journal article·2023-01

Study on wear and rolling contact damage mechanism between quenched U75V rail and wheels with different microstructures

Jihua Liu, Peng Chen, Yangting Ou, Guiyuan Zhou, Pijie Yu, Zhibiao Xu, Yongjian Li, Peng Li, Chenggang He, Xin Dai, Yujun Zhou

Wear· Volume 512-513
Publisher page

Abstract

Most existing wheel/rail hardness matching studies have been carried out using pearlite steels with different hardnesses; no relevant wheel–rail hardness matching research has been carried out for other microstructure types such as bainite and other tempered materials. In this paper, a CL60 wheel (pearlite) was quenched and tempered to obtain wheel materials with a certain hardness gradient, and matching tests between different wheel materials and a quenched U75V rail were carried out to explore the influence of wheel microstructures on wheel–rail damage. The results showed that with increasing tempering temperature, the wheel microstructure changes from tempered troostite to tempered sorbite, with ferrite changing from a needle shape to a multilateral shape; additionally, the cementite particles grow obviously larger, resulting in a gradual decrease in wheel hardness. With the increase in the wheel/rail hardness ratio, the wear rate of the wheel and wheel–rail system first increases and then decreases; the wear rate of tempered sorbite is the highest. Wear surface analyses indicate that typical peeling appears on the wear surfaces of the CL60 wheel as well as the coupled rail. Tempered sorbite shows slight peeling; however, severe peeling and delimitation occur on the wear surface of its coupled rail. Moreover, severe peeling and serious material delamination are present on the wear surface of tempered troostite, and typical peeling appears on its coupled rail surfaces. The fatigue crack initiation and propagation behaviors of wheel and rail materials are closely related to their microstructures. The cracks in pearlite always initiate on the surface and propagate along the ferrite line. Short and shallow fatigue cracks appear on the tempered sorbite with a high wear rate, and the cracks in the tempered troostite easily expand into the centre of the samples, indicating poor rolling contact fatigue (RCF) resistance. Therefore, the pearlite structure shows better comprehensive mechanical properties for wheel service; moreover, more attention should be given to wheel microstructure when conducting research on wheel–rail matching.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Railway Engineering and Dynamics · Mechanical stress and fatigue analysis · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Key problems faced in high-Speed train operation10.1631/jzus.A1400338 ↗
2. Comparisons between beam and continuum models for modeling wheel-rail impact at a singular rail surface defect10.1016/j.ijmecsci.2021.106400 ↗
3. Effect of graphite and MoS2 based solid lubricants for application at wheel-rail interface on the wear mechanism and surface morphology of hypereutectoid rails10.1016/j.triboint.2021.106886 ↗
4. An experimental study of high speed wheel-rail adhesion characteristics in wet condition on full scale roller rig10.1016/j.wear.2019.203092 ↗
5. Study of rolling contact fatigue, rolling and sliding wear of Class B wheel steel against R350HT and R260 rail steels under dry contact conditions using twin disc setup10.1016/j.triboint.2022.107711 ↗
6. Experimental study on wear properties of wheel and rail materials with different hardness values10.1016/j.wear.2021.203831 ↗
7. Investigation of the influence of rail hardness on the wear of rail and wheel materials under dry conditions (ICRI wear mapping project)10.1016/j.wear.2019.05.030 ↗
8. The low adhesion problem: the effect of environmental conditions on adhesion in rolling-sliding contact10.1016/j.triboint.2020.106521 ↗
9. Study of rolling-sliding contact damage and tribo-chemical behavior of wheel-rail materials at low temperatures10.1016/j.engfailanal.2022.106077 ↗
10. Influence of ambient humidity on the adhesion and damage behavior of wheel-rail interface under hot weather condition10.1016/j.wear.2021.204091 ↗
11. Role of ambient temperature in the adhesion and damage characteristics of wheel/rail interface during rolling-sliding contact10.1016/j.wear.2022.204458 ↗
12. Fatigue and wear behavior of pearlitic and bainitic microstructures with the same chemical composition and hardness using twin-disc tests
13. Rail-it’s behaviour and relationship to total system wear
14. Rail grade selection and friction management: a combined approach for optimizing rail-wheel contact10.1179/1743281212Y.0000000038 ↗
15. Optimization of hardness ratio in rail-wheel friction pair
16. Experimental study on hardness matching of wheel and rail materials for high speed railway
17. Experimental evaluation of rolling contact fatigue in railroad wheels10.1016/j.ijfatigue.2016.05.035 ↗
18. Hardness matching behavior of wheel/rail materials
19. New insight into the dry rolling-sliding wear mechanism of carbide-free bainitic and pearlitic steel
20. Investigation of the influence of rail hardness on the wear of rail Hardness on the Wear of Rail and Wheel and materials under dry conditions Wear and RCF mechanisms
21. Investigation on wear and rolling contact fatigue of wheel-rail materials under various wheel/rail hardness ratio and creepage conditions10.1016/j.triboint.2019.106091 ↗
22. Experimental study on wear properties of whee1 and rail materials with different hardness values10.1016/j.wear.2021.203831 ↗
23. A review of the American press
24. Slippage effects on the crack behavior of pearlitic steel induced via rolling-sliding friction
25. Towards a standard approach for the wear testing of wheel and rail materials10.1177/0954409717700531 ↗
26. Micro-mechanism of polygonization wear on railroad wheels10.1016/j.wear.2017.09.017 ↗
27. Study on the mechanism for polygonisation formation of D2 wheel steel and its effect on microstructure and properties under rolling wear conditions10.1016/j.wear.2020.203261 ↗
28. Wear by plastic ratcheting10.1016/S0043-1648(97)00083-5 ↗
29. Numerical analysis of wheel rail rolling contact ratcheting effect
30. Ratcheting behavior of high strength rail steels under bi-axial compression-torsion loadings: experiment and simulation10.1016/j.ijfatigue.2014.03.021 ↗
31. Influence of original microstructure on rolling contact fatigue property of D2 wheel steel10.1016/j.wear.2020.203380 ↗
32. Crack propagation in rails under rolling contact fatigue loading conditions based on material forces10.1016/j.ijfatigue.2012.06.002 ↗
33. The influence of microstructure on the rolling contact fatigue of steel for high-speed-train wheel10.1016/j.wear.2015.10.002 ↗
34. The effect of anisotropy on crack propagation in pearlitic rail steel10.1016/j.wear.2013.11.034 ↗