Correlation of the wear transition in CoCrMo alloys with the formation of a nanocrystalline surface layer and a proteinaceous surface film
Source abstract
Abstract
Abstract CoCrMo alloys have been widely used in metal-on-metal (MoM) hip replacements. On the one hand, they have exhibited excellent long-term survival rates, but recently high failure rates have been observed, associated with adverse local tissue reactions. It is still a puzzle why CoCrMo alloys sometimes work very well, while at the other times the wear rate is unacceptably high. There have been several reports that the formation of a surface proteinaceous layer appears to reduce the wear rate. Equally, the formation of a surface nanocrystalline layer has been observed, but it remains unclear whether this is a good or bad phenomena. The present work directly correlates the surface deformation structure and the presence of a proteinaceous film with the wear behaviour. The lowest specific wear rates were associated with the formation of a proteinaceous layer. A wear transition was observed at higher load, associated with the loss of the proteinaceous layer and the formation of a thick surface nanocrystalline layer. The formation of the proteinaceous layer appeared to be associated with some surface deformation of the CoCrMo, which presumably removed the surface oxide. Although the formation of a thick, fine nanocrystalline layer resulted in the highest surface hardness and yield strength, it also coincided with the highest wear rate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Advanced materials and composites · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. In vivo wear of 3 types of metal on metal hip prostheses during 2 decades of use10.1097/00003086-199608001-00013 ↗
2. Twenty year results of McKee-Farrar versus Charnley prosthesis10.1097/00003086-199608001-00006 ↗
3. Long-term survival of McKee-Farrar total hip prostheses10.1097/00003086-200209000-00013 ↗
4. The long-term wear of retrieved McKee-Farrar metal-on-metal total hip prostheses10.1016/j.arth.2004.09.028 ↗
5. Do the potential benefits of metal-on-metal hip resurfacing justify the increased cost and risk of complications?10.1007/s11999-010-1301-0 ↗
6. Results of Birmingham hip resurfacing at 12 to 15 years: a single-surgeon series10.1302/0301-620X.96B10.33695 ↗
7. The outcome of the Birmingham hip resurfacing in patients aged <50 years up to 14 years post-operatively10.1302/0301-620X.95B9.31711 ↗
8. Failure rates of stemmed metal-on-metal hip replacements: analysis of data from the National Joint registry of England and Wales10.1016/S0140-6736(12)60989-1 ↗
9. Five-year results of the ASRXLA acetabular system and the ASR hip resurfacing system: an analysis from the Australian orthopaedic association national joint replacement registry10.2106/JBJS.J.01727 ↗
10. Engineering issues and wear performance of metal on metal hip implants10.1097/00003086-199612000-00009 ↗
11. The pathways of dynamic recrystallization in all-metal hip joints10.1016/j.wear.2005.02.036 ↗
12. Micro-structural alterations within different areas of articulating surfaces of a metal-on-metal hip resurfacing system10.1016/j.wear.2009.01.012 ↗
13. Dynamic surface microstructural changes during tribological contact that determine the wear behaviour on hip prostheses: metals and ceramics10.1039/c2fd00002d ↗
14. P.Zeng, W.M.Rainforth, D.Sun, J.A.Wharton, R.J.K.Wood,Subsurface microstructural changes of multi-micro-scratches of biomedical CoCrMo. In preparation
15. The tribological difference between biomedical steels and CoCrMo-alloys10.1016/j.jmbbm.2012.01.007 ↗
16. The acting wear mechanisms on metal-on-metal hip joint bearings: in vitro results10.1016/S0043-1648(01)00654-8 ↗
17. Tribochemical reaction on metal-on-metal hip joint bearings a comparison between in-vitro and in-vivo results10.1016/S0043-1648(03)00127-3 ↗
18. Subsurface characterisation of wear on mechanically polished and electro-polished biomedical grade CoCrMo10.1016/j.wear.2015.02.007 ↗
19. Characterisation of the oxide film on the taper interface from retrieved large diameter metal on polymer modular total hip replacement10.1016/j.triboint.2014.12.012 ↗
20. Determination of elastoplastic properties by instrumented sharp indentation10.1016/S1359-6462(99)00011-1 ↗
21. Determination of elastoplastic properties by instrumented sharp indentation
22. Nanoindentation for probing the mechanical behavior of molecular crystals–a review of the technique and how to use it10.1039/C3CE41266K ↗
23. The effect of contact load on CoCrMo wear and the formation and retention of tribofilms10.1016/j.wear.2015.02.013 ↗
24. Wear mechanisms in metal-on-metal bearings: the importance of tribochemical reaction layers
25. Lubrication of metal-on-metal hip joints: the effect of protein content and load on film formation and wear10.1016/j.jmbbm.2011.09.008 ↗
26. The adsorption and lubrication behavior of synovial fluid proteins and glycoproteins on the bearing-surface materials of hip replacements10.1016/j.biomaterials.2008.12.062 ↗
27. Tribochemical reaction in metal-on-metal hip joints influence wear and corrosion
28. CoCrMo metal-on-metal hip replacements10.1039/C2CP42968C ↗
29. Subsurface microstructural alterations during sliding wear of biomedical metals
30. Biotribocorrosion of CoCrMo orthopaedic implant materials- assessing the formation and effect of the biofilm10.1016/j.triboint.2007.02.019 ↗
31. Deformation structure induced by sliding contact10.1080/01418619208201580 ↗