Wear of mold surfaces: Interfacial adhesion in precision glass molding

Hanhan Zhao, Asit Kumar Gain, Zhen Li, Liangchi Zhang

Wear· Volume 524-525
Publisher page

Abstract

Micro-optical components, such as glass-based microlens arrays, have become essential in applications relying on advanced optical systems such as 3D displays, optical fiber coupling, and unmanned vehicles. Precision glass molding (PGM) has emerged as a promising method for fabricating optical components based on the formability of glasses beyond their glass transition temperature (T g ), while adhesion wear strength and mechanism of mold-glass interfaces remain major obstacles. This paper aims to explore the adhesion wear mechanisms between mold surfaces and optical glass D-FK95 in PGM. The applicability of WC molds with coatings of Ta–C, AlCrN, and AlTiN was investigated respectively considering their thermodynamic properties and surface energy characteristics. The study identified three adhesion wear mechanisms in the open-air atmosphere with WO 3 oxidation on mold surfaces and four adhesion mechanisms featured by scattered distribution, island aggregation, dispersed flow, and planar coverage in an inert atmosphere. It was also found that when the temperature was close to T g, the WC-glass adhesion force was negligible. The adhesion stress increased to 0.80 MPa with an increase in the applied temperature and pressure. With coating, however, the adhesion stress reduced significantly to 0.03 MPa. The study also concluded that when paired with the D-FK95 glass, the WC mold coated with Ta–C provides the best anti-adhesive performance in comparison to those with AlCrN and AlTiN coatings.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Adhesion, Friction, and Surface Interactions · Laser Material Processing Techniques · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Nanofabrication through molding10.1016/j.pmatsci.2021.100891 ↗
2. Precision glass molding: toward an optimal fabrication of optical lenses10.1007/s11465-017-0408-3 ↗
3. Review on thin film coatings for precision glass molding
4. Present status of the functional advanced micro-, nano-printings - a mini review
5. Transfer printing techniques for flexible and stretchable inorganic electronics10.1038/s41528-018-0037-x ↗
6. A critical review on the fused deposition modeling of thermoplastic polymer composites10.1016/j.compositesb.2020.108336 ↗
7. Printable smart materials and devices: strategies and applications10.1021/acs.chemrev.1c00303 ↗
8. The evolution and generation of nanosurfaces and their microcontact mechanism in glass-embossing process10.1111/jace.18462 ↗
9. Thermoforming mechanism of precision glass moulding10.1364/AO.54.006841 ↗
10. Chip-free surface patterning of toxic brittle polycrystalline materials through micro/nanoscale burnishing10.1016/j.ijmachtools.2020.103688 ↗
11. Micro-impact testing of AlTiN and TiAlCrN coatings10.1016/j.wear.2018.11.010 ↗
12. Experimental investigation of contact heat transfer coefficients in nonisothermal glass molding by infrared thermography10.1111/jace.16029 ↗
13. Effect of pressure and temperature on viscosity of a borosilicate glass10.1111/jace.15588 ↗
14. Deformation behavior of glass nanostructures in hot embossing10.1021/acsami.0c08435 ↗
15. High-temperature friction characteristics of N-BK7 glass and their correlation with viscoelastic loss modulus10.1016/j.ceramint.2021.04.151 ↗
16. Size effect on friction and wear mechanisms of bulk metallic glass10.1016/j.wear.2017.01.068 ↗
17. Study on shape deviation and crack of ultra-thin glass molding process for curved surface10.1016/j.ceramint.2021.11.228 ↗
18. Dry sliding wear and mechanical behaviour of selective laser melting processed 18Ni300 and H13 steels for moulds
19. Wear and tribological characterization of nickel matrix electrodeposited composites: a review10.1016/j.wear.2021.204098 ↗
20. Study on mechanism of glass molding process for fingerprint lock glass plates10.3390/cryst11040394 ↗
21. A review of the techniques for the mold manufacturing of micro/nanostructures for precision glass molding10.1088/2631-7990/ac1159 ↗
22. A comprehensive review of micro/nano precision glass molding molds and their fabrication methods10.3390/mi12070812 ↗
23. Investigation on mechanical properties of tribofilm formed on Ti-6Al-4V surface sliding against a DLC coating by nano-indentation and micro-pillar compression techniques
24. Metallic glass hardening after thermoplastic forming10.1016/j.msea.2018.04.021 ↗
25. Localized rapid heating process for precision chalcogenide glass molding10.1016/j.optlaseng.2015.04.007 ↗
26. Temperature and rate dependent debonding behaviors of precision glass molding interface10.1111/jace.17478 ↗
27. Microstructural evaluation of sputtered Ru-Pt multilayer anti-stick coatings for glass molding10.1016/j.matdes.2022.110898 ↗
28. On the adhesion between metallic glass and dies during thermoplastic forming10.1016/j.jallcom.2017.04.005 ↗
29. PtIr protective coating system for precision glass molding tools: design, evaluation and mechanism of degradation10.1016/j.surfcoat.2020.125378 ↗
30. Surface integrity analysis of ultra-thin glass molding process10.1016/j.ceramint.2021.07.236 ↗
31. Characterization and growth mechanisms of adhesion-induced microcavities during debonding of softened glass10.1111/ijag.16596 ↗
32. Modeling nonequilibrium thermoviscoelastic material behaviors of glass in nonisothermal glass molding10.1111/jace.18605 ↗
33. Multi-scale cold embossing of CoCrFeNiMn high entropy alloy with ultra-high temperature durability
34. High-temperature friction behavior of amorphous carbon coating in glass molding process10.1007/s40544-020-0452-6 ↗
35. Tungsten carbide molds for precision glass molding process: mechanism of high-temperature degradation10.1016/j.ijrmhm.2022.105841 ↗
36. Influence of glass contact induced changes in surface composition of Pt, PtIr and Ir protective coatings on glass adhesion10.1016/j.apsusc.2021.149282 ↗
37. Study on the blackening phenomenon of leaded glass during microgroove molding using nickel phosphorous mold10.1016/j.ceramint.2021.12.239 ↗
38. A model for frictional stress relaxation at the interface between a soft and a hard solid10.1016/j.jmps.2020.104191 ↗
39. A comprehensive study on frictional dependence and predictive accuracy of viscoelastic model for optical glass using compression creep test10.1111/jace.16531 ↗
40. Polymer adhesion: seeking new solutions for an old problem10.1021/acs.macromol.1c01182 ↗
41. Molecular dynamics simulations on adhesion energy of PDMS-silica interface caused by molecular structures and temperature10.1016/j.apsusc.2021.151930 ↗
42. Evaluation of demolding force for glass-imprint process10.1016/j.jnoncrysol.2013.04.055 ↗
43. High-temperature friction behavior of amorphous carbon coating in glass molding process10.1007/s40544-020-0452-6 ↗
44. Temperature effects on DLC coated micro moulds10.1016/j.surfcoat.2016.08.034 ↗
45. Investigating the effect of SiC particles on the physical and thermal properties of Al6061/SiCp composite10.1016/j.jallcom.2019.05.317 ↗
46. Thermal failure mechanism of multilayer brittle TiN/CrAlN films10.1016/j.ceramint.2018.01.260 ↗
47. Enhanced bonding strength of Al2O3/AlN ceramics joined via glass frit with gradient thermal expansion coefficient10.1016/j.ceramint.2020.02.050 ↗
48. High-precision molding simulation prediction of glass lens profile for a new lanthanide optical glass10.1016/j.ceramint.2022.02.118 ↗
49. Infrared transmission and refractive index dispersion of mixed-chalcogen Ge-Sb-S-Se glasses for use in molded lens applications10.1016/j.jnoncrysol.2020.120258 ↗
50. Study on α-Al2O3 anti-adhesion coating for molds in precision glass molding10.1016/j.surfcoat.2020.125720 ↗
51. Modification of surface properties on a nitride based coating films through mirror quality finish grinding10.1016/j.cirp.2010.03.132 ↗
52. Kinetics and oxidation behavior of laser clad WC-Co and Ni/WC-Co coatings10.1016/j.ceramint.2018.04.087 ↗
53. Oxidation of WC-Co, WC-Ni and WC-Co-Ni hard metals in the temperature range 500–800 °C10.1016/0263-4368(96)00009-1 ↗
54. Surface failure analysis of AlCrN coating on WC substrate subjected to high-temperature oxidation in glass-molding machine10.1016/j.apsusc.2018.05.031 ↗