High-temperature tribological properties of coatings repaired by laser additive manufacturing on railway wheel tread damage
Source abstract
Abstract
Heavy-duty train wheels can easily cause local damage. Laser additive manufacturing technology has obvious advantages in repairing local damage to train wheels. The high temperature sliding condition caused by tread braking is a severe test for the coating of damaged wheels repaired by laser additive. In this study, three self-fluxing alloy powders, Fe-, Ni-, and Co-based, which are the most widely used in laser cladding, were selected as repair materials. The sliding friction wear performance at high temperatures was evaluated with an HT-1000 ball-disk wear tester, and the wear mechanisms of the repair area, substrate, and counterpart surfaces of the specimens were analyzed. The results show that the microstructure of the coating after the surface damage of the wheel is repaired by laser additive is mainly composed of dendritic structure and eutectic structure. Compared with the base material, the hardness of Fe-, Ni-, and Co-based alloy cladding coatings is significantly improved. At the same time, the wear resistance of the repaired wheel steel samples was improved to different degrees. The wear mechanism of the repaired area of the Fe-based alloy sample is mainly adhesive wear, and the wear mechanism of the repaired area of the Ni-based alloy sample is adhesive wear and oxidation wear. However, the surface of the wear scar of the Co-based alloy repaired sample is relatively smooth, the damage is slight, and the friction reduction effect is the best.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Damage evaluation regarding to contact zones of high-speed train wheel subjected to thermal fatigue10.1016/j.engfailanal.2015.07.021 ↗
2. Mechanical properties and fatigue behaviour of railway wheel steels as influenced by mechanical and thermal loadings10.1016/j.wear.2016.04.009 ↗
3. Investigation of effect of various processing temperatures on abrasive wear behaviour of high power diode laser treated R260 grade rail steels10.1016/j.triboint.2017.11.006 ↗
4. An integrated model for competitive damage mechanisms assessment in railway wheel steels10.1016/j.wear.2014.11.013 ↗
5. Rail defects: an overview
6. Investigation on the rolling wear and damage properties of laser dispersed quenched rail materials treated with different ratios10.1016/j.triboint.2019.03.022 ↗
7. Low carbon steel with nanostructured surface layer induced by high-energy shot peening10.1016/S1359-6462(01)00738-2 ↗
8. Enhancement of rolling contact fatigue performance of ferrite–pearlite steel with laser shock peening10.1177/1687814019850945 ↗
9. Comparison on the microstructure, bending properties and tribological behaviors of rail materials treated by laser dispersed quenching and induction assisted laser dispersed quenching10.1016/j.surfcoat.2021.126936 ↗
10. Influence of laminar plasma quenching on rolling contact fatigue behaviour of high-speed railway wheel steel10.1016/j.ijfatigue.2020.105668 ↗
11. Addressing the challenges in remanufacturing by laser-based material deposition techniques10.1016/j.optlastec.2021.107404 ↗
12. Investigation on wear and damage performance of laser cladding Co-based alloy on single wheel or rail material10.1016/j.wear.2015.03.002 ↗
13. Effect of laser claddings of Fe-based alloy powder with different concentrations of WS2 on the mechanical and tribological properties of railway wheel
14. The role of lanthanum oxide on wear and contact fatigue damage resistance of laser cladding Fe-based alloy coating under oil lubrication condition10.1016/j.triboint.2015.10.017 ↗
15. Fatigue evaluation of surface coated railway rails using shakedown theory, finite element calculations, and lab and field trials10.1016/j.ijfatigue.2004.11.002 ↗
16. Full-scale testing of laser clad railway track; Case study–Testing for wear, bend fatigue and insulated block joint lipping integrity10.1016/j.wear.2017.02.023 ↗
17. Study on wear and RCF performance of repaired damage railway wheels: assessing laser cladding to repair local defects on wheels10.1016/j.wear.2019.04.028 ↗
18. Assessment of laser cladding as an option forrepairing/enhancing rails10.1016/j.wear.2015.02.027 ↗
19. Rolling contact fatigue and wear behaviour of the infrastar two-material rail10.1016/j.wear.2004.03.054 ↗
20. Two-material rail development: field test results regarding rolling contact fatigue and squeal noise behaviour10.1016/j.wear.2004.03.067 ↗
21. Laser cladding: the alternative for field thermite welds life extension10.1016/j.matdes.2016.08.061 ↗
22. Comparative study on tribological properties of the sulfurizing layers on Fe, Ni and Co based laser cladding coatings10.1016/j.triboint.2019.01.019 ↗
23. Effect of laser remelting on microstructure and properties of WC reinforced Fe-based amorphous composite coatings by laser cladding10.1016/j.optlastec.2018.01.024 ↗
24. Phase evolution of ductile iron during laser cladding processing10.1016/j.surfcoat.2018.02.011 ↗
25. Microstructure and wear resistance of electromagnetic field assisted multi-layer laser clad Fe901 coating10.1016/j.surfcoat.2020.125876 ↗
26. Effect of deposition material and heat treatment on wear and rolling contact fatigue of laser cladded rails10.1016/j.wear.2018.07.001 ↗
27. Elevated temperature dry sliding wear behavior of nickel-based composite coating on austenitic stainless steel deposited by a novel central hollow laser cladding10.1016/j.apsusc.2011.08.072 ↗
28. Hot corrosion studies of HVOF sprayed Cr3C2–NiCr and Ni–20Cr coatings on nickel-based superalloy at 900 C10.1016/j.surfcoat.2005.12.030 ↗
29. Wear properties and microstructural analyses of Fe-based coatings with various WC contents on H13 die steel by laser cladding10.1016/j.surfcoat.2019.04.063 ↗
30. Investigation on cored-eutectic structure in Ni60/WC composite coatings fabricated by wide-band laser cladding10.1016/j.jallcom.2015.04.136 ↗
31. Effect of heat treatment on microstructure and mechanical properties of stellite 12 fabricated by laser additive manufacturing10.1007/s11665-017-2984-0 ↗
32. Investigation on the microstructure and wear behavior of laser-cladded high aluminum and chromium Fe-BC coating10.3390/ma13112443 ↗
33. Microstructure and the wear mechanism of grain-refined aluminum during dry sliding against steel disc10.1016/j.wear.2007.05.010 ↗
34. Friction–wear performances and oxidation behaviors of Ti3AlC2 reinforced Co–based alloy coatings by laser cladding10.1016/j.surfcoat.2020.126816 ↗
35. Investigation into wear of Ti–6Al–4V under reciprocating sliding conditions10.1016/j.wear.2008.12.083 ↗
36. High temperature wear resistance of laser cladding NiCrBSi and NiCrBSi/WC-Ni composite coatings10.1016/j.wear.2011.01.003 ↗
37. Friction and wear behaviors of Fe-19Cr-15Mn-0.66N steel at high temperature10.3390/coatings11111285 ↗
38. Effects of laser power on friction–wear performances of laser thermal sprayed Cr3C2–NiCr composite coatings at elevated temperatures10.1016/j.optlastec.2019.04.022 ↗
39. Friction and wear behavior of CrN coating on 316L stainless steel in liquid sodium at elevated temperature
40. Friction and wear behavior of laser cladded WC-Co and Ni/WC-Co deposits at high temperature10.1016/j.ijrmhm.2019.02.025 ↗
41. Microstructure and tribological performance of sulfurizing layer prepared on the laser cladding Co-based alloy coating10.1016/j.surfcoat.2017.10.005 ↗
42. Characteristics of oxidative wear and oxidative mildwear10.1016/j.triboint.2013.01.003 ↗
43. The gradient microstructure and high-temperature wear behavior of the CoCrMoSi coating by laser cladding10.1007/s11666-021-01184-0 ↗
44. Investigation on the microstructure and wear behavior of laser-cladded high aluminum and chromium Fe-B-C coating10.3390/ma13112443 ↗
45. Elevated temperature dry sliding wear behavior of nickel-based composite coating on austenitic stainless steel deposited by a novel central hollow laser cladding10.1016/j.apsusc.2011.08.072 ↗
46. AFM and tribological properties of thin nc-WC/a-C coatings10.1016/j.jeurceramsoc.2012.01.037 ↗
47. The tribological and electrochemical behavior of HVOF-sprayed Cr3C2–NiCr ceramic coating on carbon steel10.1016/j.ceramint.2014.12.102 ↗
48. Microstructure and high-temperature wear behaviour of Inconel 625 multi-layer cladding prepared on H13 mould steel by a hybrid additive manufacturing method10.1016/j.jmatprotec.2020.117036 ↗
49. High temperature wear resistance of laser cladding NiCrBSi and NiCrBSi/WC-Ni composite coatings10.1016/j.wear.2011.01.003 ↗
50. High-temperature wear resistance, and corrosion resistance of laser cladded Co-based coating10.1007/s11665-021-05704-5 ↗
51. High-temperature sliding wear of metals10.1016/S0301-679X(02)00041-5 ↗