Cavitation erosion performance of CVD W/WC coatings
Source abstract
Abstract
Abstract In the aviation industry, water droplet erosion (WDE) takes place when an aircraft takes off on as wet runway or flies through rain or clouds. The leading edge of turbofan blades suffers from high-speed (300–400 m/s) impingements of water droplets, resulting in material removal that subsequently changes the leading edge profile and surface roughness. This affects the aerodynamic performance of turbofan blades, which eventually leads to efficiency drop of the aircraft engine and the need to replace and/or recondition the blades. A coating solution is targeted, such that, not only that it resists the high impact pressure but also inhibits stress wave reinforcements at the coating-substrate or interlayers interfaces. Past studies indicate similar damage mechanisms to WDE are generated by cavitation erosion (CE) during the early stages (incubation). Hence, CE is introduced in this study to predict the WDE performance. The coatings studied were nanostructured CVD tungsten/tungsten carbide coatings, either hierarchical or monotonic in design, on Ti6Al4V alloy grade 5 substrates. In-depth understanding on the coating damage mechanisms are established by correlating the coating performance with microstructure, crystallographic texture, interface design, coating deposition conditions and mechanical properties for the first time. A particular crystalline texture was found that gives optimum performance. The effect of the initial coating topography on the CE performance is effectively characterised by the surface parameters Ssk and Sku. The damage was found to initiate at the grain boundaries of the exposed surfaces. The hierarchical coating microstructure demonstrated enhancement in CE performance compared to a monotonic columnar grain structure. Additionally, it is found that the coating performance under dynamic compressive loadings could not be predicted by a simple H/E approaches. However, combining the H/E ratios with the factors of microstructure and crystal orientations might further facilitate the understanding of coating performances along with better understanding of the role of compressive residual stresses and stress waves propagation or reinforcement through coating depth and at the top surface of the coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. Standard · 2010
2. Rain impact retrospective and vision for the future10.1016/S0043-1648(99)00191-X ↗
3. Water droplet erosion of wind turbine blades: mechanics, testing, modeling and future perspectives10.3390/ma13010157 ↗
4. Liquid impingement erosion
5. ELSI conference: invited lecture: liquid impact: theory, experiment, applications10.1016/S0043-1648(99)00189-1 ↗
6. High‐speed impact between a liquid drop and a solid surface10.1063/1.1657361 ↗
7. Heymann · 1967
8. Droplet impact vs. cavitation erosion
9. A comparison of liquid impact erosion and cavitation erosion10.1016/0043-1648(80)90227-6 ↗
10. Hammitt · 1966 · 245
11. Schmitt · 1979
12. Erosion behaviour of ceramic bulk and coating materials caused by water droplet impingement10.1016/j.wear.2009.02.009 ↗
13. Liquid impact erosion of single-crystal magnesium oxide10.1016/S0043-1648(99)00193-3 ↗
14. Liquid impact and fracture of free-standing CVD diamond
15. Adler · 1982
16. Analysis of rain erosion of coated materials10.1177/002199837400800302 ↗
17. Fracture of diamond coatings by high velocity sand erosion10.1080/14786430802616557 ↗
18. Cavitation erosion performance of CrAlYN/CrN nanoscale multilayer coatings deposited on Ti6Al4V by HIPIMS10.1016/j.jallcom.2019.02.238 ↗
19. Metrological changes in surface morphology of high-strength steels in manufacturing processes10.1016/j.measurement.2016.03.055 ↗
20. Influence of surface morphology and microstructure on performance of CVD tungsten coating under fusion transient thermal loads10.1016/j.apsusc.2016.08.060 ↗
21. Microstructures of chemical vapor deposited high-purity tungsten achieved by two different precursors10.1016/j.matchar.2017.10.007 ↗
22. The thermal properties of high purity and fully dense tungsten produced by chemical vapor deposition10.1016/j.jnucmat.2014.11.095 ↗
23. Tungsten chemical vapor deposition using tungsten hexacarbonyl: microstructure of as-deposited and annealed films10.1016/S0040-6090(00)00943-3 ↗
24. Structural and optical properties of RF-biased PECVD TiO2 thin films deposited in an O2/TTIP helicon reactor10.1016/j.vacuum.2016.07.004 ↗
25. Microstructure study of CVD W coating on Mo single crystal rods with< 1 1 1> axial orientation by EBSD10.1016/j.msea.2006.07.010 ↗
26. Synthesis and characterization of microcrystalline diamond to ultrananocrystalline diamond films via Hot Filament Chemical Vapor Deposition for scaling to large area applications10.1016/j.tsf.2015.11.088 ↗
27. Status review of the science and technology of ultrananocrystalline diamond (UNCD™) films and application to multifunctional devices10.1016/j.diamond.2010.03.015 ↗
28. Preece · 1979 · vol. 16 · 450
29. The residual stress, texture and surface changes in steel induced by cavitation10.1016/0043-1648(91)90302-B ↗
30. Cavitation erosion behavior of HVOF CaviTec coatings10.1016/j.wear.2017.06.003 ↗
31. Cavitation erosion mechanisms in stainless steels and in composite metal–ceramic HVOF coatings10.1016/j.wear.2016.07.015 ↗
32. Cavitation erosion of plasma-sprayed CoMoCrSi coatings10.1016/j.triboint.2016.06.014 ↗
33. Effect of initial surface roughness on cavitation erosion resistance of arc-sprayed Fe-based amorphous/nanocrystalline coatings10.3390/coatings7110200 ↗
34. Fatigue failure of SUS 304 caused by vibratory cavitation erosion10.1016/0043-1648(94)90238-0 ↗
35. Characterizing cavitation erosion particles by analysis of SEM images10.1016/j.triboint.2008.05.008 ↗
36. kocanda · 1978
37. Cavitation erosion
38. SEM observation of the vibratory cavitation-fracture mode during the incubation period and the small roughness effect
39. Relations between cavitation erosion resistance of materials and their fatigue strength under random loading10.1016/S0043-1648(99)00105-2 ↗
40. Mass loss simulation in cavitation erosion: fatigue criterion approach10.1016/j.wear.2013.01.118 ↗
41. A metallurgical approach to improved cavitation-erosion resistance10.1007/s11665-997-0057-5 ↗
42. The limitations of using “Ra” to describe surface roughness10.1115/1.4032280 ↗
43. Developing stages of ultrasonically produced cavitation erosion and corresponding surface roughness
44. A study on surface topography in cavitation erosion tests of AlSi10Mg10.1016/j.triboint.2016.06.007 ↗
45. Correlation of cavitation erosion resistance with indentation-derived properties for a NiTi alloy10.1016/S1359-6462(01)01143-5 ↗
46. Correlation of cavitation properties of metals erosion behavior with mechanical10.1016/0043-1648(90)90122-Q ↗
47. Mechanical properties of TiN/TiB2 multilayers deposited by plasma enhanced chemical vapor deposition10.1016/S0257-8972(03)00574-7 ↗
48. Stress produced in a solid by cavitation10.1063/1.322584 ↗
49. A study of cavitation erosion on engineering materials10.1016/j.wear.2012.11.026 ↗
50. Mechanics of collapsing cavitation bubbles10.1016/j.ultsonch.2015.04.006 ↗
51. Measurement of fracture toughness by nanoindentation methods: recent advances and future challenges10.1016/j.cossms.2015.04.003 ↗
52. Hard nanocomposite coatings: thermal stability, oxidation resistance and toughness10.1016/j.surfcoat.2012.05.073 ↗
53. Design criteria for wear-resistant nanostructured and glassy-metal coatings10.1016/j.surfcoat.2003.09.011 ↗
54. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
55. Toughness enhancement of nanostructured hard coatings: design strategies and toughness measurement techniques10.1016/j.surfcoat.2014.08.018 ↗
56. Cavitation erosion resistance and wear mechanisms of active screen low temperature plasma nitrided AISI 410 martensitic stainless steel10.1016/j.wear.2014.12.009 ↗
57. Effect of substrate preheating treatment on the microstructure and ultrasonic cavitation erosion behavior of plasma-sprayed YSZ coatings10.1016/j.ultsonch.2018.04.004 ↗
58. Cavitation erosion resistance of Cr–N coating deposited on stainless steel10.1016/j.wear.2005.09.018 ↗
59. The influence of TiN coatings properties on cavitation erosion resistance10.1016/j.surfcoat.2009.07.014 ↗
60. Determination of sub-surface stresses at inclusions in single crystal superalloy using HR-EBSD, crystal plasticity and inverse eigenstrain analysis10.1016/j.ijsolstr.2015.02.023 ↗
61. Cavitation erosion behavior of electroless nickel-plating on AISI 1045 steel10.1016/j.wear.2005.02.099 ↗
62. Cavitation wear behaviour of austenitic stainless steels with different grain sizes10.1016/j.wear.2004.03.024 ↗
63. Improvement in cavitation erosion resistance of AISI 316L stainless steel by friction stir processing10.1016/j.apsusc.2014.04.132 ↗
64. Microstructure and wear mechanisms of texture-controlled CVD α-Al2O3 coatings10.1016/j.wear.2017.01.071 ↗
65. Plastic deformation of CVD textured tungsten—II. Characterization10.1016/0956-7151(94)90075-2 ↗
66. Plastic deformation of CVD textured tungsten—I. Constitutive response10.1016/0956-7151(94)90074-4 ↗