball-on-disk reciprocating sliding test. The results show that the θ-Al 2Cu and γ-Al 7Cu 4Ni phases are disappeared, while the δ-Al 3CuNi, ε-Al 3 Ni, and T-Fe phases are formed with the increasing of Ni contents. The 3-D network structure is composed of α-Al matrix, eutectic Si, Q, Ni-rich, and Al 15(Mn, Fe) 3Si 2 phases, which leads to the best hardness and wear-resistance of the alloy with 2 wt% Ni. The fracture and debonding of excessive coarse ε-Al 3 Ni phase deteriorate the wear-resistance and ductility of the 3Ni alloy. The main wear mechanisms of the tested alloys are abrasive, delamination and oxidative wear at 25 °C and convert to adhesive wear at 350 °C.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Effect of δ-Al3CuNi phase and thermal exposure on microstructure and mechanical properties of Al-Si-Cu-Ni alloys10.1016/j.jallcom.2019.03.412 ↗
2. Influence of Fe-rich intermetallics on solidification defects in Al–Si–Cu alloys10.1016/j.actamat.2014.01.007 ↗
3. High strength aluminum cast alloy: a Sc modification of a standard Al–Si–Mg cast alloy10.1016/j.msea.2014.03.005 ↗
4. formation of Al15Mn3Si2 phase during solidification of a novel Al-12%Si-4%Cu-1.2%Mn heat-resistant alloy and its thermal stability
5. Effect of solution heat treatment and additives on the microstructure of Al – Si (A413.1) automotive alloys10.4028/www.scientific.net/MSF.467-470.399 ↗
6. Incipient melting of Al5Mg8Si6Cu2 and Al2Cu intermetallics in unmodified and strontium-modified Al–Si–Cu–Mg (319) alloys during solution heat treatment10.1023/A:1004383203476 ↗
7. Enhanced mechanical properties of high-temperature-resistant Al–Cu cast alloy by microalloying with Mg
8. Evolution of iron-rich intermetallics and elevated temperature mechanical properties in gravity die cast 2A16 Al alloy10.1080/13640461.2017.1409391 ↗
9. Effect of Q-Al 5 Cu 2 Mg 8 Si 6 phase on mechanical properties of Al-Si-Cu-Mg alloy at elevated temperature10.1016/j.msea.2017.03.087 ↗
10. Investigation of the effects of Ni, Fe, and Mn on the formation of complex intermetallic compounds in Al-Si-Cu-Mg-Ni alloys10.1007/s11661-011-0764-2 ↗
11. Improvement in elevated-temperature properties of Al-13% Si piston alloys by dispersoid strengthening via Mn addition10.1557/jmr.2018.117 ↗
12. Effect of heat treatment and Fe content on the microstructure and mechanical properties of die-cast Al–Si–Cu alloys10.1016/j.matdes.2015.07.074 ↗
13. Improvement of elevated-temperature strength and recrystallization resistance via Mn-containing dispersoid strengthening in Al-Mg-Si 6082 alloys10.1016/j.jmst.2019.08.027 ↗
14. Effects of Mn addition and related Mn-containing dispersoids on the hot deformation behavior of 6082 aluminum alloys
15. Effects of heat treatments and minor addition of small amounts of Cu and Mg on the microstructure and mechanical properties of Al-Si-Cu and Al-Si-Mg cast alloys10.1016/j.jallcom.2018.12.365 ↗
16. Tensile and compressive deformation behavior of the Al–Si–Cu–Mg cast alloy with additions of Zr, V and Ti10.1016/j.matdes.2014.02.060 ↗
17. A. Buzaianu new quaternary type of Al-Sr-Ti-B master alloy for grain refining and modifying of Al-Si10.4028/www.scientific.net/AMR.23.295 ↗
18. Supportive strengthening role of Cr-rich phase on Al–Si multicomponent piston alloy at elevated temperature10.1016/j.msea.2011.02.047 ↗
19. On the origin of a remarkable increase in strength and stability of an Al rich Al-Ni eutectic alloy by Zr addition10.1016/j.actamat.2019.03.025 ↗
20. Thermal stability of (AlSi) x (ZrVTi) intermetallic phases in the Al–Si–Cu–Mg cast alloy with additions of Ti, V, and Zr10.1016/j.tca.2014.08.037 ↗
21. Effects of Ni content on low cycle fatigue and mechanical properties of Al-12Si-0.9Cu-0.8Mg-xNi at 350 °C10.1016/j.msea.2017.08.114 ↗
22. Quantitative comparison of three Ni-containing phases to the elevated-temperature properties of Al–Si piston alloys10.1016/j.msea.2010.07.073 ↗
23. Phase formation in as-solidified and heat-treated Al–Si–Cu–Mg–Ni alloys: thermodynamic assessment and experimental investigation for alloy design10.1016/j.jallcom.2012.10.182 ↗
24. Quantitative comparison of three Ni-containing phases to the elevated-temperature properties of Al–Si piston alloys10.1016/j.msea.2010.07.073 ↗
25. Micromechanisms and mechanics of ultra-mild wear in Al–Si alloys10.1016/j.actamat.2008.07.043 ↗
26. Dry sliding wear behaviour of Al–12Si and Al–12Si–3Cu cast alloys10.1016/j.matdes.2008.07.003 ↗
27. Dry sliding wear behaviour of hypereutectic Al–Si piston alloys containing iron-rich intermetallics10.1016/j.matchar.2010.07.001 ↗
28. Effect of iron-rich intermetallics on the sliding wear behavior of Al–Si alloys10.1016/j.msea.2008.01.001 ↗
29. Improved mechanical properties in cast Al–Si alloys by combined alloying of Fe and Cu10.1016/j.msea.2010.08.058 ↗
30. Eutectic Al–Si–Cu–Fe–Mn alloys with enhanced mechanical properties at room and elevated temperature10.1016/j.matdes.2011.04.005 ↗
31. Three-dimensional rigid multiphase networks providing high-temperature strength to cast AlSi10Cu5Ni1-2 piston alloys10.1016/j.actamat.2011.07.006 ↗
32. The effects of manganese on the Τ-phase and creep resistance in Al–Si–Cu–Mg–Ni alloys10.1016/j.msea.2013.06.030 ↗
33. Evolution of nickel-rich phases in Al–Si–Cu–Ni–Mg piston alloys with different Cu additions10.1016/j.matdes.2011.06.058 ↗
34. Thermal exposure of Al-Si-Cu-Mn-Fe alloys and its contribution to high temperature mechanical properties - ScienceDirect10.1016/j.jmrt.2019.12.018 ↗
35. Three-dimensional study of Ni aluminides in an AlSi12 alloy by means of light optical and synchrotron microtomography10.1016/j.actamat.2009.05.010 ↗
36. Dry reciprocating wear and frictional behaviour of B4C reinforced functionally graded and homogenous aluminium matrix composites10.1016/j.jmrt.2019.11.084 ↗
37. Ageing characteristics and high-temperature tensile properties of Al–Si–Cu–Mg alloys with micro-additions of Mo and Mn10.1016/j.msea.2015.11.049 ↗
38. Improvement in dry sliding wear resistance of Al-17Si-5Cu alloy after an enhanced heat treatment process10.1016/S1003-6326(18)64814-9 ↗
39. Measurement of hardness, wear rate and coefficient of friction of surface refined Al-Cu alloy10.1016/j.proeng.2014.12.416 ↗
40. Effect of Nickel content on hardness and wear rate of surface modified cast aluminum bronze alloy10.1016/j.matpr.2017.11.317 ↗
41. Effect of the silicon content and thermomechanical treatment on the dry sliding wear behavior of spray-deposited Al–Si/SiCp composites10.1016/j.wear.2006.05.019 ↗
42. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
43. Effect of particle size on dry sliding wear behaviour of sillimanite reinforced aluminium matrix composites10.1016/j.ceramint.2017.09.132 ↗
44. Dry sliding friction and wear characterization of in situ TiC/Al-Cu3.7-Mg1.3 nanocomposites with nacre-like structures10.1016/j.jmrt.2019.11.005 ↗
45. Wear behavior of Al–Mg–Cu–based composites containing SiC particles10.1016/j.triboint.2009.04.030 ↗